Influencia de la impregnación con soluciones tánicas en la estabilidad dimensional de la madera de Pinus pinaster Ait. procedente de España
1992 - IRG/WP 92-3686
En virtud de la importancia que presenta la madera de Pinus pinaster Ait. en el sector constructivo español, se ha sometido a esta a tratamientos en autoclave con distintas soluciones tánicas naturales y artificiales a fin de estudiar su incidencia en la estabilidad dimensional frente a exposiciones exteriores. En el estudio se pone de manifiesto el efecto creado por el tratamiento protector en ...
J A Rodríguez Barreal, J Cubillo Jordan de Urries, L Garcia Esteban


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Improvements of stability and durability of beechwood (Fagus sylvatica) by means of treatment with acetic anhydride
1991 - IRG/WP 3645
In the present investigations, beechwood (Fagus sylvatica) was treated with non-catalysed acetic anhydrid at 120°C and some physical- and biological parameters of the treated wood were compared with those of non-treated wood. The radial and tangential shrinkage and swelling, respectively, and the absorption capacity of the acetylated wood against moisture is considerably lower. The durability aga...
H Militz


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Effect of alkaline phenolic resin adhesive on the stability of preservatives incorporated into the glue-line of plywood
1991 - IRG/WP 3650
Stability of preservatives was determined by gaschromatographic analysis when they were applied to glue-line treatment of plywoods. Among organophosphorous insecticides, emulsified forms of chlorpyrifos, dichlofention and diazinon were more stable than others. Fenitrothion, pyridafenthion and phoxim were not practically acceptable as emulsifieable forms due to the relatively low recovery rates aft...
S Fushiki, Y Katuzawa


Copper linoleate: A new low toxcity wide spectrum, heavy duty wood preservative
1995 - IRG/WP 95-30082
Copper linoleate, a "fixed" copper soap has been developed and evaluated in South Africa over a 30-year period. The initial product, an organic solvent based preservative has been tested in pine poles against termites and fungi. Results indiate that the product has performed well against existing heavy duty wood preservatives such as CCA and creosote in long term field trials (30 years). The paper...
D Conradie, P Turner, W E Conradie, A J Pendlebury, T Pizzi


Effect of boron compounds-furfuryl alcohol treatment of wood on dimensional stability, termite resistance and boron leachability
2001 - IRG/WP 01-40195
Sapwood blocks of Japanese cedar (Cryptomeria japonica) and Caribbean pitch pine (Pinus caribaea) measuring 20 (tangential) x 20 (radial) x 10 (longitudinal) mm were impregnated with furfuryl alcohol (FFA) by a vacuum-diffusion process followed by curing under heating. Boron compounds (boric acid, ammonium borate and ammonium biborate) were mixed in the impregnation solution of FFA. Anti- swelling...
S K Ozaki, M K Yalinkilic, Y Imamura, M F Souza


The Protection of Wood with Oxy-aluminium Compounds
2002 - IRG/WP 02-30286
Wood inorganic composites (WICs) containing aluminium compounds were developed and tested in relation to some essential requirements of preservative treated wood. Four different oxy-aluminium treatments were developed and identified according to the final insoluble compounds formed (sodium aluminate, aluminium hydroxide, magnesium aluminate and aluminium borate) in wood. Vacuum impregnation or dou...
F A Ximenes, P D Evans


Tebuconazole - A new triazole fungicide for wood preservation
1990 - IRG/WP 3629
The main cause of economic damage to timber and millwork worldwide are Basidiomycetes (brown and white rot). After testing a wide range of triazole derivatives for their effectiveness against decay fungi, Tebuconazole, a triazole compound, was selected. The physico-chemical, toxicological and ecotoxicological data of this substance are described. Tebuconazole is unleachable, light-stable, heat-sta...
R Gründlinger, O Exner


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


The use of natural and synthetical tannins to improve the dimensional stability and durability of beechwood (Fagus sylvatica)
1993 - IRG/WP 93-30016
Synthetical tannins and natural extractives of oak, spruce and chestnut have been combined with different fungicides to make the wood more dimensionally stable and more durable. The anti-shrink-efficiency and the improvement of the durability of different synthetical and natural tannins have been evaluated. The results make clear, that an application of the mentioned agents for common use cannot b...
H Militz, W J Homan


