Your search resulted in 86 documents. Displaying 25 entries per page.
Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman
Recent developments in the treatment of sawn spruce by double vacuum impregnation
1978 - IRG/WP 3114
The timbers used for building purposes in the U.K. and on the Continent of Europe are mainly softwoods. The two types of wood most used are redwood (Pinus sylvestris) and whitewood (Picea abies or Picea sitchensis). Other species are used to a lesser extent when considerations such as a long length requirement or width requirement demand the use of, for example, hemlock, Douglas fir or Parana pine...
C T Kyte, L D A Saunders
The treatment of sawn whitewood with organic solvent wood preservative
1982 - IRG/WP 3192
The impregnation schedules approved in the UK for the treatment of sawn European whitewood (Picea abies) with organic solvent borne preservatives result in comparitively high loadings relative to the limited depth of penetration they achieve. Results are presented, which show how substantial reduction in the overall loading may be achieved without concomitant reduction in penetration. A model for ...
L D A Saunders
A technique for determinging the efficacy of wood preservatives for partially treated timber
1988 - IRG/WP 2322
A technique is described for determining the efficacy of wood preservatives either for certain wood species where a full penetration cannot be achieved by normal vacuum-pressure methods or for more permeable species to look at efficacy of treated zone in preventing decay of an untreated core. Both sapwood and heartwood planks of spruce (Picea abies) and pine (Pinus sylvestris) were treated by CCA ...
A J Nurmi
Paper for discussion - Incising of spruce to improve preservative penetration
1973 - IRG/WP 318
Large quantities of whitewood or Norway spruce (Picea abies) are regularly imported into the United Kingdom from continental Europe. In addition, increasing amounts of Sitka spruce (Picea sitchensis) are likely to become available over the next decade from the Forestry Commission. In many ways spruce is a good structural timber, eg it is relatively cheap and easily available, it has adequate stren...
W B Banks
Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring
Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens
Comparative study on leaching of CCA from treated timber: Modelling of emission data
1994 - IRG/WP 94-50027
Results of a comparative study on leaching of CCA from treated timber are reported. The study aims at investigating the applicability of prestandard leaching test methods for modelling purposes. Prestandards used are the European standard proposed by CEN/TC38/WG11 and NEN 7345 (Dutch prestandard for building materials). Parameters of study are type of fixation, wood species (pine - spruce), specim...
G M F Van Eetvelde, M Stevens, L Van der Mijnsbrugge
The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen
Generation of hydroxyl radical by the brown-rot fungus, Postia placenta
1988 - IRG/WP 1360
In an electron spin resonance (ESR) survey of various liquid cultures and wood slivers innoculated with the brown-rot fungus, Postia placenta, the spin trap dimethyl-l-pyrroline N-oxide (DMPO) was used to detect the presence of the hydroxyl radical. The ESR spectra for the paramagnetic DMPO- hydroxyl radical adduct was observed in (1) nitrogen-limited, liquid cultures having 1.0% glucose or 0.1% c...
B Illman, D C Meinholtz, T L Highley
Effect of wood species on decomposition efficiency of metham sodium
1992 - IRG/WP 92-3699
The effect of wood species and temperature on efficiency of metham sodium (32.1% sodium N-methyldithiocarbamate) decomposition to methylisothiocyanate (MITC) was investigated on 10 hardwoods and 9 conifers over a 144 hour period. Gas chromatographic analyses of headspace samples and ethyl acetate extracts of the wood revealed that decomposition never approached the theoretical decomposition effici...
J J Morrell
Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang
Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury
The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King
Influence of felling time on the natural durability of norway spruce (Picea abies (L.) Karst.)
1998 - IRG/WP 98-10250
Natural durability was tested in a laboratory test according to EN 113. The test fungi were Coniophora puteana and Poria placenta. Additionally, the test method was modified by using water agar instead of malt agar, so that wood was the only nutrient source for the fungi. In a third attempt the samples were inoculated with Trichoderma harzianum before testing.
The trees were felled on the 22.7.97...
M Hirmke, K Messner, J Fellner, A Teischinger, R Wimmer
The use of spruce for transmission poles
1973 - IRG/WP 326
A series of preservative treatments with creosote using Lowry and Rueping schedules was undertaken. From these treatments the most suitable impregnation conditions for water stored Sitka spruce (Picea sitchensis) and Norway spruce (Picea abies) transmission poles were determined. Preservative distribution and permeability values for poles of both species were used to decide the optimum season and ...
J A Dunleavy, D J Balfe, J P Prendergast
The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric
Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg
Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt
The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens
Leachability of didecyldimethylammonium chloride (a quaternary ammonium compound) from four wood species
1982 - IRG/WP 3204
Sapwood blocks prepared from red pine, ponderosa pine, southern yellow pine and hem-fir (a commercial mixture of western hemlock and amabilis fir) were treated with didecyldimethylammonium chloride, (an alkylammonium compound, AAC). After oven drying the blocks were vacuum impregnated with distilled water and subjected to a static leach cycle for 48 hours. The leachate was analyzed and the amount ...
J N R Ruddick, A R H Sam
The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire
Field evaluation of CCA movement in sap-displaced copper chrome arsenic treated softwood poles
1989 - IRG/WP 3539
Commercial sap-displaced UK grown Scots and Corsican pine, and Sitka and Norway spruce poles were exposed in a field site at Dundee, Scotland and radial distribution profiles of CCA monitored prior to implantation and after subsequent field exposure. Results show that groundline levels of all preservative elements were higher after 1 and 2 years field exposure compared with those recorded prior to...
S D Hainey, G M Smith, A Bruce, P D Evans, B King, H J Staines
Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp
The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta