An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Laboratory tests on artificial weathering of Quercus rubra crossties
1986 - IRG/WP 2252
Clear red oak (Quercus rubra) blocks were used to evaluate various types of accelerated aging tests including boil, steaming, and cyclic weathering. It was found that the repeated vacuum and pressure treatment of wood in water, steaming, oven-dry, and freezing appeared to be most effective in reducing the MOE in compression and hardness modules of wood specimens. Red oak crossties which were press...
P Chow, A J Reinschmidt, E J Barenberg, S L Lewis


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner


In-house accelerated method for testing decay resistance of treated wood
2004 - IRG/WP 04-20286
Fungicidal compounds often change their effectiveness when they are incorporated into candidate formulations. For this reason fungistatic effectiveness needs to be re-evaluated as many times as the formula has been modified for better performance. To avoid multiple expenses, in-house fungistatic tests are essential. Our goal was to develop in-house usable, simple but reliable and reproductive proc...
N Vidovic


The influence of staining fungi on the decay resistance of wood treated with alkylammonium compounds
1984 - IRG/WP 3308
Although found to be very effective in laboratory tests, alkylammonium compounds (AAC's) have failed to perform as well in field stake tests. Examination of leachability showed that this was not the cause. The present study investigated the possibility that staining fungi, (which have been observed to rapidly infect the field stakes), degrade the AAC wood preservative. Soil-blocks were tr...
J N R Ruddick


Comments on leaching in view of accelerated testing
1977 - IRG/WP 294
We developed an accelerated test for leaching at elevated temperatures (75-85°C). This test was used for the examination of 11 preservative formulations containing Cu, Zn and As. The data obtained from these experiments were compared with data on some formulations tested by ASTM standard leaching test. The method consists in making a large surface to volume ratio of wood from a treated block by c...
J Rak


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Evaluation of the protective means of some wood preservatives by means of accelerated tests
1973 - IRG/WP 232
In site conditions of the eastern site in the forest-steppe part of the Krasnovarsk region, the relative effectiveness of a series of wood preservatives was obtained by means of field tests. To obtain a more accurate evaluation of the protective qualities of these accelerated tests were carried out in laboratory conditions. In 9 boxes filled with non-sterile soil taken from the site, 72 samples of...
I A Petrenko


Control of wood biodeterioration by fungal metabolites
1992 - IRG/WP 92-1527
Treating wood with different conventional preservative chemicals for protection and economic utilisation is well known. Tough some of these chemicals are toxic to skin, their use as wood preservative is unavoidable as they should be toxic to biodeteriorating organisms also. Recent advances in chemistry of natural products enabled the use of wood extractives as biocidal compounds against biodeterio...
H S Ananthapadmanabha, H C Nagaveni, V V Srinivasan


Accelerated testing for out of ground contact using natural biological preconditioning
1996 - IRG/WP 96-20088
Small blocks made of Scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. Bacteria and moulds colonised the vermiculite and miniblocks well. Aureobasidium pullulans was common on TnBTO tre...
S Molnar, D J Dickinson, R J Murphy


Physiological properties of fungal test strains according to the European Standard EN 113
1986 - IRG/WP 2258
For the discussion of the European standard EN 113 the EMPA's procedure of culturing the test fungi and the corresponding virulence of the test fungi as well as the wood moisture content at the end of the test are shown. It is mainly shown that within the standard the choice of the solvent may not be left at the test lab if reproducible results shall be obtained. The different solvents in...
E Graf, B Zgraggen, P Manser


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


A comparison of fungal strains used in the bioassay of wood preservatives
1984 - IRG/WP 2220
Previously published data are presented relating to a number of strains of wood-destroying basidiomycetes (Coniophora puteana, Coriolus versicolor, Gloeophyllum abietinum, Gloeophyllum sepiarium, Gloeophyllum trabeum, Lentinus lepideus, Poria placenta, Fibroporia vaillantii and Serpula lacrymans) commonly used as test fungi in the bioassay of wood preservatives. The data, which has not been statis...
J Wazny, H Greaves


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans