Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 5. Treatment of Sitka spruce and Scots pine
1999 - IRG/WP 99-40136
The suitability of the MPP Process for CCA treatment and accelerated fixation of species other than Radiata pine was assessed by pilot plant trials on UK-grown Sitka spruce (Picea sitchensis) and Scots pine (Pinus sylvestris). Pressure and vacuum kickbacks of spruce (14 l/m3) and Scots' pine (122 l/m3) were both substantially lower than that generated during treatment of radiata pine (369...
M E Hedley, K Nasheri, G Durbin


The leachability, biological resistance, and mechanical properties of wood (Pinus sylvestris L.) treated with CCA and CCB preservatives
1999 - IRG/WP 99-30207
Scots pine (Pinus sylvestris L.) specimens treated with CCA and CCB preservative solutions (1.0%) were subjected to several fixation processes and leached elements from the specimens were determined. In addition, the specimens exposed to different fixation temperatures were subjected to soil-block test using two brown-rot fungi and one white-rot fungus in order to investigate the effects of fixati...
S N Kartal


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


The formation of organotin carboxylates in bis(tributyltin) oxide - treated Pinus sylvestris sapwood
1990 - IRG/WP 3618
Tributyltin compounds have been successfully used for many years as wood preservatives, although their chemical nature in timber have not been fully elucidated. This study by 119Sn and 13C NMR spectroscopy has shown that, on impregnation into Pinus sylvestris sapwood, bis(tributyltin) oxide, (Bu3Sn)2O, is rapidly converted to tributyltin carboxylates, Bu3SnOCO·R, via reaction with components of t...
S J Blunden, R Hill


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Kinetic modelling of adsorption of quaternary ammonium compounds by Scots pine wood sawdust (Pinus sylvestris L.)
2005 - IRG/WP 05-30369
The adsorption of new quaternary ammonium compounds from aqueous solutions onto Scots pine wood (Pinus sylvestris L.) sawdust was studied. The pseudo first- and second- order kinetic models were used for the mathematical description of the sorption dynamic process of QACs onto wood. The highest correlation coefficients were obtained for the pseudo-second order kinetic model, those suggest that che...
J Zabielska-Matejuk


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Sub-group on Basidiomycete tests: Proposals for Sub-group programme of work
1979 - IRG/WP 2127
During the IRG 10 Meetings in Peebles, Scotland in September 1978, it was resolved to establish within Working Group II a sub-group on testing wood preservatives against basidiomycete fungi. The terms of reference and scope of the sub-group's activities were to be determined by consensus among members who registered an interest. Dr A F Bravery (PRL, UK) was asked to act as co-ordinator. D...
A F Bravery


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Absorption of inorganic salts solutions. Retentions of inorganic salts. Fire retardants
1990 - IRG/WP 3625
The study aims evaluated the impregnation capacity using fire retardants on woods with differents densities. At the same time, impregnation with several fire retardant salts were carried out in order to obtain their absortion and retention in wood....
A Garcia, J Navarro


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Tests on preservation of wood against marine borers
1976 - IRG/WP 417
The Instituto del Legno has carried out for some years a series of trials about the biodeterioration of wood in the sea. The investigations included the settlement and activity of marine borers, the natural durability of indigenous and tropical woods and the preservation of wood for marine use. This paper reports the trials on the effectiveness of some preservatives in protecting wood against mari...
A Gambetta, E Orlandi


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton