Insight in moisture dynamics of wood treated with organosilicon compounds
2016 - IRG/WP 16-20598
The SILEX project “Improving sustainability of construction materials using innovative Silicon based treatment” is a Life+ project with reference LIFE+11 ENV/BE/1046 and started in April 2013. This project intends to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. The project aims at demonstra...
J Van Acker, J Van den Bulcke, I De Windt, S Colpaert, S De Rocker, S Salvati, J-P Lecomte


Assessing the natural durability for different tropical timber species using the mini-block test
2017 - IRG/WP 17-10886
The Xylarium in the Royal Museum for Central Africa (RMCA, Tervuren, Belgium) contains over 60,000 wood-samples, comprising over 12,000 species. These samples are of great historical and scientific value yet have a random format, which complicates standard testing. The wood-durability against Coniophora puteana and Trametes versicolor was tested for 36 species. Due to the random sample sizes the s...
V Deklerck, I De Windt, N Defoirdt, J Van den Bulcke, H Beeckman, E Espinoza, J Van Acker


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


Moisture behaviour and biological durability of high performance flax fibre reinforced composites
2017 - IRG/WP 17-40803
For natural fibre composites in structural and load bearing applications long reinforcing fibres are required. Therefore, much research is performed on flax fibre reinforced composites to optimize them for high performance use. In most cases such research focuses on the mechanical properties, yet the assessment of moisture behaviour, dimensional stability and biological durability is an important ...
N Defoirdt, J Van den Bulcke, F Bensadoun, J Ivens, I Verpoest, J Van Acker


Organosilicon-based impregnation hydrophobers for wood
2017 - IRG/WP 17-40808
The SILEX project “Improving sustainability of construction materials using innovative Silicon based treatment” is a Life+ project with reference LIFE+11 ENV/BE/1046 and started in April 2013. This project intends to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. The project aims at demonstra...
J-P Lecomte, J Van Acker, J Van den Bulcke, M Kutnik, M Montibus, S Salvati, S Derocker


Assessing the nutrient value of bio-based materials in relation to early fungal growth
2017 - IRG/WP 17-20631
Bio-based materials are gaining importance in the building industry, as the focus on sustainability and life-cycle-assessment has increased dramatically over the last decade. Wood and wood-engineered products as well as insulation materials made from flax, hemp, etc. are hence increasingly used. These materials originate from renewable resources and are often biodegradable, which can cause problem...
L De Ligne, J Van den Bulcke, J Baetens, B De Baets, J Van Acker


Impact of temperature and relative humidity on spatio-temporal fungal growth dynamics of Basidiomycetes
2018 - IRG/WP 18-10905
Basidiomycetes can cause considerable damage to wood and other bio-based building materials. Knowing at which environmental conditions these decay fungi generally thrive, and how the environmental conditions affect fungal growth characteristics, is therefore of particular interest. In this paper, we use image analysis to assess the impact of the environmental conditions on the growth dynamics of C...
L De Ligne, G Vidal-Diez de Ulzurrun, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Enhancing service life performance of oak decking and cladding using organosilicon treatments
2018 - IRG/WP 18-40838
The Life+ project SILEX, in full “Improving sustainability of construction materials using innovative Silicon based treatment” started in April 2013 and was finalized mid 2017. The aim of this project was to demonstrate that a new class of compounds can be used for wood treatment for an extended service life combined with enhanced new testing methodology. Ultimately, it was the intention to de...
J Van Acker, J Van den Bulcke, J-P Lecomte


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Combining MRI and X-ray CT to monitor fungal decay of plywood and OSB in a lab test
2022 - IRG/WP 22-20683
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, T Núñez Guitar, C Vanhove, J Van Acker, J Van den Bulcke


Moisture sorption behaviour of poplar and thermally modified poplar using dynamic vapour sorption (DVS)
2022 - IRG/WP 22-40947
The moisture sorption behaviour of wood has a critical impact on service life. In Europe, softwood is mostly used to manufacture engineered wood products such as cross-laminated timber (CLT) or glue-laminated timber (GLT or glulam). Yet fast-growing and widespread tree species such as hybrid poplar with or without modification, have potential to meet the increasing demand. This study shows the moi...
X Jiang, J Van den Bulcke, L De Boever, M Minsart, A Mignon, J Van Acker


Investigating moisture dynamics and fungal decay risk: integrating X-ray CT visualization and simulation benchmarks through a Fungal Control Unit
2024 - IRG/WP 24-11045
Wood is susceptible to fungal attack and over time the structural integrity can be compromised. This risk is of course strongly related to moisture dynamics, as moisture is needed for fungal growth. While existing methodologies, such as lab and field tests, provide valuable insights into wood decay, they often fall short in replicating real-life conditions, particularly within the intricacies of t...
J Van den Bulcke, J Van Acker, M Delbeke, A Blommaert, N Van Den Bossche, M Steeman, L De Ligne


Service life of poplar, a low durability hardwood
2024 - IRG/WP 24-41007
Hybrid poplar is the most common plantation hardwood of the temperate climate zone and is complementary to natural stands of aspen with mainly plantations in Europe and China. Poplar wood has been considered as a valid alternative for many of the construction applications of softwoods especially when considering engineered wood products. The natural durability of hybrid poplar is low and for a ra...
J Van Acker, X Jiang, L De Ligne, J van den Bulcke


Über den Nagekäfer Oligomerus ptilinoides (Wollaston), Col., Anobiidae: Verbreitung und Einschleppung, Bestimmung, Lebens- beziehungen und Befallsmerkmale mit Vergleichen zu Nicobium
1980 - IRG/WP 1102
Oligomerus ptilinoides occurs in the Mediterranian and Black-sea area, in North-Africa and Asia minor as an important pest causing severe damage to dry wood. By travelling, by the immigration of people from south to north, and by accidental introductions the species tends to establish itself north of the Alps. Severe damage has recently been observed in two museums. An account is given of aspects ...
S Cymorek


Schrifttum über den Hausbockkäfer Hylotrupes bajulus L. (Serville) (Coleoptera, Cerambycidae)
1977 - IRG/WP 164
H Becker


Untersuchungen über das Vorkommen und den Schaden der Rossameisen (Camponotus herculeanus und Camponotus ligniperda) in Gebäuden in Schweden
1976 - IRG/WP 147
Die wichtigsten Ergebnisse der vorliegenden Untersuchung der von Rossameisen befallenen Häuser in Schweden können wie folgt zusammengefasst werden. Rossameisenschaden kommt in ganz Schweden vor, jedoch hauptsächlich in Küstengebieten und in der Nähe von grossen Seen. Beide Rossameisenarten schaden in gleicher Weise. Camponotus herculeanus ist im ganzen Lande zu finden, Camponotus ligniperda d...
V Butovitsch


Wood plastic composites from modified wood. Part 3. Durability of WPCs with bioderived matrix
2008 - IRG/WP 08-40423
The decay resistance of fully bio-derived wood plastic composites, WPCs, was tested in both laboratory and field tests. The laboratory tests were performed according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils) and the field tests according to EN 252 (stakes in ground) and EN 275 (resistance to marine borers). The WPC materials for laboratory tes...
M Westin, P Larsson Brelid, B K Segerholm, M Van den Oever


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker