Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur