A simple leaching procedure for in-plant monitoring of CCA fixation
1993 - IRG/WP 93-30023
A simple leaching test is described to quantitatively estimate the extent of fixation of chromated copper arsenate (CCA) preservative treated wood products. It is based on the reaction between diphenylcarbazide and unreacted hexavalent chromium leached from borings taken from treated wood during the fixation process. The test requires about 20 minutes to complete and can be set up in a treating pl...
P A Cooper, Y T Ung


Preservative-treated wood as a component in the recovered wood stream in Europe – A quantitative and qualitative review
2004 - IRG/WP 04-50218
Wood preservatives have been used for the protection of timber products in the European market in appreciable quantities for about 100 years. Between the 1960s up to the present day this usage has been particularly noticeable. The aim of this paper is to present quantitative and qualitative data on the volumes of preservative treated wood placed on the market in the UK and Sweden and to evaluate t...
R J Murphy, P Mc Quillan, J Jermer, R-D Peek


nvestigation of anomalous fixation and leaching of CCA-treated red maple
2004 - IRG/WP 04-30341
The fixation of CCA-C preservative was investigated in red maple sawdust (Acer rubrum L.) at target retentions of 4.0, 6.4, 9.6 and 30.0 kg/m3. The effect of water-soluble extractives on the course of fixation was evaluated comparing the non-extracted with pre-extracted samples treated to 6.4 and 30 kg/m3. Leaching of the CCA components was monitored after complete fixation for all retentions. Fix...
S Radivojevic, P A Cooper


Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


Soft rot and bacterial decay in preservative treated eucalypt power transmission poles
1982 - IRG/WP 1155
Bacterial type decay was observed in CCA and PCP treated eucalypt power transmission poles. Detailed observations made with the SEM revealed bacterial colonisation and decay, especially in fibres. Plug samples taken from poles throughout Queensland were examined for preservative retention and presence of soft-rot decay. The severity of decay was different according to location, retention and speci...
L E Leightley


An effective preservative treatment of borak bamboo (Bambusa balcoona Roxb.)
1996 - IRG/WP 96-40070
Adequate penetration and retention of CCA and CCB has been obtained in predried Borak Bamboo (Bambusa balcooa Roxb.), aboundantly grown in Bangladesh, with Full Cell Pressure Process. The treated bamboo can be used as building materials, the sufficient treatability ensured its long term best utilization at ground contact and indoors. Which will keep the environmental & socio economical conditi...
A K Lahiry, S Begum, G N M Ilias, M A Matin Sheikh, M A B Fakir, M I Hossain


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 5. Treatment of Sitka spruce and Scots pine
1999 - IRG/WP 99-40136
The suitability of the MPP Process for CCA treatment and accelerated fixation of species other than Radiata pine was assessed by pilot plant trials on UK-grown Sitka spruce (Picea sitchensis) and Scots pine (Pinus sylvestris). Pressure and vacuum kickbacks of spruce (14 l/m3) and Scots' pine (122 l/m3) were both substantially lower than that generated during treatment of radiata pine (369...
M E Hedley, K Nasheri, G Durbin


Inorganic wood preservative levels in soil near a noise barrier treated with different preservatives after 8 years in service
2005 - IRG/WP 05-50234
In March 1996 nine test sections of a noise barrier were installed near Stockholm Sweden. The test sections include untreated Scots pine, spruce and larch and Scots pine, treated with different wood preservatives. After 8 years in service, the untreated spruce, pine and larch boards in contact with the soil were significantly decayed, with an estimated service life of about 5-10 years, while the u...
P A Cooper, Y T Ung, M-L Edlund, J Jermer, O Söderström


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


Comparative evaluation of the barrier effect against Hylotrupes bajulus L. of different types of wood preservative
1986 - IRG/WP 1307
This paper settles the difference of contact action against females of Hylotrupes bajulus the likelihood of egg-laying, the ovicide effect and the hazards of development of newly hatched larvae between some preservatives belonging to three differents types: mineral waterborne products, organic products and emulsions. The results show that against females, the action is fast with organic products, ...
M-M Serment


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


A fixation model, based on the temperature dependence of CCA-C fixation
2000 - IRG/WP 00-40163
A model was prepared for the fixation of 1% CCA-C in red pine that allows the prediction of extent of fixation based on the temperature history of the treated wood following pressure treatment. The reaction kinetics of the rapid initial reaction and the slower main reaction were characterized using the Van t'Hoff equation. The initial reaction could be represented by a 10th order chemical...
P A Cooper, K M F Kazi, Jianbin Chen, Y T Ung


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


The effect of temperature on the rate of fixation of an alkyl ammonium compound (AAC) wood preservative
1984 - IRG/WP 3293
The rate of fixation of an alkyl ammonium compound wood preservative was measured by soaking samples of wood wool in various preparations of the preservative for arbitrary times followed by immediate leaching in water. The wood wool was then analysed for residual preservative. The results indicated that fixation was very rapid and increased at higher temperatures....
P Vinden


Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


CCA fixation experiments. Part 1
1989 - IRG/WP 3504
A method of squeezing solution from CCA treated wood that has not been dried at various times after treatment appears to be useful in following the fixation of CCA in wood. Experiments confirm that temperature governs the rate of fixation....
W S McNamara