IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 329 documents. Displaying 25 entries per page.


A comparison of the effectiveness of a vacuum oven and a wind tunnel in the accelerated ageing of treated wood by evaporation
1989 - IRG/WP 2334
R J Orsler, G E Holland


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Determination of thermal degradation of isothiazolone treated wood
1997 - IRG/WP 97-30154
Wood treated with 4,5-dichloro-2-n-octyl-4-isothiazolin-3-one was the subject of thermal degradation study. The study included burning isothiazolone treated wood under various temperatures with and without oxygen. The result showed that no harmful combustion products, such as polychlorinated dibenzo-p-dioxins, polychlorinated dibenzo-p-furans and polychlorinated biphenyls, were detected. These fin...
Bing Yu


The Effect of Flavonoids on Colour and Spectral Changes of the Wood Surface Caused by Heat Treatment or Ultra-violet Irradiation
2006 - IRG/WP 06-40341
Both heat treatment and UV irradiation can cause discolouration and change in the spectral properties of wood surface. Some of the characteristic flavonols have significant role on colour and spectral changes, despite of their relative small quantities in wood. Colour changes and spectral properties of natural and extracted black locust (Robinia pseudoacacia L.) and poplar (Populus nigra L.) were...
R Csonka-Rákosa, L Molnár-Hamvas, E Börcsök, J Molnár, K Németh


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures with a surprising result. Carbon nanotubes (CNTs) were produced when a specific heating regime was used to carbonize the wood fiber. ...
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


Utilization of TG-DSC to study thermal degradation of beech and silver fir
2013 - IRG/WP 13-40628
Thermal treatment of wood is, besides other wood modification system, used to improve the decay resistance and dimensional stability. However, the chemical changes that are caused by treatment process are still difficult to quantify, characterize and control. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during...
K Candelier, A Treu, J Dibdiakova, E Larnøy, A Petrissans, S Dumarçay, M Pétrissans, P Gérardin


Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen


An evaluation method for less termite attack execution on thermal insulation for fundation walls
2002 - IRG/WP 02-20245
According to the results by the real scale Japanese building tests, the termite installation was observed at very little spaces between foundation and insulation. The termite penetration spaces between foundation and insulation on foundation systems in Japanese wooden houses were checked by the way of streaming speed of colored water. Because of difficulty for its execution, the parts of outside a...
K Suzuki, Y Tanaka


Fungal and bacterial attack of CCA-treated Pinus radiata timbers from a water-cooling tower
1991 - IRG/WP 1488
Transmission electron microscopy of decaying CCA-treated Pinus radiata timbers from an industrial water cooling tower showed presence of a thick biofilm covering some areas of the wood. The biofilm contained various morphologically distinct forms of microorganisms embedded in a slime. The study provided evidence of the activity of soft rot fungi and tunnelling and erosion bacteria in wood cells. T...
A P Singh, M E Hedley, D R Page, C S Han, K Atisongkroh


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


Effect of medium-term degradation of beech wood by erosive (Phanerochaete chrysosporium) and lignin-selective (Ceriporiopsis subvermispora) strains of white rot fungi on its selected physical properties
2004 - IRG/WP 04-40292
At the Faculty of Wood Sciences and Technology a fungal delignification of normal and tension beech wood by erosive and lignin-selective strains white-rot fungi has been studied. The pre-treatment of both kind of wood samples was accompanied by partial delignification and apparent changes of their physical properties influencing the polar liquids penetration....
R Solár, S Kurjatko, M Mamonová, J Hudec


Detoxification of preservatives: Tri-n-butyltin oxide as a biocide
1982 - IRG/WP 1156
T E Dudley-Brendell, D J Dickinson


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


The present classification of wood degradation factors
1994 - IRG/WP 94-10071
The revised version of classification of wood degradation factors is presented after discussion and remarks sended by IRG-Members. The classification contains the biotic and abiotic factors in two aspects: etiological and symptomatical....
J Wazny


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Resistance of Alstonia scholaris vestures to degradation by tunnelling bacteria
1992 - IRG/WP 92-1547
Electron microscopic examination of vessels and fibre-tracheids in the wood of Alstonia scholaris exposed to tunnelling bacteria (TB) in a liquid culture showed degradation of all areas of the secondary wall. The highly lignified middle lamella was also degraded in advanced stages of TB attack. However, vestured pit membranes and vestures appeared to be resistant to degradation by TB even when oth...
A P Singh, T Nilsson, G F Daniel


Borate thermal treatments
1992 - IRG/WP 92-3715
Green, partially seasoned (air-dried, steam conditioned), or kiln-dried southern pine timbers were treated thermally using 15% disodiumoctaborate tetrahydrate solution. After treatment, sections were stored under non-drying conditions to allow for diffusion. Results showed that effective treatment meeting the AWPA minimum retention (0.17 B203 pcf [2.72 kg/m³] in the outer inch) and penetration (2...
H M Barnes, R W Landers, L H Williams


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Corrosion of fasteners in heat-treated wood – progress report after two years’ exposure outdoors
2005 - IRG/WP 05-40296
The corrosion of common fastener materials now in use - mild steel, zinc-coated steel, aluminium and Sanbond Z-coated steel – has been evaluated after two years’ exposure outdoors in untreated and heat-treated spruce (Picea abies) respectively. Spruce from South-western Sweden was used. The heat-treatment was carried out in Finland according to the ThermoWood process at a maximum temperature ...
J Jermer, B-L Andersson


Accelerated ageing of preservatives in treated wood
1988 - IRG/WP 3476
New preservatives are tested in the laboratory and often in field tests before they are used commercially. Some preservatives, however, tested in the laboratory do not show the expected stability when used in service. The differences between laboratory tests and practical use can never be completely eliminated but must be minimized as far as possible by relevant testing methods. Studies of the eff...
M-L Edlund, B Henningsson, B Jensen, C-E Sundman


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


The effect of didecyldimethylammonium chloride on growth of different strains of mould fungus Gliocladium roseum
1995 - IRG/WP 95-10105
The tolerance and degrading ability of different strains of Gliocladium roseum towards didecyldimethylammonium chloride (DDAC) were studied. All four of the strains of Gliocladium roseum were tolerant to DDAC and after their growth on amended malt agar, the retention of DDAC in the medium was reduced....
Yu Zheng, J N R Ruddick