IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 51 documents. Displaying 25 entries per page.


Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


Insect growth regulators: modes of action and mode of action-dependent peculiarities in the evaluation of the efficacy for their use in wood preservation
1997 - IRG/WP 97-30155
Up to now, the insecticides used in wood preservation are either of more or less non-specific mode of action - like boron - or of neurotoxic mode of action - like chlorinated hydrocarbons, carbamates and pyrethroids. The active ingredients actually used are primarily mirroring the progress in active ingredient research in plant protection. The methods of testing of the insecticidal efficacy of woo...
M Pallaske


Screening test methods with termites as first laboratory evaluation of new active substances for wood preservation
1995 - IRG/WP 95-10135
European test methods (EN) with termites have been compared with long-standing experience from screening test methods in the laboratory of Eberswalde. The results are discussed in terms on the possibility of using screening test methods as the first laboratory evaluation of new active substances in wood preservatives. The advantages and disadvantages of these methods are considered. Only a small a...
W Unger


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Leachability of active ingredients from some CCA treated and creosoted poles in service. A progress report after 10 years testing
1990 - IRG/WP 3627
CCA K33 TYPE B treated or creosoted poles, 10 pieces of each treatment type, have been monitored from the treatment plant to an electricity line, which was build up in Southern Finland in 1978. Preservative retention was determined by taking borings at four different levels: 1.5 m from the top end, 1 m above ground line, ground line and 0.5 m below ground. Determinations were made before setting u...
A J Nurmi


Measuring Soil Respiration as a New Approach to Describe the Interaction Between Wood (Treated and Untreated) and Microbiologically Active Soil
2006 - IRG/WP 06-20344
Soil respirometry was employed to examine the relationship between both the performance of copper organic preservatives in contact with and the amount of carbon dioxide evolved from soil and the effect of wood treated with preservatives on carbon turnover in soil. Wood was treated with a range of copper organic preservatives intended for use in ground contact as well as an organic preservative in...
I Stephan, W Mierke


Ionic liquids with organic and inorganic anions as highly active wood preservatives
2006 - IRG/WP 06-30411
Quaternary ammonium tetrafluoroborates, nitrates(V), propionates, acetates and formates with alkoxymethyl substituents were prepared and tested on wood destroying and sapstaining fungi. These new compounds are ionic liquids (ILs), which penetrate very well into Scot pine wood. Alkoxymethyldecyldimethylammonium tetrafluoroborates and nitrates(V) show better microbial activity against Coniophor...
J Zabielska-Matejuk, A Skrzypczak


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


Emission Rates of Active Substances from Preserved Wood in Use Class 3
2008 - IRG/WP 08-50256
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes scenarios for preserved wood (e.g. cladding on a house), in which the predicted environmental concentration (PEC) in soil is calculated, using an emission rate for the active subs...
E F Baines


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Use of biological and low toxicity products against subterranean termites
2009 - IRG/WP 09-20410
The climatology of Mediterranean countries is favourable to the development of termites that cause important damage to wood structures in both furniture and buildings. Until a few years ago the treatment for this type of insect was based on the impregnation of the wood with chemical products. The use of these chemicals is now being restricted in Europe since the publication and harmonization of n...
M T Troya, M J Prieto, F Rubio


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


First report on the termiticidal activity of extracts of Annona squamosa (Annonaceae) seeds and on its active constituent squamocins
2012 - IRG/WP 12-30605
Termites inflict severe damage on wood commodities and impede usage of several forest species. The biological metabolites could potentially replace synthetic termiticidal products which are becoming more restricted to use. Annona squamosa is well known for its edible fruits - tropical custard apple. Annonaceous tetrahydrofuran acetogenins have attracted much interest due to their broad range of bi...
T S Djenontin, N Amusant, P H Ducrot, D C K Sohounhloué, D Pioch


Survival of Bursaphelenchus xylophilus exposed to different active ingredients of wood protectors
2013 - IRG/WP 13-10802
The pine wilt nematode (PWN) Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken....
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Fire protection of wooden facades in Norway
2015 - IRG/WP 15-40710
Wood products are experiencing a renaissance as construction material in Europe due to their environmental benefits. In Norwegian building design however, timber has always played an important role but has had its limitations in urban architecture. One of the reasons is a high demand to fire safety in dense house building and multi-story buildings. Though novel construction methods and fire safety...
U Hundhausen, K-C Mahnert


Simulation of surface climate and mould growth on wooden façades
2016 - IRG/WP 16-20585
The weathering of wooden surfaces is normally caused by mould growth, lignin deterioration and leaching of extractives. For well insulated buildings, the effect of the interior climate on the outer surface is small and sometimes negligible. This paper describes simple models for surface temperature and moisture conditions on a wooden façade that can further be used to model weather degradation an...
T K Thiis, I Burud, D Kraniotis, L Ross Gobakken


Prediction of service life – does aesthetic matter?
2017 - IRG/WP 17-20618
Building structures should be designed in order to satisfy requirements regarding safety, serviceability, durability and aesthetics, assuring proper structure performance along the entire service life. For that reason it is essential to understand overall deterioration mechanism at levels of element, component, façade and entire building. This work focuses specifically on the façade aesthetical ...
A Sandak, J Sandak


Colour changes in unpainted wooden façades – Fifty Shades of Grey
2018 - IRG/WP 18-10903
In Norway the use of weathered unpainted, wooden façades has increased in popularity the last 20 years, both in single family houses as well as in multi-story and non-residential buildings. The benefit of using unpainted wood as façade material can be several: low maintenance costs, low environmental impact and low carbon footprint as well as contemporary and trendy aesthetic appearance. The va...
K Zimmer, L R Gobakken, O Flindall, M Nygaard


Simulation and visualization of aesthetic performance of bio-based building skin
2018 - IRG/WP 18-20633
Performance of 120 selected façade materials provided by over 30 industrial and academic partners is under evaluation. The experimental data, acquired during BIO4ever project duration are used for development of the numerical models simulating the material degradation in a function of time and exposure. The weather data calculated according to the ASHRAE 2013 database allows numerical simulation ...
J Sandak, A Sandak, P Grossi, M Petrillo


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Using satellite-retrieved soil moisture data to model the decay risk of in-ground timber
2022 - IRG/WP 22-20689
Satellite-derived soil moisture data from the Soil Moisture Active Passive (SMAP) was extracted for a 9 x 9 km point grid over Europe. The data was then used as input to a dose-response wood decay model based on terrestrial microcosm (TMC) tests. The resulting hazard map plotted dose as an indicator of in-ground wood decay based on differences in annual temperature and soil moisture characteristic...
P B van Niekerk, M Schönauer, B N Marais, C Brischke


Analytical retentions of active ingredients in H2F treated framing over a 12-year period
2023 - IRG/WP 23-20702
The H2F hazard class in Australia was developed to treat internal framing timber with a surface application of an insecticide, to control mainly termites. Two of the actives approved in AS 1604.1-2010 (and subsequent revisions) for this hazard class are bifenthrin and imidacloprid. The penetration zone of both actives is 0 – 2 mm from the wood surface. Radiata pine sapwood framing timber wa...
A Siraa


Previous Page | Next Page