IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 84 documents. Displaying 25 entries per page.


Laboratory evaluation of chlorothalonil formulation for stain and mold control on rubberwood and maple
1998 - IRG/WP 98-30175
We evaluated the efficacy of several chlorothalonil and carbendazim fungicides (F1 and F2), etc. in the control of mold and stain fungi on rubberwood and maple. The results showed that these formulations effectively inhibited the selected fungal species such as Aspergillus niger, Penicillium sp., Trichoderma sp. (P71H), Aureobasidium pullulans, Ceratocystis minor (C-188), Ceratocystis pilifera (RW...
Mingliang Jiang, T L Highley, L Ferge, T L Woods


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Termite resistance of Malaysian and exotic woods with plantation potential: Laboratory evaluation
1998 - IRG/WP 98-10280
The resistance of selected Malaysian woods to attack by the representative aggressive subterranean termite Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae) was evaluated in four-week, no-choice laboratory tests. This is part of an ongoing effort between the Forest Research Institute Malaysia and the University of Hawaii to document the termite resistance of Malaysian timber species of po...
J K Grace, A A H Wong, C H M Tome


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...
A P Singh, Yoon Soo Kim


Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods


Wharf-borer a threat to stored archaeological timbers
1992 - IRG/WP 92-1560
Increased interest in marine archaeology has occured in recent years. Stored waterlogged archaeological timbers have been shown to be degraded by physical and microbial agents. In recent years a new threat has been highlighted, namely the wharf-borer Nacerdes melanura (L.). The objective of this paper is to outline studies of the morphology, biology, life-history and carbohydrate digestion by this...
A J Pitman, E B G Jones, A M Jones, M Rule


Evaluation of chlorothalonil for stain and mould control on lumber
1992 - IRG/WP 92-3713
Chlorothalonil is a commercially important fungicide with many industrial and agricultural applications. It has a very low mammalian toxicity and is considered to be an environmentally benign material. This paper describes the laboratory evaluation of chlorothalonil as a wood antisapstain treatment. Chlorothalonil was tested as three formulation types - an emulsifiable concentrate (EC), a water-ba...
P E Laks, T L Woods, D L Richter


Efficacy of Didecyl Dimethyl Ammonium Chloride (DDAC), Disodium Octaborate Tetrahydrate (DOT), and Chlorothalonil (CTL) against Common Mold Fungi
2004 - IRG/WP 04-30338
The fungitoxic properties of four fungicides, alone and in combination, against four different mold fungi commonly associated with indoor air quality problems were evaluated on two different wood species and sheetrock. The fungicides were chlorothalonil (2,4,5,6-tetrachloroisophthalonitrile) (CTL) in a 40.4% aqueous dispersion, disodium octaborate tetrahydrate (DOT) in two different forms - a ...
J A Micales-Glaeser, J D Lloyd, T L Woods


Assessing the leachability of chlorothalonil and methylene bis thiocyanate from antisapstain treated radiata pine
1998 - IRG/WP 98-30176
Rain wash-off and leaching of antisapstain fungicides from wood may cause pollution of waterways and may also lead to a decrease in the efficacy of a formulation against fungal degrade as chemicals deplete from the timber surface. In the current study, the leachability of chlorothalonil (CTL) and methylene bis thiocyanate (MBT), the active ingredients of a commercial antisapstain formulation, was...
B Kreber, T L Woods


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Sampling and analysis of NeXgen-treated timber
1998 - IRG/WP 98-20134
Green sawn timber surfaces of the softwood Caribbean pine and the hardwood white cheesewood were treated by dipping, spraying, and precise spiking with the antisapstain product NeXgen. After storing for either two hours or two weeks, the treated surfaces were sampled by one of four alternative protocols, which included two involving a square wad sampling punch (one hit or six hits), one involving ...
M J Kennedy, D E Ferlazzo, T L Woods, M H Freeman


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Site characteristics impacting historic waterlogged wood: A review
2000 - IRG/WP 00-10344
Survival of waterlogged wood from hundreds and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depostional environment, have not been completely degraded. Although degradation patterns of various types of microbial wood decay have been studied in detail, the site parameters of the ...
B A Jordan, E L Schmidt


Application of non-destructive techniques (durometric and ultrasonic) to evaluate the degradation of woods in service by Gloeophyllum trabeum
2001 - IRG/WP 01-20220
In order to establish the degree of degradation of wood used in construction, it is necessary to employ non-destructive methods (ultrasonic, durometric, densitometric). In this study, ultrasonic and Pilodyn durometric techniques have been applied to try to establish parameters of relationship between the values obtained by both, for their immediate application to wood in service. As a method of re...
M T De Troya, L Palaia, A Navarrete, V Galvañ, R Molina, A Guijarro, J Camacho


Antisapstain field trials of NeXgen in New Zealand
1997 - IRG/WP 97-30145
This document covers the results of summer and winter log trials of NeXgen, an antisapstain formulation containing methylene bis thiocyanate plus chlorothalonil. Log billets (20 - 25cm diameter) were stripped of bark using a commercial maul debarker and antisapstain treated within 8 hours of felling by dip application. Billets were stored in a pole barn and assessed for internal sapstain and decay...
R N Wakeling, T L Woods, D R Eden, C M Chittenden, B Carpenter


Ultrastructure of Prumnopitys ferruginea wood from a buried forest in New Zealand
1991 - IRG/WP 1489
The buried wood of Prumnopitys ferruginea, a New Zealand native tree, was examined by scanning and transmission electron microscopy to investigate the extent to which the wood had deteriorated and the cause of its deterioration. Examinations showed that some deterioration of wood had occurred. Microscopy revealed a decay pattern similar to that produced by cavitation bacteria. Lenticular cavities ...
A P Singh, T Nilsson, G F Daniel


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Information from the COIPM wood group. (With Appendix: Préserver les matériaux en milieu marin sauvegarder l'environment marin telles sont la vocation et la mission du C.O.I.P.M.)
1989 - IRG/WP 4156
During the last COIPM Meeting, up to date information on cooperative work to test the resistance of plastic wrapping for pilings were submitted and discussed. In 1986 untreated wood samples wrapped with shrinkable polyolefin sleeves were submerged in 9 stations, situated in temperate and tropical waters. After 1 or 2 years of immersion the samples showed no sign of penetration by marine borers and...
A Gambetta


Degradation of woods by obligately anaerobic fungi
1990 - IRG/WP 1452
Little is known about the processes occurring during the degradation of wood by obligately anaerobic fungi. When woods from a range of hardwood species were incubated for 11 days with a strain of the Chytrid Neocallimastix frontalis many of the woods were measurably fermented; Fagus sylvatica (23%) was the most highly degraded. Microscopic examination of Populus tremuloides wood after incubation w...
K N Joblin, G E Naylor


Effects of boron formulation on specific timber types used in ships of historical importance
1991 - IRG/WP 3676
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
B King, G M Smith, J W Palfreyman, S McCutcheon


Bioefficacy of Cunapsol® treated western cedar and southern yellow pine
1996 - IRG/WP 96-30120
Western red cedar and southern yellow pine sapwood were dip treated with a new formulation of waterborne copper naphthenate (Cunapsol®) which complies with VOC regulations. Cunapsol dip treated samples were oven dried at 50°C for 48 hours and then water leached for two weeks. Decay resistance and leachability of preservatives from dip treated specimens were evaluated according to AWPA (American ...
D P Kamdem, M H Freeman, T L Woods


The results of detection on CCA components of the soils contacted with CCA-treated woods - A trial study for the availability of the burial Method as a disposal CCA treated wood waste
1993 - IRG/WP 93-50005
The objecteve of this experiment is to get a knowledge that, when CCA treated wood wastes were buried in a soil as a disposal, the soil would be or not be contaminated by the components of CCA preservatives in wood wastes. The specimens used were cutting logs and chips made of the CCA treated electric pole waste. The soil was buried to the 15 cm depth and the log specimens were set in the soil for...
K Suzuki, H Sonobe


Previous Page | Next Page