TMT–Interlab–Test to establish suitable quality control techniques - Structure and first results
2010 - IRG/WP 10-40503
As a result of growing quality demands from manufacturers and end-consumers of thermally modified timber (TMT) recent scientific research activities are increasingly focussed on modification mechanisms and by this on the development of suitable quality control methods. To deepen the knowledge in modification mechanisms and to obtain a larger variety of scientific data for TMT depending on the trea...
C R Welzbacher


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


E.R.C. Pole Tester
1982 - IRG/WP 2190
Operating instructions for the ECRC pole-strength tester 120kNm 'PEST'....
G Elcock


Effects of various preservative treatments on the mechanical and physical properties of plywood
1993 - IRG/WP 93-40007
The technical properties of plywood are related to both the intrinsic characteristics of its composing wood species and the quality and performance of the glue bond which acts as an interface between veneer sheets. Consequently mechanical and physical testing and glue bond strength analysis offer an appropriate means for studying the effect of preservative treatments on the overall quality of plyw...
J Van Acker, M Stevens


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


The utilisation and preservation of Eucalyptus globulus agricultural stakes from Portugal
1989 - IRG/WP 3520
This paper reviews the development and utilisation of Tanalith C treated Eucalyptus globulus stakes: particular reference is made to their use in vineyards. The treatment characteristics of commercially available stakes will be described and penetration patterns evaluated....
A Milne e Carmo, D A Lewis, A Lyman


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


A direct method for testing plywood and particle boards against fungal decay
1984 - IRG/WP 2214
A method directly inspired from the French standard testing method of the resistance of particle boards against fungal decay (AFNOR N° 51.295 May 1980) is described. But in that experimentation, the infestation is localized and realized in non sterile conditions. Small blocks of Fagus sylvatica (60 x 20 x 10 mm³) used as " inoculates " are infested with basidiomycetes, in Kolle flask for 4 to 6 ...
L N Trong


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


The performance of softwood species used as poles in Queensland
1985 - IRG/WP 1253
In Queensland, the conifer Pinus elliottii could provide material suitable for use as poles. Full size pole material has been readily treated with CCA with no significant loss in strength. Seasoning of logs prior to treatment requires particular attention in the wet tropical and sub-tropical regions of Queensland. Experimental and in service field tests have indicated excellent performance of CCA ...
L E Leightley


Bibliography: Interactions of wood preservatives with wood, metals, glues, paints and concretes
1983 - IRG/WP 3271
H Becker


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas