Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


Accelerated H3 above-ground decay testing
2013 - IRG/WP 13-20520
An above-ground H3 fungal field trial was installed at two sites in Australia and one in New Zealand, as well as in two Accelerated Field Simulators. The aim was to find a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter H3 retentions were installed, as first results suitable for registration occur when these reach 70% soundness. Twel...
L J Cookson, D Page, T Singh


Critical moisture levels and mould resistance of five different wood treatments
2013 - IRG/WP 13-30632
Mould resistance of five different treatments were tested using two methods, a recently developed method for the determination of critical moisture levels of building materials (RHcrit), and ASTM D3273-94. The critical moisture level method exposed samples at 22 °C and 98, 92, 86 and 82% relative humidity (RH) for 12 weeks. ASTM D3273-94 was performed at 29 °C and about 95% RH. Treatments c...
G Bok, P Johansson, A Ekstrand Tobin, S Bardage


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


Effects of UV Radiation on Melanization and Growth of Fungi Isolated from Weathered Wood Surfaces
2015 - IRG/WP 15-10842
This research tests the hypothesis that fungi isolated from weathered wood will respond to elevated levels of UV radiation by increasing their melanin production. To test this hypothesis, we measured the melanin production and mycelial color of Aureobasidium pullulans and Cladosporium cladosporioides, before and after the fungi were grown under artificial UV, visible light and complete darkness. T...
V A Hernández, P D Evans


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Application of diverse hyperspectral imaging systems for evaluation of heritage objects
2020 - IRG/WP 20-10971
Advanced imaging techniques are able to non-invasively characterize, monitor and evaluate the impact of conservation treatments on cultural heritage (CH) objects. In this specific field, hyperspectral imaging (HI) allows non-destructive characterization of materials by identifying and characterizing colouring agents, binders and protective coatings as constituents of an object’s original constru...
J Sandak, A Sandak, L Legan, K Retko, M Kavčič, J Kosel, F Poohphajai, R Herrera Diaz, V Ponnuchamy, N Sajinčič, Č Tavzes, P Ropret


Dynamics of fungi colonization on the surface of Scots pine wood during natural weathering in different European climate zones
2022 - IRG/WP 22-10984
Wood The presence of fungi leads to biomaterial decay and/or changes in aesthetical appeal. The start of fungi colonization as well as the following growth on wood are primarily influenced by four factors: ambient temperature, moisture history of the object, access to oxygen, and intrinsic properties of the exposed wood, considered here as a source of nutrients for microorganisms. A prevalence of ...
F Poohphajai, O Myronycheva, O Karlsson, L Rautkari, J Sandak, A Sandak


Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund


Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...
J K Carey, D F Purslow, J G Savory


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


Improvements of monitoring the effects of soil organisms on wood in fungal cellar tests
1996 - IRG/WP 96-20093
Accelerated testing the durability of preservative treated timber in a so called "fungal cellar" or "soil-bed" to evaluate its performance in ground contact is widespread practice. In order to obtain a more accurate and reproducible estimate of preservative performance, several institutes, among them the BAM in Berlin, have routinely carried out static bending tests in addition to visual examinati...
I Stephan, S Göller, D Rudolph


Testing of wood preservatives against marine borers (Part 1). Method of testing wood preservatives against marine borers (Part 2)
1971 - IRG/WP 37
P C Trussell, C C Walden


Improved techniques designed for evaluation of fungicides in soil for control of dry rot fungus Serpula lacrymans
1985 - IRG/WP 2238
Improved techniques provide a laboratory method for the evaluation of chemicals in soil for control of dry rot fungus Serpula lacrymans. Results with their application to three chemicals were reported. These techniques are useful to eliminate chemicals lacking the necessary toxicity and weatherbility for dry rot control when the chemicals have been applied to the soil....
M Takahashi, K Nishimoto


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


Detection of feeding behaviour of termites using AE monitoring
1991 - IRG/WP 1514
Using acoustic emission (AE) monitoring, the feeding activity of the termite inhabiting a wood specimen was investigated. The amplitude and the rate of AE from the specimen of Coptotermes formosanus Shiraki was larger than that of Reticulitermes speratus Kolbe. The AE event rate was higher in the specimen with soldiers than without soldiers. The AE event rate decreased according to the resistance ...
Y Imamura, M Tokoro, M Owada, Y Fujii, M Noguchi


A medium for mass culturing of a bamboo boring beetle Dinoderus minutus Fabricius
1983 - IRG/WP 1182
The bamboo is a traditional product of Japan. But its susceptibility to insects is one of the most important problems. The author has found that for the determination of the effectiveness of insecticides it is very easy to obtain sufficiently numerous adults of Dinoderus minutus by using Buckwheat Cake. The Buckwheat Cake is prepared with buckwheat flour and thin paper. The author has previously f...