Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Termite resistance of Malaysian and exotic woods with plantation potential: Laboratory evaluation
1998 - IRG/WP 98-10280
The resistance of selected Malaysian woods to attack by the representative aggressive subterranean termite Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae) was evaluated in four-week, no-choice laboratory tests. This is part of an ongoing effort between the Forest Research Institute Malaysia and the University of Hawaii to document the termite resistance of Malaysian timber species of po...
J K Grace, A A H Wong, C H M Tome


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Biocidal screening method of wood extractives by a direct use of cellulose TLC plate
2001 - IRG/WP 01-20226
Most of the methods to evaluate the biological durability of woods have focused on decay fungi and termite as deteriorating organisms and it is well known that one of the most important factors affecting the biological characteristics of wood is extractives. Bioassays for evaluating the biological activities of wood extractives have been mainly conducted with treated filter papers for termites or ...
R Yusiasih, T Yoshimura, T Umezawa, Y Imamura


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


Work programme of CEN/TC 38 (May 1995) - Durability of wood and derived materials
1995 - IRG/WP 95-20069
Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes; - the test methods (wood preservatives as treated wood and wood based materials) and inte...
R Hüe


Natural resistance of Bamboo (Bambusa sp.) to marine wood-borers in Goa waters (India)
1993 - IRG/WP 93-10032
The paper deals with the natural durability of Bambusa sp. against the attack of marine wood-borers in Goa waters. Test specimens of this species were completely destroyed within a short period of nine months due to severe attack of borers indicating its very low natural resistance. Wood-borers involved were Martesia striata (Linnaeus), Nausitora hedleyi Schepman and Lyrodus pedicellatus (Quatrefa...
L N Santhakumaran, S G Sawant


Relationship of wood durability and extractives
2003 - IRG/WP 03-10493
The durability of the following five wood species, Zelkova carpinifolia, Ulmus glabra, Pterocarya fraxinifolia, Carpinius betulus and Acer laetum, were studied. Wood blocks were exposed to Coriolus versicolor under laboratory conditions according to DIN 52176 standard. After 16 weeks incubation the heart wood of Z carpinifolia showed 2,19 % weight loss, U glabra 41,69 %, C betulus 45,64 %, A laetu...
S M Kazemi


Wood preservation in Portugal
1985 - IRG/WP 3325
This report deals with the forest potential of Portugal and its timber industry and outlines the evolution of wood preservation in the country. The main hazards to timber in service are noted and the timbers used classified according to their natural durability and treatability. The wood preservatives used are detailed with estimates of the total consumption of the different types. Addresses are l...
D De Sousa Castro Reimão, R Cockcroft


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Evaluation of wood durability by laboratory test - A new equation to predict wood durability
2001 - IRG/WP 01-20230
To estimate the wood durability in a short term, periodical weight determination was carried out in a laboratory test. This test provided the results comparable to those of the field test and the fungus cellar test, but it required much more jobs in comparison to the usual accelerated laboratory test. To save the time and jobbing for this method, a new equation was devised from simple two assumpti...
I Momohara, K Yamamoto


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury