Biological and chemical observation on the early fungal colonization of TBTO treated Swedish redwood stakes
1984 - IRG/WP 3311
Data on the early fungal colonization of Swedish redwood stakes, impregnated with 1% TBT0 / 0.5% dieldrin solution, both by double vacuum impregnation and immersion processes are presented. Results of chemical analyses of wood samples from the outer 1 mm of separate painted and unpainted stakes, exposed over the same twelve month period, are also discussed....
R Hill, A H Chapman, A Samuel, K Manners, G Morton


About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu


Effects of pretreatments for the amelioration of preservative impregnability using the Oscillating pressure method (OPM)
1995 - IRG/WP 95-40044
For the purpose of an amelioration of preservative impregnability, three types of pretreatment: the steaming, the explosion and the boiling, were tested. The specimens were prepared by the domestic four species: Itajii, Ryukyumatsu, Sugi and Hinoki, and 1 refractry imported species: Douglas-fir. The dimension of specimens was 20 x 20 x 300 mm³ and were treated with CCA in a laboratory OPM machine...
K Suzuki, I Asaoka, S Tani, K Okada, T Hidaka


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


Chlorodioxines dans le pentachlorophénol
1975 - IRG/WP 346
H Alliot


Tebuconazole - Efficiacy, toxicity, physical properties
1995 - IRG/WP 95-30093
An overview ahout the physical properties and toxicology of tebuconazole as well as an update of efficacy data of this triazole are given....
H-U Buschhaus


Programme section 4, Processes
1997 - IRG/WP 97-40096
IRG Secretariat


Fipronil - le nouvel insecticide de Rhone Poulenc pour la preservation du bois
1995 - IRG/WP 95-30078
After the 3rd International Symposium in Cannes '95. More trial results and practical information on FIPRONIL, this new insecticide from Rhone Poulenc for Wood Preservation and PCO....
M G E J Van Maanen


Programme Section 4 Processes
1999 - IRG/WP 99-40150
IRG Secretariat


Tolylfluanid - fungicide against blue stain in service
1992 - IRG/WP 92-3736
Physical and chemical properties and efficacy of Tolylfluanid are compared with the properties of Dichlofluanid. Whereas the difference in the molecular structure influences the physical properties significantly, the efficacy of both fungicides is comparable. The toxicological and ecotoxicological profile of Tolylfluanid is summarised....
H-U Buschhaus


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Copper naphthenate-treated Southern Pine pole stubs in field exposure. -Part 2: Chemical characterization of full size pole stubs 12 years after treatment
2000 - IRG/WP 00-30246
This study examines the influence of pre-treatment and post-treatment steaming on the character and physio-chemical nature of copper naphthenate in hydrocarbon solvent treated pine in larger, pole diameter, pole stub-length samples. This work is the continuation of two projects that began almost a decade ago. Previous reports indicated that certain morphological changes might occur in small labora...
H M Barnes, D P Kamdem, M H Freeman


Termiticidal chemicals derived from tropical tree resins
1991 - IRG/WP 1477
To test the hypothesis that defensive chemicals protect tropical primary forest trees against biological attack, a bioassay and fractionation program was conducted in Indonesia. Fresh dipterocarp resins were fed in no-choice tests to Neotermes dalbergiae termites on 4.5 cm filter papers, or tested for inhibition of fungal growth. Fractionation of biologically active resins via flash column chromat...
A Messer, K McCormick, D Richardson, Sunjaya, H Hagedorn, J Meinwald


Chemical analysis of TnBTO in lap-joints
1999 - IRG/WP 99-20173
This research was performed as part of the EU project FACT (contract SMT4-CT96-2135) on field tests out of ground contact and ageing methods. The results reported here are part of the work on the experimental lap-joint standard (ENV 12037). TNO investigated the TBTO content of 32 lap-joints by analysing the tin content of 90 samples. The lap-joints were treated with two different TBTO-concentratio...
A Voss, P Esser, W L D Suitela


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Preventing fungal attack of freshly sawn lumber using cinnamon extracts
2007 - IRG/WP 07-30432
The potential for using cinnamon oil as an anti-mold and stain compound was investigated on ponderosa pine sapwood. Cinnamon oil was highly effective when used in ethanol, but its activity declined when it was mixed with only water. Attempts to enhance water solubility with surfactants improved solution stability, but had no apparent effect on biological activity. Further studies with other co-so...
Shujun Li, C Freitag, J J Morrell


The Chemical and Biological Properties of Polymeric Betaine
2009 - IRG/WP 09-30512
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. DPAB as a wood preservative has been reported previously. This paper summarizes the chemical, physical, and biological properties of DPAB. ...
H Härtner, S Schmitt, Futong Cui, H M Barnes


Laboratory and field evaluation of Plasmite Reticulation System using bifenthrin as a chemical barrier within wall cavities against subterranean termites.
2005 - IRG/WP 05-20307
Laboratory and field bioassays undertaken to demonstrate Plasmite Reticulation system effectively delivers the termiticide (bifenthrin) within a simulated wall cavity at the required concentration. The chemical assay indicated that the amount of bifenthrin sampled at 5, 10, 15, 20, and 25m along the simulated reticulation system tested (30m) exceeded the manufacturer’s minimum recommendation of ...
J R J French, B M Ahmed, J Thorpe, A Anderson


Electronic noses for detection of rot in wood
1996 - IRG/WP 96-20098
In an ongoing project an electronic nose is being studied and developed for detection of volatile organic compounds (VOC) emitted from wood colonised and decayed by fungi. The electronic nose consists of an array of gas sensors with different selectivity patterns for different groups of volatile organic compounds (VOC). The use of pattern recognition routines implemented by artificial neural netwo...
K Nilsson


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson