Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Identifying compatible waterborne timber preservatives and fire retardants for use in a VPI system: a practical approach
2023 - IRG/WP 23-30796
To enhance the use and suitability of timber in all applications in both exterior and interior settings, timber typically needs to be treated with a preservative and/or a fire retardant chemical. Combining fire retardants with preservatives into a single treatment process has been a long-term aim of researchers in the timber preservative industry because of the significant logistic and economic ad...
R Robinson, S Meldrum


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Wood preservation in Poland
2004 - IRG/WP 04-30362
Dynamic growth of market demand for wooden elements and articles, generated in Poland increase of interest in industrial preservation. Today, Poland is a substantial producer and exporter of wood made products. Majority of exported wood - approximately 70% - is scotch pine (Pinus silvestris L.), which, due to its natural durability, requires preservation....
A Kundzewicz


Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix


Wood preservatives: Field tests out of ground contact. Brief survey of principles and methodology
1976 - IRG/WP 269
This paper contains the following spots: 1.: The general need for field tests. 2.: Interests and limits of field tests in ground contact. 3.: Various methods in use for out-of-ground contact field tests. 4.: Fungal cellar tests are they an alternative to above-ground decay exposure tests? 5.: Conclusions....
M Fougerousse


A suggested method to test the toxicity of wood preservatives towards the house longhorn beetle
1977 - IRG/WP 275
This method was developed in the Institute for Wood Technology in Sarajevo, Yugoslavia and is used to get quick information on the toxicity of wood preservatives against house longhorn beetle (Hylotrupes bajulus). The method can be used for superficially treated or deeply impregnated wood blocks, and by using small or normal size test material it can be used as a laboratory or field test, and also...
N Vidovic


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Environmental status of wood preservation in the UK
1994 - IRG/WP 94-50018
The environmental status of wood preservatives and treated wood in the UK is summarised. The current legislatory position with respect to approvals, supply, use and waste disposal is considered. The bibliography at the end of this paper contains details of all publications referred to together with other relevant information although this cannot be exhaustive....
M Connell


Manual of a mini treating plant for waterborne preservative treatment of timber and bamboo
1999 - IRG/WP 99-40130
This contributional article includes machinaries and equipments necessary for a small wood treating plant for the pressure treatment of tim bers with waterborne preservatives along with the cost and design. The preservative treatment limitations, treatment schedules and specifications for different products have been described. The cost of a mini treating plant will be 6,00,000 Tk. (13,000 US$), s...
A K Lahiry


Registration and approval of wood preservatives in Australia and New Zealand
2001 - IRG/WP 01-50166-06
Wood preservatives are treated as agricultural chemicals in Australia and, at the time of writing, as pesticides in New Zealand. Antisapstain products are currently considered to be agricultural chemicals in New Zealand while wood preservatives in the future will be considered as hazardous substances under the Hazardous Substances and New Organisms Act when this Act is fully implemented. They are ...
H Greaves


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States. The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...
J Habicht, D Häntzschel, J Wittenzellner


Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Third update and first report
1996 - IRG/WP 96-10174
At the 24th annual meeting of IRG in Orlando, USA, in May 1993 an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives, copper-chrome-arsenic (CCA) and copper naphthenate (Cu-Na) against the subterran...
J R J French


A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli


Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan


Laboratory decay test of Burmese in and kanyin treated with three wood preservatives
1982 - IRG/WP 3210
Laboratory decay tests were performed on samples of In (Dipterocarpus tuberculatus Roxb.) and Kanyin (Dipterocarpus alatus Roxb. and Dipterocarpus turbinatus Gaertn f.) pressure treated with three wood preservatives - copper arsenic additive (CAA - a variation of ammoniacal copper arsenate), Arquad C-33 (a waterborne quaternary ammonium formulation), and tributyltin acetate (TBTA) dissolved in eth...
J N R Ruddick, R S Smith, A Byrne


Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt


Protocol for evaluation and approving new wood preservative
1985 - IRG/WP 2159
M E Hedley, J A Butcher


A new concept of oxalic acid biosynthesis in physiology of copper-tolerant brown-rot fungi
2001 - IRG/WP 01-10394
Recently, a wide variety of roles of oxalic acid (oxalate) in wood decay systems have been receiving much attention. Copper tolerance of wood-rotting basidiomycetes has been believed to be due to the detoxification of copper wood preservatives by oxalate produced by these fungi. However, biochemical mechanism of oxalate biosynthesis in relation to physiology of wood-rotting fungi has not been eluc...
E Munir, T Hattori, M Shimada


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson