Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Factors affecting decay rates in a fungus cellar II
1986 - IRG/WP 2259
Tests were initiated to investigate the influence of various factors on the decay rate in a "Fungus Cellar". Birch and pine stakes treated with chromated copper arsenate and didecyldimethyl ammronium chloride, as well as untreated control stakes, were incubated in two soils in a Fungus Cellar test and installed at two field sites for comparative purposes. The visual rating vs actual stake weight l...
P A McKaig


Effect of soil type and moisture content on soft rot testin
1986 - IRG/WP 2270
Several soils of different types were tested at a range of moisture contents for their suitability for use in a soil burial soft rot test. Their effectiveness was assessed by weight loss in CCA treated and untreated beech and birch outerwood. A horticultural loam (John Innes No. 2) was the most appropriare soil in terms of amount of weight loss caused, tolerance to changes in soil moisture content...
S M Gray


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Electrochemical deterioration of wood in sea-water
1981 - IRG/WP 464
In the specialistic literature only few items can be found dealing with the specific kind of wood deterioration called electrochemical corrosion of wood. This deterioration occurs predominantly on marine vessels, yachts, and other marine craft where wood is jointed by means of various metal connectors. Up to date information demonstrates that in wood surrounding copper connectors, when in proximit...
J Raczkowski


Copper based water-borne preservatives: Copper adsorption in relation to performance against soft rot
1987 - IRG/WP 3452
As part of a fundamental study concerned with the performance of copper based water-borne preservatives the adsorption of copper from aqueous solutions by 4 hardwood and 1 softwood species has been studied. Experiments were conducted to determine the influence of solution pH, solution concentration and solution temperature. The results obtained were consistent with an acid form ion-exchange mechan...
P M S Rennie, S M Gray, D J Dickinson


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig


Interactions between soft rot fungi and CCA preservatives in Betula verrucosa
1988 - IRG/WP 1367
Ultrastructural investigations were carried out to obtain information on the cell wall distribution of CCA elements during soft rot decay of 4% K33 CCA preservative treated birch (Betula verrucosa) wood. TEM observations on fibres at various stages of S2 cavity formation by mutabilis showed a distinct pattern of electron dense materials to occur within the S2 cell wall region. These materials (gra...
G F Daniel, T Nilsson


Immunolabelling studies on the detection of enzymes during the degradation of wood by Phanerochaete chrysosporium
1988 - IRG/WP 1364
The degradation of lignin in native lignocellulosic substrates by white rot fungi is poorly understood. Biochemical studies have shown the involvement of a number extracellular ligninolytic enzymes released by white rot fungi which are capable of the oxidative conversion of DHP's (lignin model compounds) in vitro, but to date conclusive evidence for occurrence of these enzymes in wood und...
G F Daniel, T Nilsson, B Pettersson


Use of the enzyme-linked immunoassay (ELISA) and immunocytochemistry to detect soft rot in preservative treated and untreated wood
1990 - IRG/WP 2347
A polyclonal antibody was raised against mycelial extracts from the soft rot fungus Phialophora mutabilis. In ELISA assays, the antibody showed strong reactions with its own antigen and strong to moderate cross reactions with 6 other Phialophora soft rot species. With the exception of Ceratocystis albida, the antibody gave only weak or negative reactions with 11 other mold, blue stain and rot fung...