Your search resulted in 222 documents. Displaying 25 entries per page.


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


Improvements of stability and durability of beechwood (Fagus sylvatica) by means of treatment with acetic anhydride
1991 - IRG/WP 3645
In the present investigations, beechwood (Fagus sylvatica) was treated with non-catalysed acetic anhydrid at 120°C and some physical- and biological parameters of the treated wood were compared with those of non-treated wood. The radial and tangential shrinkage and swelling, respectively, and the absorption capacity of the acetylated wood against moisture is considerably lower. The durability aga...
H Militz


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Effect of alkaline phenolic resin adhesive on the stability of preservatives incorporated into the glue-line of plywood
1991 - IRG/WP 3650
Stability of preservatives was determined by gaschromatographic analysis when they were applied to glue-line treatment of plywoods. Among organophosphorous insecticides, emulsified forms of chlorpyrifos, dichlofention and diazinon were more stable than others. Fenitrothion, pyridafenthion and phoxim were not practically acceptable as emulsifieable forms due to the relatively low recovery rates aft...
S Fushiki, Y Katuzawa


Effect of boron compounds-furfuryl alcohol treatment of wood on dimensional stability, termite resistance and boron leachability
2001 - IRG/WP 01-40195
Sapwood blocks of Japanese cedar (Cryptomeria japonica) and Caribbean pitch pine (Pinus caribaea) measuring 20 (tangential) x 20 (radial) x 10 (longitudinal) mm were impregnated with furfuryl alcohol (FFA) by a vacuum-diffusion process followed by curing under heating. Boron compounds (boric acid, ammonium borate and ammonium biborate) were mixed in the impregnation solution of FFA. Anti- swelling...
S K Ozaki, M K Yalinkilic, Y Imamura, M F Souza


Influence of different resin treatments on the dimension stability of wood
1997 - IRG/WP 97-40090
The dimension stability of wood is considered to be an important contribution to its durability and its performance in practice. A number of different treatments have been developed to improve the dimension stability of wood. One applied method is the treatment of wood with monomers or resins. The application of appropriate impregnation conditions seemed to be essential to enhance the efficiency o...
M Sailer, A O Rapp


The Protection of Wood with Oxy-aluminium Compounds
2002 - IRG/WP 02-30286
Wood inorganic composites (WICs) containing aluminium compounds were developed and tested in relation to some essential requirements of preservative treated wood. Four different oxy-aluminium treatments were developed and identified according to the final insoluble compounds formed (sodium aluminate, aluminium hydroxide, magnesium aluminate and aluminium borate) in wood. Vacuum impregnation or dou...
F A Ximenes, P D Evans


Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS
2000 - IRG/WP 00-20201
Beside the biological effectiveness the approval of a chemical wood preservative requires also techniques for the analytical determination of active ingredients in different matrices. Fulfilling of the last requirement is particularly difficult in the case of impregnated timber treated with wood preservatives containing organic compounds. This paper describes a procedure for the determination of t...
P Jüngel, J Wittenzellner, E Melcher


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


The identification of organic compounds in wood using thermal desorption GC-MS - possibilities and limitations
2001 - IRG/WP 01-20224
There is a clear need for the analytical characterisation and identification of organic compounds and their derivatives in different phases especially in timber. In this context the paper describes a rapid and powerful gas chromatographic method for the determination of insecticides, biocides and "other" organic substances in treated and/or modified wood. The main advantage of this procedure is th...
P Jüngel, E Melcher


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


The use of natural and synthetical tannins to improve the dimensional stability and durability of beechwood (Fagus sylvatica)
1993 - IRG/WP 93-30016
Synthetical tannins and natural extractives of oak, spruce and chestnut have been combined with different fungicides to make the wood more dimensionally stable and more durable. The anti-shrink-efficiency and the improvement of the durability of different synthetical and natural tannins have been evaluated. The results make clear, that an application of the mentioned agents for common use cannot b...
H Militz, W J Homan


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Improvement in dimensional stability against water of the main Spanish timbers impregnated with water repellent organic protectors
1988 - IRG/WP 3468
The study reported the increase of dimensional stability against water of the main Spanish timbers, both broadleaved and coniferous, after impregnation in the autoclave with organic protector, with contains 33.3% water repellent waxes and resins. The proposed Spanish standard, U.N.E. n° 56541 is used, where dimensional stability of the impregnated wood is expressed as a% of that of the non-impreg...
J A Rodríguez Barreal


Ammoniacal wood preservatives for use in non-pressure treatment of spruce and aspen poplar. Part 2
1984 - IRG/WP 3274
A series of thermal diffusion treatments were carried out on unseasoned white spruce (Picea glauca (Moench) Voss) lumber and air dry aspen poplar (Populus tremuloides Michx.) timbers using an ammoniacal copper arsenate wood preservative. Under the specific conditions described, certain charges of lumber met the present Canadian Standards Association Wood Preservation Committee's requireme...
C D Ralph, J K Shields


The quantitative determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using TD-GC-MS
2001 - IRG/WP 01-20223
Last year we presented the paper (IRG/WP/00-20201) "Determination of N-cyclohexyl-diazeniumdioxide (HDO) containing compounds in treated wood using GC-MS". Based on the intensive discussion at the meeting, the first experiences made with the calibration of the system for this application will be reported. For the quantitative determination of N-cyclohexyl-diazeniumdioxide in treated wood, milled m...
P Jüngel, J Wittenzellner, E Melcher


Stability, performance and distribution of propiconazole (R 49362) in acceleratedly aged wood
1991 - IRG/WP 3647
The permanency of propiconazole (R 49362 - WOCOSENÔ technical - Janssen Pharmaceutica) in wood was examined in an 18 month storage test, an evaporative ageing study (EN 73), a volatilization stress experiment, and water-leaching studies (EN 84). The biological efficacy against two brown rot fungi: Coniophora puteana BAM Ebw. 15 and Gloeophyllum trabeum BAM Ebw. 109 was assessed according to the E...
A R Valcke, M Stevens


Durability of Wood/Plastic Composites Made From Parthenium species
2002 - IRG/WP 02-40225
Previous study indicated that the natural chemical constituents of the guayule plant (Parthenium argentatum) improved some durability properties of wood when it was treated with resin extracted from guayule. At present, there are about a dozen species of Parthenium growing in the North American continent. P. argentatum is the only species with harvestable amounts of the rubber latex. Other specie...
P Chow, F S Nakayama , J A Youngquist, J H Muehl, A M Krzysik