Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt


Principles and procedure of the planeing test
1981 - IRG/WP 2162
Small end-sealed samples of pine-sapwood (1.5 x 2.5 x 5 cm³) are treated by brushing and afterwards different parts of the treated surface are removed. The remaining part of the sample is tested against either insects or fungi. If no attack occurs sufficient amounts of biocides have been penetrated at least beyond the zone which has been removed. In spite of some problems the test seems the only ...
H Willeitner, M Gersonde


Supplement to Document No: IRG/WP/56. Health and safety aspects of the use of wood preservatives
1975 - IRG/WP 356
H Willeitner


Use of biossay to determine CCF and CCB preservative retentions in treated Pinus sylvestris
1984 - IRG/WP 2216
The retention of each a copper/chromium/boron and copper/chromium/fluoride preservative in pressure treated pinepoles was tested by bioassay using Aspergillus niger as test fungus. Small samples of 5 mm³ were taken from various depth of the poles and placed on potato-dextrose agar plates. The inhibition of fungal growth depends on the preservative retention in the cubes and corresponds closely to...
J C Moreschi, H Willeitner


Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm


Health and safety aspects of the use of wood preservatives. Preliminary evaluation of the answers to the IRG-Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 56
This preliminary evaluation of the answers to the IRG/WP-Questionnaire only gives a general survey on those questionnaires, which the author received until June 13, 1974. Details, such as correlations between importance of wood preservation and pollution control, could not be considered due to lack of time. For the same reason it was not possible so far, to evaluate the additional remarks given in...
H Willeitner


2nd IRGWP - Questionnaire on the state of pollution control in the field of wood preservation (Introductory letter)
1981 - IRG/WP 3184
H Willeitner


2nd IRGWP - Questionnaire on the state of pollution control in the field of wood preservation
1981 - IRG/WP 3185
H Willeitner


Questionnaire on the state of pollution control in the field of wood preservation
1974 - IRG/WP 52
H Willeitner


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


An evaluation of the potential of ion mobility spectrometry for detection of organic wood preservative components in solutions and treated wood
1994 - IRG/WP 94-20038
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Until now, no highly sensitive rapid analytical methods are available for the detection of wood preservatives under industrial process conditions. Preliminary experiments showed that Ion Mobility Spectrometry (IMS) could be a promising method for rapid detection of organic preser...
A Voss, J N R Ruddick, W J Homan, H Militz, H Willeitner


World survey on the status of pollution control in the field of wood preservation
1976 - IRG/WP 369
In 1974 the IRG/WP-Secretariat distributed a "Questionnaire on the state of pollution control in the field of wood preservation" which was prepared by the author. The questionnaire consisted of two parts. Part A asked "General questions" on - the position of wood preservation in the respective country - the use of preservatives - the type of application of wood preservatives in different fields - ...
H Willeitner


Influence of sampling on the composition of test solutions
1985 - IRG/WP 2235
For four commercial products of CCB-salts the influence of the kind of sampling on the composition of test solutions has been tested. For each product several 5 g samples have been taken at random, after careful mixing the content of each bottle, and after grinding the whole content. With each sample a 5% test solution was made and analyzed on the content of chromium, copper and boron. Altogether ...
H Willeitner, K Brandt


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Five years leaching of Boron
1999 - IRG/WP 99-30195
The diffusibility of Boron in wood and thus its leaching behaviour in water contact is known since long. Nevertheless quantitative data on the long-term leaching behaviour are rare. Consequently, field exposure tests were started with beam-segments treated with pure boric acid and with poles treated with CCB. Detailed data of more than five years of field exposure are now available. Pure boron tre...
A Peylo, H Willeitner


Influence of hydrophobic agents on the leachability of boron
1995 - IRG/WP 95-30064
Besides its low mammalian toxicity and a broad range of activity towards both fungi and insects, boron shows a high diffusibility, encouraging it to treat wood species of low permeability. However, its difussibility is at the same time responsible for a high risk of leaching, known since long. Nevertheless quantitative data about this process are only rarely available. Therefore, the leaching of b...
A Peylo, H Willeitner


Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Fixation of CCA preservatives in cocos-, oil- and rattan-palm
1986 - IRG/WP 3371
In previous tests with jubaea-palm almost no fixation of a CCA-preservative Type B could be achieved, consequently, further leaching tests were carried out with samples of 1 cocos-, 1 oil- and 2 rattan-palms from Malaysia. A good fixation of chromium and copper took place in cocos-palm after 4 weeks storage at 28°C. Nevertheless the fixation was slower than in pine-wood and demanded an elevated t...
H Willeitner, K Brandt


Preliminary evaluation of the answers to the 2nd IRG/WP-questionnaire on the state of pollution control in the field of wood preservation
1982 - IRG/WP 3209
This preliminary evaluation of the answers to the 2nd IRG/WP-Questionnaire only gives a general survey on those questionnaires which the author received until April 30th, 1982. Details, such as correlations between importance of wood preservation and pollution control, as well as a comparison of the answers with those to the first questionnaire (Doc. IRG/WP/369), could not be considered due to lac...
H Willeitner