Bio-friendly preservative systems for enhanced wood durability - the first periodic report on DURAWOOD
2015 - IRG/WP 15-30677
The objective of the paper is the DURAWOOD scientific project carried out within Polish-Norwegian Research Programme, which lasts from September 2013 till August 2016. The aim of the project concentrates on the developing of a new, eco-friendly and biocide-free wood protective systems as an alternative to traditional, commonly used preservatives or coatings, containing biocides. Several wood prese...
B Mazela, M Broda, W Perdoch, L Ross Gobakken, I Ratajczak, G Cofta, W Grześkowiak, A Komasa, A Przybył


A review of the analytical methods used in determining the decay resistance of heat treated wood
2015 - IRG/WP 15-40690
Heat treatment as a wood process is increasingly used because of its non-biocide behaviour and its low environmental impact. This sort of treatment is based on biopolymer chemical degradation by heat transfer. This process improves mainly the dimensional stability and the decay resistance of wood. Wood becomes darker after this type of treatment and thus gives it an aesthetic appearance. These i...
K Candelier, M-F Thévenon, A Pétrissans, S Dumarçay, P Gérardin, M Pétrissans


High-frequency monitoring of mass loss due to brown rot degradation of modified wood
2016 - IRG/WP 16-10862
Fungi growing in liquid culture undergoes three separate phases in which they i) adapt to the new environment, ii) grow unrestrictedly and exponentially, and iii) are inhibited to increase in number/mass due to lack of nutrients etc. Filamentous fungi have been shown to exhibit similar growth phases in a solid food substrate and have been modelled to grow in this way also in solid wood. In modifie...
R Ringman, A Pilgård, K Richter


Markers of quality in self-bonded beech boards
2017 - IRG/WP 17-40820
A self-bonding phenomenon takes place when five layers of beech (Fagus Sylvatica L.) veneers are pressed at temperatures higher than 200ºC. If the pressing temperature between veneer surfaces reaches at least 225ºC during pressing and if the pressure applied is optimal, water-resistant bonds are formed between veneers. This study investigates the relation of thickness reduction (marker of compre...
C Cristescu, D Sandberg, O Karlsson


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Summary of development of pile wrappings in Los Angeles Harbour
1987 - IRG/WP 4141
G Horeczko


Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


A medium for mass culturing of a bamboo boring beetle Dinoderus minutus Fabricius
1983 - IRG/WP 1182
The bamboo is a traditional product of Japan. But its susceptibility to insects is one of the most important problems. The author has found that for the determination of the effectiveness of insecticides it is very easy to obtain sufficiently numerous adults of Dinoderus minutus by using Buckwheat Cake. The Buckwheat Cake is prepared with buckwheat flour and thin paper. The author has previously f...
K Suzuki


The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker


Temperature influence on the growing velocity and cellulolytic activities of Poria placenta strains from several locations
1986 - IRG/WP 2263
The differences observed on the FPRL 280 Poria Placenta strain at several Research European Laboratories for determining up the fungicide effectiveness of wood preservative has carry us to do a comparative study about the cellulolytic activity and growth velocity of each of this strains at different temperatures (22, 24 and 28°C). The results show significative differences when the temperature is...
A M Navarrete, M T De Troya


Spore germination of Gloeophyllum trabeum on wood is related to the mass of the wood sample
1978 - IRG/WP 2118
E L Schmidt, D W French


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Virulence testing of cultures of different origins of the test fungus Coriolus versicolor strain CTB 863 A
1986 - IRG/WP 2267
The virulence of cultures of different origins of Coriolus versicolor CTB 863 A - a strain which is mentioned in EN 113 - was tested. Standard blocks of beech wood were used at temperatures of 20-22°C and 26-28°C and particleboard was tested at 26-28°C. The decay capacity of the different inoculations varied widely, as could be expected it was greatest at the higher temperature level....
W Kerner