Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Leaching of active components from preservative-treated timber. Stages 2 & 3: Laboratory testing and comparison with semi-field testing
2004 - IRG/WP 04-20303
This part of the project is focussed on leaching from preservative-treated wood obtained by the laboratory test method CEN/OECD draft guideline, February 2003 ”OECD guideline for the testing of chemicals proposal for new guideline XXX. Estimation of Emissions from Preservative-treated Wood to the Environment: Laboratory Method for wood held in the storage yard after treatment and for wooden comm...
N Morsing, B Lindegaard


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


The ecotoxicology assessment of wood preservatives and their active ingredients by means of germination tests using cress - A critical consideration
1999 - IRG/WP 99-50125
With putting the Biocidal Products Directive 98/08/EC (BPD) in place an environmental risk assessment for wood preservatives and impregnated timber is requested. To assess possible risks, suitable test methods are required, which reveal the ecotoxicological profile including environmental fate and behaviour of treated commodities. Germination and growth tests could contribute to the determination ...
P Jüngel, A O Rapp, E Melcher


Quantification des émanations de substances dans l'air ambiant a partir des bois traités
1993 - IRG/WP 93-50001-27
Pesticides on wood for the purpose of its protection may evaporate. Eventual toxicity of such emanations justifies risk assessment procedures for indoor air in building. This document describes bench scale tests based on the technique of chambers developped by CTBA/BIOTEC to determine the amount of pesticides and associated substances released to the ambient air. Results obtained with various pest...
H Sageot, M Lamour


The involvement of extracellular substances for the generation of hydroxyl radical during wood degradation by white-rot fungi
1997 - IRG/WP 97-10218
The activities of one-electron oxidation, hydroxyl radical generation, and phenol oxidase during the incubation of cultures of four white-rot fungi containing either glucose or wood were periodically measured. Further, their degradation activities against wood were examined during the course of cultivation. The generation of hydroxyl radical was correlated to the activity of wood degradation and i...
H Tanaka, S Itakura, A Enoki


Animal blood protein as a component of new, non-toxic wood preservatives fixing organic active compounds in wood
2003 - IRG/WP 03-30312
Application of natural organic compounds and simple physico-chemical treatments in wood conservation has, as its objective, not only its protection against biological agents but, equally importantly, protection of natural environment by gradual abandonment of toxic constituents still applied commonly on a wide scale. The introduction into wood of new, non-toxic impregnation agents manufactured on ...
B Mazela, I Polus


Method to determine the depth of penetration of the biologically active components of wood preservatives
1978 - IRG/WP 2108
A time-saving method for determining the depth of penetration of the biologically active components of wood preservatives is described. The test specimens were obtained by cutting thin slices from the wood either parallel or perpendicular to the treated surface. The slices were then exposed to fungal attack. A good correlation was found between the test results obtained by the modified German Stan...
H-P Sutter


Insect growth regulators: modes of action and mode of action-dependent peculiarities in the evaluation of the efficacy for their use in wood preservation
1997 - IRG/WP 97-30155
Up to now, the insecticides used in wood preservation are either of more or less non-specific mode of action - like boron - or of neurotoxic mode of action - like chlorinated hydrocarbons, carbamates and pyrethroids. The active ingredients actually used are primarily mirroring the progress in active ingredient research in plant protection. The methods of testing of the insecticidal efficacy of woo...
M Pallaske


Practical considerations of the Formosan subterranean termite in Louisiana: A 50-year-old problem
2000 - IRG/WP 00-10330
In an eleven-year censusing (1989 through 1999) in the French Quarter of New Orleans and surrounding areas, Coptotermes formosanus alate numbers were found to be increasing dramatically in all years but one. Moreover, in parks and neighborhoods in New Orleans and Lake Charles, LA, as well as in Sam Houston Jones State Park near Lake Charles surveyed in 1998, alarmingly high numbers of this exotic ...
G Henderson


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Leachability of active ingredients from some CCA treated and creosoted poles in service. A progress report after 10 years testing
1990 - IRG/WP 3627
CCA K33 TYPE B treated or creosoted poles, 10 pieces of each treatment type, have been monitored from the treatment plant to an electricity line, which was build up in Southern Finland in 1978. Preservative retention was determined by taking borings at four different levels: 1.5 m from the top end, 1 m above ground line, ground line and 0.5 m below ground. Determinations were made before setting u...
A J Nurmi


Measuring Soil Respiration as a New Approach to Describe the Interaction Between Wood (Treated and Untreated) and Microbiologically Active Soil
2006 - IRG/WP 06-20344
Soil respirometry was employed to examine the relationship between both the performance of copper organic preservatives in contact with and the amount of carbon dioxide evolved from soil and the effect of wood treated with preservatives on carbon turnover in soil. Wood was treated with a range of copper organic preservatives intended for use in ground contact as well as an organic preservative in...
I Stephan, W Mierke


Ionic liquids with organic and inorganic anions as highly active wood preservatives
2006 - IRG/WP 06-30411
Quaternary ammonium tetrafluoroborates, nitrates(V), propionates, acetates and formates with alkoxymethyl substituents were prepared and tested on wood destroying and sapstaining fungi. These new compounds are ionic liquids (ILs), which penetrate very well into Scot pine wood. Alkoxymethyldecyldimethylammonium tetrafluoroborates and nitrates(V) show better microbial activity against Coniophor...
J Zabielska-Matejuk, A Skrzypczak


The role of chromium in wood preservatives under BPD - a review and the current situation in Europe
2008 - IRG/WP 08-30468
Already during the IRG-meeting in Trømso a paper was presented to give an overview regarding the situation on chromium (JÜNGEL et al. 2006). Already in that year there was an increased attempt to achieve a science-based correct and harmonised solution in Europe regarding the chromium-question by the European Commission. Nevertheless the competent authorities (CAs) and the industry were similarly...
P Jüngel, S Hellkamp


Use of biological and low toxicity products against subterranean termites
2009 - IRG/WP 09-20410
The climatology of Mediterranean countries is favourable to the development of termites that cause important damage to wood structures in both furniture and buildings. Until a few years ago the treatment for this type of insect was based on the impregnation of the wood with chemical products. The use of these chemicals is now being restricted in Europe since the publication and harmonization of n...
M T Troya, M J Prieto, F Rubio


Using plant oils as hydrophobic substances for wood protection
2010 - IRG/WP 10-30550
The increased interest to use oils as hydrophobic agents and the current debate about the further use of creosote emphasises the urgent need of better understanding of plant and other oils as wood protectors. The present study sheds light on the hydrophobic properties and distribution of various plant oils in the anatomical structure of Scots pine sapwood. Oil retentions from approximately 70 to 5...
D Panov, N Terziev, G Daniel


First report on the termiticidal activity of extracts of Annona squamosa (Annonaceae) seeds and on its active constituent squamocins
2012 - IRG/WP 12-30605
Termites inflict severe damage on wood commodities and impede usage of several forest species. The biological metabolites could potentially replace synthetic termiticidal products which are becoming more restricted to use. Annona squamosa is well known for its edible fruits - tropical custard apple. Annonaceous tetrahydrofuran acetogenins have attracted much interest due to their broad range of bi...
T S Djenontin, N Amusant, P H Ducrot, D C K Sohounhloué, D Pioch


Survival of Bursaphelenchus xylophilus exposed to different active ingredients of wood protectors
2013 - IRG/WP 13-10802
The pine wilt nematode (PWN) Bursaphelenchus xylophilus (Steiner and Buhrer 1934) Nickle, 1970 is a quarantine organism with a high potential to damage Conifer forests in Europe. This has driven the European Union to protect forest stands from the propagation and dispersion of this pathogen.The nematode was first detected in Europe in Setubal (Portugal) in 1999 and eradication measures were taken....
S C Arcos, M T Troya, L Robertson, F Llinares, M Conde, A Navas


Penetration behaviour of different hydrophobic carrier substances for oily wood preservatives in Beech and Scots pine sapwood
2017 - IRG/WP 17-40804
The use of creosote as a wood preservative has a long history. Current areas of application are railway sleepers, transmission poles, timber bridges and marine applications. If the approval for creosote will not be prolonged, alternative wood preservatives will be needed. As the penetration behaviour after pressure impregnation of different alternative oily products in this fields of application i...
M Starck, A Gellerich, H Militz


Using satellite-retrieved soil moisture data to model the decay risk of in-ground timber
2022 - IRG/WP 22-20689
Satellite-derived soil moisture data from the Soil Moisture Active Passive (SMAP) was extracted for a 9 x 9 km point grid over Europe. The data was then used as input to a dose-response wood decay model based on terrestrial microcosm (TMC) tests. The resulting hazard map plotted dose as an indicator of in-ground wood decay based on differences in annual temperature and soil moisture characteristic...
P B van Niekerk, M Schönauer, B N Marais, C Brischke


Analytical retentions of active ingredients in H2F treated framing over a 12-year period
2023 - IRG/WP 23-20702
The H2F hazard class in Australia was developed to treat internal framing timber with a surface application of an insecticide, to control mainly termites. Two of the actives approved in AS 1604.1-2010 (and subsequent revisions) for this hazard class are bifenthrin and imidacloprid. The penetration zone of both actives is 0 – 2 mm from the wood surface. Radiata pine sapwood framing timber wa...
A Siraa


What products are architects using? Relationships between deterioration part and structural performance in wooden houses
2023 - IRG/WP 23-50374
Architects work in the development of ideas around buildings and all the nuclei where human activity is generated. It is a work of organization of matter, in time and space, where the conceptual world of ideas and the aspirations of inventions, the interior world interact with the exterior in many kinds of realities. But as architects, we have always been interested in why and how things have bee...
I de las Casas


Previous Page