Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The effect of nanozycosil on the water absorption and dimensional stability of Beech wood
2012 - IRG/WP 12-40606
Zycosil is a clear penetrating water repellent. This product works by penetrating into the substrate and modifying the surface tension to inhibit water intrusion. Beech wood (Fagus orientalis) was modified by treatment with nanozycosil. Then water absorption and dimensional stability in terms of volumetric swelling percent and anti-swelling efficiency were determined and found to be improved on t...
M Ghorbani, F Bavaneghi


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Effect of Nano-Wollastonite on Water Absorption in Particleboard
2014 - IRG/WP 14-40662
Effects of wollastonite nanofibers on physical properties of particleboard were studied. Nano-wollastonite (NW) was applied at 5, 10, 15, and 20 g/kg, based on the dry weight of wood-chips, and compared with control specimens. Two application methods of NW were used: surface application (SA), and internal application (IA). Density was kept constant at 0.68 g/cm3 for all treatments. Tests were carr...
S Karimi, H Reza Taghiyari, A Karimi, P M Tahir, J Abdul Halip


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Leachability and Dimensional Stability of Nanosilver-Steamed Densified Poplar
2014 - IRG/WP 14-40684
This study was aimed to investigate leachability and dimensional stability of nanosilver impregnated poplar (Popolus alba), steamed before hot compression. Wood samples were impregnated with nanosilver suspension (200 and 400 ppm) under pressure of 4 bar for 20 minutes. Steam treatment was carried out at 150°C for 2 hours. Then samples were compressed (33%) radially in a hot press at 170°C for 3...
G Rassam, A Talaei, A Ahmadi


The effect of acetylation on physical properties of beech (Fagus orientalis) and Alder (Alnus subcordata) wood
2016 - IRG/WP 16-40759
In this study the effect of acetylation on physical properties such as water absorption, volumetric swelling and anti-shrink efficiency (ASE) of beech and alder were investigated. After 24 hours soaking in acetic anhydride, in order to achieving two surface of weight gains, acetylated samples were heated in oven at 120 0C for 90 and 360 minutes. Then water absorption and dimensional stability in...
M Akhtari, M Arefkhani


Water absorption characteristics of CLT
2017 - IRG/WP 17-40817
CLT is initialism of Cross Laminated Timber. CLT is generally large-sized panel which can use many woods efficiently, so it is attracted attention recently in Japan. Therefore, many studies about CLT are carried out. However, there are few studies about durability of CLT. Avoiding water infiltration is important for durability of wooden building. CLT has many edge-glued points which has risk of w...
D Yokoi, H Ishiyama, Y Hirano


Short-term absorption of water and coatings on thermally modified blue-stained spruce wood
2023 - IRG/WP 23-40984
The importance of wood has been increasing in the last decades. Among conifers, predominantly spruce (Picea abies) wood is often used in building constructions in Europe. Namely for construction and facades of buildings, decking and fences. Due to the increased public concerns about biocides, alternative techniques for protection, such as thermal modification and protection by construction, are ga...
R Hasanagic, M Bahmani, M Humar, L Fathi, L Cai


Evaluation of the water exclusion ability and inherent bioactivity of heartwood against decay in Japanese and European wood species via above-ground exposure and water absorption tests
2024 - IRG/WP 24-40998
The natural durability of wood has been thought to mainly depend on bioactive extractives and the water exclusion ability. To clarify the contribution of each factor to wood durability, above-ground exposure tests were conducted on Japanese and European wood species. A double-layer test was carried out using heartwood specimens of four wood species, i.e., Japanese cedar, Japanese cypress, Scots pi...
T Osawa, R Noda, K Yamamoto


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Fungal and bacterial attack of CCA-treated Pinus radiata timbers from a water-cooling tower
1991 - IRG/WP 1488
Transmission electron microscopy of decaying CCA-treated Pinus radiata timbers from an industrial water cooling tower showed presence of a thick biofilm covering some areas of the wood. The biofilm contained various morphologically distinct forms of microorganisms embedded in a slime. The study provided evidence of the activity of soft rot fungi and tunnelling and erosion bacteria in wood cells. T...
A P Singh, M E Hedley, D R Page, C S Han, K Atisongkroh


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 2nd Interim Report
1981 - IRG/WP 477
Three reference wood species - Alstonia scholaris, Fagus sylvatica and Pinus sylvestris, untreated and treated with 3%, 6% and 10% CCA and CCB solutions were supplied to all participants for submergence at local sites. Regular examination of samples is being carried out - 6 months, 12 months and then annually for 7 years....
R A Eaton


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley


Leaching of components from water-borne paints and fungitoxic effects
1995 - IRG/WP 95-20062
Water-borne model paints, acrylics and alkyd emulsion paints, of known composition were leached according to a procedure modified in accordance with ASTM 6271.1. The effectiveness of fungicidal compounds in the painted specimens before and after leaching was evaluated with a biotest in which Penicillium brevicompactum was used as a test fungus. The leaching of the fungicide Troysan Polyphase accor...
J Bjurman