Insect resistance of preservative treated tropical plywood against Lyctus
1990 - IRG/WP 1453
Seven plywood types composed of tropical wood species, vulnerable to Lyctus, were treated with various commercial water-borne and oil-borne preservatives. A wide range of preservative retentions was obtained by treating boards with dip treatment, steeping, double-vacuum and vacuum-pressure impregnations. Selected samples were subsequently tested for their insect resistance against Lyctus africanus...
J Van Acker, M Stevens, M Pallaske


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


Effect of protective additives on leachability and efficacy of borate treated wood
2002 - IRG/WP 02-30290
Borate preservatives have been used extensively in many countries as an effective means for protecting wood against fungal and insect attack especially in interior environments. Under exterior conditions, borate compounds have a main disadvantage as they can be leached from treated wood as a result of their water solubility. In this study, we compared the potential of different additives for re...
A Mohareb, J Van Acker, M Stevens


Laboratory culturing and decay testing with Physisporinus vitreus and Donkioporia expansa orginating from identical cooling tower environments show major differences
1996 - IRG/WP 96-10184
Both Basidiomycete fungi Physisporinus vitreus (Pers.:Fr.) P. Karst. and Donkioporia expansa (Desm.) Kotl. & Pouz. were isolated from identical cooling tower environments. Azobé heartwood (Lophira alata), a very durable tropical wood species was totally deteriorated in cooling towers in a similar way by both fungi. First attempts to culture Physisporinus vitreus in laboratory circumstances sh...
J Van Acker, M Stevens


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


An appraisal of methods for environmental testing of leachates from salt-treated wood (2)
1998 - IRG/WP 98-50110
For wood preservatives for use in hazard class 4 information on the ecotoxicity of preservatives and ingredients as well as on the effect of losses from impregnated timber is needed for a proper environmental risk assessment. In the evaluation of a suitable test procedure the leaching behaviour of copper-based formulations was studied using analytical and ecotoxicological test methodology. These ...
H W Wegen, A Platen, G M F Van Eetvelde, M Stevens


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Investigation into the heterogeneous nature of the impregnability of some poplar hybrids
1995 - IRG/WP 95-40052
Retention figures of some poplar hybrids are very heterogeneous when pressure impregnated. This makes it hard to prescribe impregnation processes for fast grown poplars that make it suitable for higher hazard uses. In order to gain fundamental knowledge in their variability in impregnation properties two trees were selected for a detailed investigation. Both trees originate from the same plantatio...
J Van Acker, M Stevens


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Highly virulent wood-rotting Basidiomycetes in cooling tower timbers
1995 - IRG/WP 95-10125
Over the past ten years most industrial cooling towers changed their water treatment systems in order to meet environmental requirements. Since this alterations wood rot attack has been reported more frequently. Several Basidiomycete fungi were isolated and determined. Amongst the most important ones are strains of Physisporinus vitreus (Pers.:Fr.) P. Karst., Phellinus contiguus (Fr.) Pat. and Don...
J Van Acker, M Stevens, V Rijckaert


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Microscopical analysis of formaldehyde-acid modified wood
1981 - IRG/WP 3182
Cross-linking of wood with gaseous formaldehyde improves its hygroscopic and dimensional behaviour, and its resistance against micro-organisms. However, formaldehyde cross-linking reactions take place only in the presence of an acid catalyst, which results in losses in mechanical By optimization of a formaldehyde-sulfur dioxide vapour phase process the reaction conditions were established to limit...
M Stevens, N Parameswaran


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Comparative study on leaching of CCA from treated timber: Modelling of emission data
1994 - IRG/WP 94-50027
Results of a comparative study on leaching of CCA from treated timber are reported. The study aims at investigating the applicability of prestandard leaching test methods for modelling purposes. Prestandards used are the European standard proposed by CEN/TC38/WG11 and NEN 7345 (Dutch prestandard for building materials). Parameters of study are type of fixation, wood species (pine - spruce), specim...
G M F Van Eetvelde, M Stevens, L Van der Mijnsbrugge


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


Influence of clonal variability on the impregnability of poplar hybrids. (+ correction document of 23 April 1990)
1990 - IRG/WP 3614
The new Western European poplar clones (Populus nigra x deltoides and Populus trichocarpa x deltoides) were compared with the reference clone 'Robusta' and some old hybrids. Samples (5x5x50 cm³) with pure tangential/radial surfaces were sawn, including the transition zone between heartwood and sapwood. Treatment by a standard vacuum-pressure impregnation cycle with CCA showed a ...
J Van Acker Van, M Stevens, C De Haas


Qualifying ecotoxicity research on tropical hardwood leachates
1997 - IRG/WP 97-50096
Almost as a rule, quantification and identification of various types of environmental contamination is grounded on chemical evaluation principles. Yet for monitoring surface water pollution, aquatic bio-assays may provide a more direct way to assess the potential hazard of environmental samples. A battery of such tests is experienced onto leachates of tropical hardwoods used in ground and water co...
G M F Van Eetvelde, P Marchal, M Stevens


Resistance of acetylated wood to basidiomycetes, soft rot and blue stain
1994 - IRG/WP 94-40021
Poplar (Populus spp.), beech (Fagus sylvatica) and pine sapwood (Pinus sylvestris) samples were acetylated in a semi-industrial acetylation plant and tested for durability according to European standards. Resistance to Gloeophyllum trabeum, Coniophora puteana and Coriolus versicolor could be reached at a weight percent gain (WPG) of 12%. Susceptibility of acetylated pine to Poria placenta was high...
E P J Beckers, H Militz, M Stevens


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens