Some experiments with hexabutylditin against fungi
1977 - IRG/WP 388
The investigation was carried out in 1972 and 1973 to collect experimental data about the poisonousness of hexabutylditin (HBDT) against the woodrotting fungi Coniophora puteana (Coniophora cerebella), strain 15, and Chaetomium globosum, strain hexabutylditin was being manufactured by the Organisch Chemisch Instituut (O.C.I.) TNO, at Utrecht....
J W P T Van der Drift


LCA applied for wooden products
1995 - IRG/WP 95-50059
This paper presents some of the international developments within ISO and SETAC to standardize and harmonize LCA methodologies. In this framework it is also important to be aware of the problems that companies have to generate and validate data for the complete product chain from cradle to grave. This concerns problems in nomenclature of substances and processes, system boundaries, allocation prob...
A Kloppenburg, A Van Dam


Fipronil - le nouvel insecticide de Rhone Poulenc pour la preservation du bois
1995 - IRG/WP 95-30078
After the 3rd International Symposium in Cannes '95. More trial results and practical information on FIPRONIL, this new insecticide from Rhone Poulenc for Wood Preservation and PCO....
M G E J Van Maanen


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Reporting from SPC and Working Party sessions at IRG 45
2015 - IRG/WP 14-60375
J Van Acker


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals


Investigation into the heterogeneous nature of the impregnability of some poplar hybrids
1995 - IRG/WP 95-40052
Retention figures of some poplar hybrids are very heterogeneous when pressure impregnated. This makes it hard to prescribe impregnation processes for fast grown poplars that make it suitable for higher hazard uses. In order to gain fundamental knowledge in their variability in impregnation properties two trees were selected for a detailed investigation. Both trees originate from the same plantatio...
J Van Acker, M Stevens


Statistically stable models for determination of PEC
1999 - IRG/WP 99-50135
In June 1998 the European Wood Preservative Manufacturer's Group prepared a document to support the Technical Guidance concerning the placing of products on the market with respect to the Directive 98/08/EC (BPD). The essentials of this document were presented at the COST E2 meeting in Cannes last year and at the following IRG conference (Baines and Davis, 1998; IRG/WP/98-50101/20). The d...
W J Homan, A L Van Oosten Van


Current models used by the European Health Authorities to evaluate the volatilization of active ingredients from treated wood used inside dwellings. A case study: Volatilization of azaconazole and propiconazole from treated wood
1990 - IRG/WP 3565
The use of wood preservatives inside houses may result in measurable aerial concentrations of active ingredients. These airborne contaminants may be inhaled by the inhabitants over periods lasting from a couple of days to several months. To assess the potential health hazard of preservative residues in the air, various risk-assessment models have been worked out. Three schemes, currently used by t...
A R Valcke, L Van Leemput


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Effect of wood moisture on ability of Sphaeropsis sapinea to colonise Pinus radiata
1999 - IRG/WP 99-10311
The factors influencing colonisation of unseasoned radiata pine logs by sapstaining fungi which can result in detrimental wood discolouration, are being explored. The objective of the current study was to determine the effect of wood moisture content on fungal growth and wood colouration (melanisation). Five replicate trials were set up using increment cores (10mm diameter) which were taken from ...
B Kreber, D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Highly virulent wood-rotting Basidiomycetes in cooling tower timbers
1995 - IRG/WP 95-10125
Over the past ten years most industrial cooling towers changed their water treatment systems in order to meet environmental requirements. Since this alterations wood rot attack has been reported more frequently. Several Basidiomycete fungi were isolated and determined. Amongst the most important ones are strains of Physisporinus vitreus (Pers.:Fr.) P. Karst., Phellinus contiguus (Fr.) Pat. and Don...
J Van Acker, M Stevens, V Rijckaert


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Environmental risk assessment of treated timber in service: The Environment Focus Group approach
2000 - IRG/WP 00-50162
In the context of the Biocidal Products Directive (98/8/EC), and of the OECD work on wood preservatives, the Environment Focus Group (EFG), comprising 8 institutes and the European Wood Preservative Manufacturers Group, has been working on the environmental risk assessment of treated timber in service. A literature review of emissions from treated timber has revealed that very little existing data...
G Deroubaix, G Labat, I Le Bayon, S Legay, P Marchal, C Yrieix, E Melcher, R-D Peek, S De Geyter, J Van Acker, W J Homan, D J Dickinson, R J Murphy, E D Suttie, A J Nurmi, A-C Ritschkoff, D Rudolph, I Stephan, D Aston, E F Baines, J B Simonin


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...
A Omidvar, M H Schneider, A R P Van Heiningen


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker