Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Radical changes in the requirements for more safe pressure impregnation in the Nordic countries in 1988
1990 - IRG/WP 3581
After introduction of quality control schemes and standards in the Nordic countries during the seventies, the first radical change of the standards and practice of work took place after pressure from the labor unions and authorities in 1988 and 1989 in Denmark and in Sweden. A new class of preservation with less retention for out of ground contact use was introduced, fixation times were prolonged ...
B Moldrup


A note on testing the efficacy of wood preservatives above ground
1995 - IRG/WP 95-20078
A number of test methods have been used to evaluate the performance of wood preservatives in above ground situations. These have included EN 113 tests following natural exposure weathering (NEWT), L-joint or T-joint tests, lap-joint tests, and decking tests. A new test referred to as the A-frame test has been developed and is under evaluation. This is based on a sandwich-type test in which a thin ...
G R Williams, J A Drysdale, R F Fox


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Practical consideration in developing an international hazard class standard: The hazards and risks
1996 - IRG/WP 96-20091
This paper discusses the concept of hazards and risks in relation to the way in which the hazard class philosophy may be used for international standardization. The difference between hazard and risk is considered as a basis for a simple classification of biological hazards for timber in use based upon its service environment. The paper proposes that the moderating influences within a service envi...
R J Orsler


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Permanence of permethrin and bifenthrin in framing timbers subjected to hazard class 3 exposure
2005 - IRG/WP 05-30383
End-sealed Pinus radiata specimens measuring 235 x 90 x 35 mm were treated using a modified Lowry schedule with permethrin or bifenthrin in white spirit to Hazard Class 2 (H2) retentions. After conditioning, the specimens were exposed at 45o on north facing racks near Melbourne (Australia). Samples of the specimens were taken before installation, and after three and six months exposure. Analyses o...
A C Hunt, D G Humphrey, R Wearne, L J Cookson


Towards a unified international hazard class system
1996 - IRG/WP 96-20081
Working party 2.5 on International Standardisation has set the development of a unified hazard class system as a short-term objective. This document is intended to stimulate the discussion required to work towards such a system. Two possible approaches are discussed, the compromise approach and the development of a basic system from first principles. For the second approach, the factors impacting ...
P I Morris


Evaluation of wood preservatives for Nordic wood preservation class AB
2002 - IRG/WP 02-30297
In the Nordic countries there are restrictions in the use of wood preservatives based on chromium and arsenic. For above ground use, class AB according to the Nordic system, only copper based preservatives are allowed in Sweden. Thus several new preservatives, copper based or metal free are now used. They have been approved by the Nordic Wood Preservation Council after passing laboratory tests ag...
M-L Edlund, J Jermer


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Emission Rates of Active Substances from Preserved Wood in Use Class 3
2008 - IRG/WP 08-50256
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes scenarios for preserved wood (e.g. cladding on a house), in which the predicted environmental concentration (PEC) in soil is calculated, using an emission rate for the active subs...
E F Baines


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Durability of modified wood in UC3 and UC4. Results from lab tests and 5 years testing in 3 fields
2011 - IRG/WP 11-40562
In 2005 an extensive test program including field tests was set up in order to obtain more data on the durability and long term performance of modified wood and semi-durable wood species. One of the main challenges for modified wood is to predict accurate service life time in UC3 (use class 3, above ground) and UC4 (use class 4, in soil or fresh water contact). So far, data from in-service condi...
M Westin, G Alfredsen


Evaluation of fungal infestation and decay in a simulated use class 3 situation (block test) after some years of exposure
2012 - IRG/WP 12-20487
The so named “block test” was designed as part of the assessment methodology for testing the behaviour of natural and modified wood used under use class 3 (EN 335-2) conditions. The test was developed to expose the wood close to the ground to an environment with high humidity and high biological activity, but not in soil contact. The present study describes the evaluation of fungal infestatio...
A Gellerich, K Röhl, S Adamopoulos, H Militz


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Glueline fungicides in veneer based engineered wood products - results from laboratory work for the H1.2 hazard class in New Zealand
2012 - IRG/WP 12-30593
The use of glueline insecticides in plywood and laminated veneer lumber is commonplace in several countries. However, few glueline fungicides are registered for commercial use with previous work suggesting that achieving control of decay from the glueline is very challenging. This paper summarises two tests completed on Pinus radiata plywood with a new glueline fungicide comprising the active in...
A Siraa, K Day, P Lobb


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt