IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 226 documents. Displaying 25 entries per page.


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


The present classification of wood degradation factors
1993 - IRG/WP 93-10031
Contemporary classification of biotic and abiotic wood degradation factors is presented in two aspects: etiological and simptomatical one....
J Wazny


Bacterial wood degradation by a pure culture
1995 - IRG/WP 95-10093
A single-celled bacterium isolated from lake water yielded cell wall degradation in Scots pine sapwood samples. The bacterium attacked all cell wall layers in one month of laboratory culture. It was identified as Aureobacterium luteolum....
O Schmidt


Interaction mechanisms of F/Cr/As/B type preservative and wood
1981 - IRG/WP 3183
The paper reports results of investigations on the fixation of the components of a F/Cr/As/B preservative in wood and its lignin and cellulosic components....
N Ermush, I Andersone


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


Susceptibility of angiosperm sapwood to white-rot fungal colonization and subsequent degradation: a hypothesis
1997 - IRG/WP 97-10211
It has long been recognized that angiosperm sapwood in nature is relatively easily and preferentially degraded by white-rot fungi. This susceptibility to white-rot fungi is generally believed to be mainly caused by the structure and concentration of angiosperm lignin. However, an explicit explanation as to why lignin structure makes a particular wood vulnerable to white-rot colonisation and subseq...
T Schultz, D D Nicholas


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


Proposed degradation pathway for quaternary ammonium compounds by mould fungi
1996 - IRG/WP 96-10166
One group of chemicals that has attracted considerable attention as potential wood preservatives are the quaternary ammonium compounds (QACs). Based upon results of previous research this study confirmed the degradation pathway employed in QAC-tolerant fungi. For this experiment the two dialkylammonium compounds didecyldimethylammonnium chloride and dioctyldimethylammonium chloride were used. QAC-...
J L Bürgel, J Dubois, J N R Ruddick


Use of fluorescent-coupled lectins as probes for studying fungal degradation of wood
1986 - IRG/WP 1288
The ability of the fluorescent-coupled lectins wheat germ agglutin (WGA) and Concanavalin A (Con A) to react with selected Basidiomycetes, Ascomycetes, and Fungi Imperfecti was evaluated using pure cultures of 35 fungi grown on malt extract agar. WGA, which binds specifically to the n-acetylglucosamine residues found in fungal chitin, reacted with nearly all hyaline fungal structures but did not r...
J J Morrell, R L Krahmer, L C Lin


Immunogold labelling of size marker proteins in brown rot-degraded pine wood
1990 - IRG/WP 1428
Pine wood degraded by Fomitopsis pinicola was infiltrated with a mixture of ovalbumin (45 kDa) and myoglobin (16.7 kDa). After crosslinking of the proteins with glutaraldehyde and preparation for electron microscopy ultrathin sections were labeled with gold-conjugated antibodies. Simultaneous labeling of both proteins on the same section showed that at 50-70% weight loss ovalbumin did not penetrat...
E Srebotnik, K Messner


Fungal degradation of wood treated with metal-based preservatives. Part 2: Redox states of chromium
1996 - IRG/WP 96-10164
Concerns have arisen about the leaching of heavy metals from wood treated with metal-based preservatives, such as chromated copper arsenate (CCA). Of particular concern is the toxic redox state of chromium and arsenic in aging and decayed CCA-treated wood. Generally, hexavalent chromium is more toxic than trivalent chromium and trivalent arsenic is more toxic than pentavalent arsenic. The desired ...
B Illman, S Bajt, T L Highley


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


Biological degradation resistance of pine wood treated with dimethylol compounds
1989 - IRG/WP 3528
The study reports the increase of dimensional stability and biological degradation resistance of pine wood (Pinus sylvestris L) after impregnation with dimethyloldibydroxyethyleneurea. Decay resistance was determined according to BS 838:961. Nearly complete protection against Coniophora puteana, (Schum.ex Fr. Karst) weight loss of 2-3% was shown when modification, expressed as weight gain, exceede...
C L Videlov


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


The preliminary characterization of ß-1,4-xylanase of the brown-rot fungus Gloeophyllum trabeum
1990 - IRG/WP 1447
The extracellular ß-1,4-xylanase of the brown-rot fungus, Gloeophyllum trabeum, was isolated from crude extract by chromatofocusing method (PBE 94 column chromatography). The isoelectric point was estimated to 4.2-4.8 by cromatofocusing and 4.5 by isoelectric focusing (IEF). The molecular weight of the enzyme was estimated to 37,000 dalton by SDS-PAGE. The optimal temperature for the crude extrac...
A-C Ritschkoff, M Rättö, L Viikari


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


Stability and performance of tributyltin compounds
1984 - IRG/WP 3275
Based on the critical examinations of the disputable permanence of tributyltin compounds in wood, this paper deals with a number of examinations of the relative evaporation, thermal stability and oxidation stability of some TBT-compounds. While thermal and oxidative stability is high for all TBT-species, the relative evaporation at elevated temperature is highly variable, and lowest for the TBT-es...
F Imsgard, B Jensen, H A B Landsiedel, H Plum


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Evaluation of New Zealand staining fungi for degradation of radiata pine
1999 - IRG/WP 99-10310
This investigation sought to determine the potential of selected NZ staining fungi to induce weight loss and changes in toughness (impact bending strength) and composition in unseasoned radiata pine sapwood. Furthermore, assays were performed to eveluate enzyme production by staining fungi. Sets of side-matched specimens were inoculated with Ophiostoma floccosum, Sphaeropsis sapinea and O. plurian...
A Schirp, R L Farrell, B Kreber


Previous Page | Next Page