Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


Leachabilty and efficacy of fatty acid derived boron esters as wood preservatives - leachability and efficacy of fatty acid derived boron esters as wood preservatives
2004 - IRG/WP 04-30351
Borates have many advantages as wood preservatives. However, boron is susceptible to depletion under humid conditions and this restricts its outdoor use. In order to reduce boron leachability in treated wood, one of the anticipative approaches is to use organic fixed boron-based preservatives. This study investigated the leachability of six boron ester compounds as potential preservatives. Scots p...
A Mohareb, J Van Acker, M Stevens


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Environmental fate of copper-based wood preservatives in different soil substrates - Part 1: Screening of the metal adsorption potential
1998 - IRG/WP 98-50101-21 a
In treatment plants, spillage of wood preservatives onto soil may be of environmental concern. This potential soil contamination served as an objective for a screening study. Three different mineral soils, a mineral substrate and two horticultural substrates are examined for their sorptive potential of copper through mixing with wood preservative solutions. Depending on the soil/substrate charact...
G M F Van Eetvelde, J M Mwangi, F Tack, R Hartmann, M Stevens


Creosote losses due to ageing methods prior to laboratory efficacy testing
2002 - IRG/WP 02-20256
Laboratory efficacy testing of creosote is affected by the impact of volatile components on the fungal growth. European test methods for assessing efficacy against Basidiomycetes and soft rot fungi is based on two standard methods, EN 113 and ENV 807 respectively. Combined with both fungal tests two pre-treatment methods are commonly used, namely EN 84 (leaching) and EN 73 (evaporation). Within th...
J Van Acker, K Ghekiere, M Stevens


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


The accelerated L-joint test method for determination of the out of ground natural durability
1998 - IRG/WP 98-20146
The accelerated L-joint test incorporates a moistening device and uses a close end water trap in an open joint connection with a laminated tenon member consisting of the perishable reference wood species scots pine sapwood and beech. After one year of exposure it is possible to show a distinct identification of natural durability classes 4 and 5 against the more durable wood species. Both weight ...
J Van Acker, C Brauwers, M Stevens


Stability, performance and distribution of propiconazole (R 49362) in acceleratedly aged wood
1991 - IRG/WP 3647
The permanency of propiconazole (R 49362 - WOCOSENÔ technical - Janssen Pharmaceutica) in wood was examined in an 18 month storage test, an evaporative ageing study (EN 73), a volatilization stress experiment, and water-leaching studies (EN 84). The biological efficacy against two brown rot fungi: Coniophora puteana BAM Ebw. 15 and Gloeophyllum trabeum BAM Ebw. 109 was assessed according to the E...
A R Valcke, M Stevens


Wood Preservation in Belgium
1981 - IRG/WP 3170
The report reviews wood preservation activities in Belgium and notes the number of authorized treatment depots has doubled during the past five years. It lists the timbers that are allowed to be used for joinery and constructional building purposes and the preservatives and treatments with which these timbers may be protected. In Belgium not only have the wood preservative product and its treatmen...
M Stevens, R Cockcroft


Restrictions on the use of chlorosilanes as potential wood preservatives
1985 - IRG/WP 3345
The biological protection of wood by chemical modification with different types of chlorosilanes has been investigated. The impregnation of wood has been carried out by means of liquid phase and vapor phase treatments using pure silane and silane-solvent systems. The biological efficacy against wood rotting fungi, molds and staining fungi was determined in a number of screening trials, subsequentl...
M Stevens


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Increased biological durability differs for traditional wood preservation and new non-biocidal systems (NBS)
2000 - IRG/WP 00-20212
Wood preservation is a way to increase the biological durability of wood by the addition of chemical components with a biocidal effect. The effect of such treatment is clearly concentration dependent. At distinct levels of fungicide concentration fungi are killed or inhibited in their enzymatic functioning to provide nutrients. The toxic limits allow decision-makers to provide treating prescriptio...
J Van Acker, M Stevens


The development of blue stain in service in sapwood of European softwood species
1997 - IRG/WP 97-10236
The utilisation of softwood species for window joinery applications is gaining importance in countries frequently using tropical hardwood species up to now. Since wood preservation is not always part of the total concept of window frames manufactured from sapwood containing wood elements it is essential to know the impact of durability on the performance. Moisture content control is a major tool i...
J Van Acker, R Klaassen, H Militz, M Stevens


Modelling of copper emission fron treated wood leached according to NEN 7345 and ENV 1250.2
1996 - IRG/WP 96-20097
A series of water leaching experiments is carried out investigating pine and spruce treated and fixed using different copper-containing preservative solutions and process technologies. Water changes took place as prescribed in the Dutch standard NEN 7345 and the European test method ENV 1250.2, each of the leachates being chemically analysed for their copper content. Irrespective of the preservati...
G M F Van Eetvelde, S G L Michon, M Stevens


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


Screening of the technical performance and aquatic toxicity of N-methylolacrylamide treated wood
2000 - IRG/WP 00-40166
In the course of the last decades chemical modification of wood species, with a limited natural durability, has been subjected to intensive research. As a possible alternative and supplementary treatment of non-durable wood in a range of applications it remains one of the major topics in the wood preservation world. Different modification systems have been scaled-up and are now in an industrialisi...
V Rijckaert, S De Geyter, J Van Acker, M Stevens


Recycling of CCA treated wood in the US
1998 - IRG/WP 98-50101-08
The production of CCA treated wood has increased dramatically in recent years. Previous estimates of the volume of treated wood to be removed were based on the assumed service life of the material, generally 20 to 25 years. This study based on a survey of contractors installing treated decks, determined that the actual service life of these decks is much shorter than their assumed functional servi...
J McQueen, J Stevens, D P Kamdem


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens