Radical changes in the requirements for more safe pressure impregnation in the Nordic countries in 1988
1990 - IRG/WP 3581
After introduction of quality control schemes and standards in the Nordic countries during the seventies, the first radical change of the standards and practice of work took place after pressure from the labor unions and authorities in 1988 and 1989 in Denmark and in Sweden. A new class of preservation with less retention for out of ground contact use was introduced, fixation times were prolonged ...
B Moldrup


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Scientific development for prolonging the service life of timbers by impregnating with creosote or organic solvent type preservatives in which additive has been incorporated
1977 - IRG/WP 382
Chemically impregnated wood has played a prominent part in the Telephone and Electricity Distribution Industry during the past century and there is no doubt that it will play an equally prominent part in the future. The reasons why wood poles and wooden, structures predominate, are that when adequately chemically impregnated with a recognised timber preservative to ensure the expected service life...
P R B D De Bruin


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Patent on the use of tannic acid and ferric chloride against marine borers, etc
1982 - IRG/WP 495
R Mitchell, T D Sleeter


Report of the meetings of the Refractory Timbers Sub-group, Rotorua, New Zealand, 15 & 17 May 1990
1990 - IRG/WP 3637
R J Murphy


Collaborative soft rot tests: Summary of comments on 'Proposals for a standardized soil burial test'
1971 - IRG/WP 202
J G Savory


New developments in wood preservation
1974 - IRG/WP 335
Most of the developments in wood preservation in recent years have been stimulated by changing circumstances, particularly the increasing interest in reducing hazards and environmental, pollution but also the serious difficulties that are now being encountered in obtaining economic supplies of established preservatives. There is perhaps a danger that new controls to reduce pollution dangers may be...
B A Richardson


A comparison of the effectiveness of a vacuum oven and a wind tunnel in the accelerated ageing of treated wood by evaporation
1989 - IRG/WP 2334
R J Orsler, G E Holland


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


In-situ pressure injection for preservation of rubber wood (Hevea brasiliensis Muel Arg.)
1992 - IRG/WP 92-3688
Rubber wood is widely used for the manufacture of furniture, doors for housing and packing cases. However in an untreated condition it is highley susceptible to sapstain and decay fungi and borers. Its utility gets considerably reduced if the wood is not treated well in time. Preservative treatment has to be given within the period of felling and transport to prevent not only loss of structural pr...
H S Ananthapadmanabha, V R Sivaramakrishnan


Analysis of organotin fungicides in wood preservative solutions and double-vacuum treated wood
1983 - IRG/WP 3250
A new analytical method using high-performance thin-layer chromatography (HPTLC), for the assay of organotin compounds in preservative-treated wood, is presented. The organotin compounds are extracted from the ground wood sample with a mixture of hydrochloric acid and ethanol. After HPTLC-separation, exposure of the thin-layer plate to ultraviolet light, and dipping of the plate into a 0.1% pyroca...
W Hintze, S V Ohlsson


Specific gravity and moisture content of particleboards treated with various chemicals
2005 - IRG/WP 05-40310
The aim of the study was to investigated the effects of particleboard treated with various chemical substances on specific gravity and moisture content The wood raw material used in the experiments were the mixture of coniferous wood [70%, Pinus brutia Ten., Pinus nigra Arn (Lamb.), Cedrus libani Ait.] and black poplar (30%, Populus nigra L.). In this mixture, barks have been accepted up to 5 per...
Ü C Yildiz, A A Var, H Kalaycioglu, S Yildiz


Final report on world survey of sap displacement impregnation of timber
1975 - IRG/WP 345
The present contribution to the World Survey of Sap Displacement Impregnation of Timber covers the information received since the presentation of the interim report to the 6th Annual Meeting of the International Research Group on Wood Preservation held in Vienna, 20th June 1974....
F B Shorland, C G W Mason


The influence of formulation on the behaviour of LOSP's during industrial impregnation of spruce
1986 - IRG/WP 3387
Evidence is presented that the comparative behaviour of two LOSP formulations during impregnation treatment of spruce cannot be predicted purely on the basis of their physical characteristics (viscosity, surface tension and contact angle) nor on the extent of their 'passive' penetration into pine sapwood....
L D A Saunders, D M Zuvencko


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Treatment of messmate (Eucalyptus obliqua L'Hérit) by double-diffusion: Preliminary report
1983 - IRG/WP 3234
Modified double-diffusion is suggested as a method of impregnation for mixed tropical hardwoods for certain types of ground contact use in less developed countries. Compared with vacuum/pressure impregnation, capital costs are low and little skill is needed for the operations involved. Treatment of messmate (Eucalyptus obliqua L'Herit) rounds involving pre-heating in water prior to their ...
F F K Ampong, C-W Chin


Improvement of liquid penetration of wood by precompression under appropriate conditions and recovery process
1993 - IRG/WP 93-40014
A new system for enhancing the penetration of liquid into wood using a precompression treatment was designed, and the effects of compressive deformation and recovery on liquid uptake were evaluated. Precompression of up to 60% under appropriate moisture and heat conditions effectively increased the penetration of liquid into refractory wood samples of practical sizes without producing any strength...
I Iida, Y Imamura


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


A behaviour of CCA penetration of fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications
2006 - IRG/WP 06-40346
A behaviour of CCA penetration of Bornmulleriana fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications was illustrated for the main flow directions by the experimental pictures....
I Usta, R Despot, M Hasan


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


Treating Eucalyptus tereticornis wood with boron: Optimizing treatment conditions
2005 - IRG/WP 05-40309
Even though Eucalyptus tereticornis wood is suitable for small timber purposes, being non-durable, it needs to be treated with preservative chemicals. As it is a heavy, hard and difficult to treat species, the possibility of using diffusible boron compounds was investigated. The present study explored the effect of impregnation conditions such as treatment schedule, concentration of treatment solu...
T K Dhamodaran, R Gnanaharan


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


Health hazards and environmental aspects when using Cu-HDO-containing wood preservatives in vacuum pressure plants
1993 - IRG/WP 93-50001-11
Apart from the biological efficacy of wood preservatives, the health and environmental aspects concerning the utilisation of wood preservatives, the use of treated timber and the disposal of impregnated wood are of high significance today. Therefore, information on a possible aerial concentration of wood preservatives, on the mobility of active substances in soil leached from treated timber in ser...
W Hettler, S Breyne, M Maier