IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 840 documents. Displaying 25 entries per page.


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 6: The length of the primary precipitation period
1975 - IRG/WP 359
The end of the primary precipitation fixation period of CCA preservatives coincides with the first peak in pH versus time. This offers a simple way of estimating the duration of the period. The duration is determined by a number of factors and their interactions, the most important of which are: wood species (anatomy, natural pH, accessibility of reducing agents), preservative type, preservative c...
S-E Dahlgren


The fate of salt preservatives in facility yard soils and decontamination of soils and drainage waters
1993 - IRG/WP 93-50001-25
Extensive studies during the past 10 to 15 years revealed that noticeable amounts of preservative components may be released in the environment by dripping off or by rain prior to fixation unless adequate precautions are taken. Therefore, soil and groundwater contamination especially from chromium-VI compounds but also from other inorganic and organic constituents exist in impregnation plants, pos...
R-D Peek, H Klipp, K Brandt


Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Environmentally benign wood preservatives based on organic biocide antioxidant combinations: A brief review of laboratory and field exposure results and discussion of a proposed mechanism
2004 - IRG/WP 04-30335
The combination of various organic biocides with commercial antioxidants generally increased the biocides’ efficacy 2-3 fold against wood-destroying fungi in short-term laboratory decay tests, and some positive results have been obtained after 2-4 years of outdoor exposure. The two antioxidants principally examined, propyl gallate and butylated hydroxytoluene, are low cost and, since both are f...
T Schultz, D D Nicholas, W Henry, C Pittman, D Wipf, B Goodell


Copper based water-borne preservatives: Copper adsorption in relation to performance against soft rot
1987 - IRG/WP 3452
As part of a fundamental study concerned with the performance of copper based water-borne preservatives the adsorption of copper from aqueous solutions by 4 hardwood and 1 softwood species has been studied. Experiments were conducted to determine the influence of solution pH, solution concentration and solution temperature. The results obtained were consistent with an acid form ion-exchange mechan...
P M S Rennie, S M Gray, D J Dickinson


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Recycling and disposal of timber treated with waterborne copper based preservatives
1993 - IRG/WP 93-50008
Recycling and disposal technologies are briefly reviewed. Details are given of chemical extraction techniques suitable for recovery of copper from timber treated with a new copper based preservative, and traditional chromium based products. Details of thermal decomposition tests according to the DIN 53436 protocol under flaming and non-flaming conditions are given. The decomposition products were ...
J A Cornfield, S Vollam, P Fardell


Inorganic preservative levels in soil under treated wood decks after 8 years natural exposure in Borås, Sweden
2005 - IRG/WP 05-50233
Inorganic preservative components (Cu, Cr and As) were measured to a depth of 150 mm under deck structures made with Scots pine lumber treated with several different wood preservatives and installed in Borås Sweden 8 years ago. Higher contaminant levels were observed mainly under the drip lines and in the top 50 mm of soil. Under CCA treated decks, soil arsenic concentrations increased from ba...
P A Cooper, Y T Ung, M-L Edlund, J Jermer


Changes of EPR spectra of wood, impregnated with copper based preservatives, during exposure to Antrodia vaillantii
2000 - IRG/WP 00-10355
Spruce wood (Picea abies) samples were impregnated with two different aqueous solutions: copper(II) octanoate with ethanolamine or copper(II) sulfate (cCu = 1,0 x 10-2 mol/l). Impregnated and unimpregnated test pieces were exposed to wood rotting fungus Antrodia vaillantii. Some strains of this fungus are known as copper tolerant. After four weeks of exposure to A. vaillantii, we could not detect ...
M Humar, M Petric, F Pohleven, M Šentjurc


Technologies for the Management of Wood Waste Containing Metals-Based Preservatives
2005 - IRG/WP 05-50224-16
Disposal of the metals from preservative treated wood can occur through two general strategies: “removal and confinement” or “dilution”. The acceptability of each of these two choices is typically dictated through the disposal regulations of a particular region. A considerable amount of research has been conducted to develop new and innovative “removal and confinement” technologies...
H M Solo-Gabriele, T G Townsend


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Fungal degradation of wood treated with metal-based preservatives. Part 1: Fungal tolerance
1996 - IRG/WP 96-10163
In recent years, concerns have arisen about the leaching of heavy metals from wood treated with chromated copper arsenate (CCA), particularly because of the large amount of CCA treated wood that will be discarded in the coming years. The long term objectives of this work are to determine the fate of copper, chromium and arsenic with the aging and potential decay of CCA-treated wood, and to develop...
B Illman, T L Highley


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


Corrosiveness of metal by copper-based preservatives
2006 - IRG/WP 06-40329
The corrosive rates of 4 types of metal as well as epoxy-coated metal by a variety of preservatives derived from different copper source and ingredients were conducted in this paper. The main results shown that: CCA is less corrosive to red brass and Q235A steel than other copper formulations; Copper-based preservatives such as ACQ and copper azole derived from basic cupric carbonate or cupric hyd...
Ying Zhang, Mingliang Jiang


Use of the Digital Refractometer for the On-site Analysis of Copper-based Preservative Systems
2007 - IRG/WP 07-20371
In some counties, there are no on-site chemical analysis methods available for treatment plants to use to determine the key active ingredients in the preservative treatment solutions. The complexity of the sophisticated methodology; cost of analytical instruments and training required for operating these instruments in treating plant level are the reasons for lacking such practice. In this paper...
L Jin, T Cashman, A Preston, J Trompetter, H Trompetter


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Physical and Mechanical Properties of Bamboo Oriented Strand Board Treated with Copper-based Preservatives
2009 - IRG/WP 09-40482
Oriented strand board (OSB) has been gradually accepted, used and developed in China. Bamboo is a renewable and potential non-wood fibre resource for making OSB. But the nature of bamboo makes its products including bamboo OSB (BOSB) more prone to decay and mold. Protection BOSB from biodegradation is the key both to efficiently using bamboo resource and to improving the durability of the final pr...
Juwan Jin, Daochun Qin


Previous Page | Next Page