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Improvement in dimensional stability against water of the main Spanish timbers impregnated with water repellent organic protectors
1988 - IRG/WP 3468
The study reported the increase of dimensional stability against water of the main Spanish timbers, both broadleaved and coniferous, after impregnation in the autoclave with organic protector, with contains 33.3% water repellent waxes and resins. The proposed Spanish standard, U.N.E. n° 56541 is used, where dimensional stability of the impregnated wood is expressed as a% of that of the non-impreg...
J A Rodríguez Barreal


Stability, performance and distribution of propiconazole (R 49362) in acceleratedly aged wood
1991 - IRG/WP 3647
The permanency of propiconazole (R 49362 - WOCOSENÔ technical - Janssen Pharmaceutica) in wood was examined in an 18 month storage test, an evaporative ageing study (EN 73), a volatilization stress experiment, and water-leaching studies (EN 84). The biological efficacy against two brown rot fungi: Coniophora puteana BAM Ebw. 15 and Gloeophyllum trabeum BAM Ebw. 109 was assessed according to the E...
A R Valcke, M Stevens


Effect of post-treatment drying schedule on the modulus of elasticity of CCA-treated southern pine dimension stock using nondestructive methods
1987 - IRG/WP 3413
This paper describes the results from the nondestructive testing for modulus of elasticity (MOE) of southern pine (Pinus sp.) 2 x 6's treated with chromated copper arsenate and redried using three commercial kiln schedules. The data indicate that redrying CCA-treated southern pine dimension stock treated to above-ground retentions (4 kg/m³) has no deleterious effect on the MOE, regardles...
H M Barnes, S Moore


Durability of Wood/Plastic Composites Made From Parthenium species
2002 - IRG/WP 02-40225
Previous study indicated that the natural chemical constituents of the guayule plant (Parthenium argentatum) improved some durability properties of wood when it was treated with resin extracted from guayule. At present, there are about a dozen species of Parthenium growing in the North American continent. P. argentatum is the only species with harvestable amounts of the rubber latex. Other specie...
P Chow, F S Nakayama , J A Youngquist, J H Muehl, A M Krzysik


The effect of heat treatment on the properties of spruce
1994 - IRG/WP 94-40032
The effect of high temperature treatment (above 150°C) on the wood quality is studied at the VTT. Improved dimensional stability, lower equilibrium moisture content and increased durability against biodeterioration is achieved, depending on the environmental factors. The biodeterioration resistance of spruce is improved due to changes in chemical composition and lower equilibrium moisture content...
H Viitanen, S Jämsä, L Paajanen, A J Nurmi, P Viitaniemi


Dimensational stabilisation of wood
1981 - IRG/WP 3171
A review is given of the studies on the dimensional stabilisation of wood which have been carried out in the laboratory 5.14 "Wood Technology" since 1967. All stabilisation methods known have first been compiled from the available literature. Practical studies were then started. Wood was treated with monomers (styrene, methyl metacrylate, isocyanate), formaldehyde, tannin and sugar. Despite a sati...
A Burmester


Solution stability and Mechanical properties of Chitosan treated Pine
2005 - IRG/WP 05-30377
During the last years the research on chitosan as a wood preservative has been enhanced. Up to now, most of the research has been applied to the anti-fungal properties of chitosan, and no research was conducted on the solution stability of chitosan solutions in repeated trials by impregnation of wood, or on the mechanical properties of chitosan-treated wood. In this paper, the stability of high- a...
E Larnøy, M Eikenes, H Militz


Characteristics of thermally modified wood in vacuum
2004 - IRG/WP 04-40287
In commercial thermal wood modification processes nitrogen, steam or oil has been used for the reduction of oxygen content in the reactor atmosphere. In present study no special heating medium, but an initial vacuuming step has been used for this purpose. Mass loss, resistance to fungal decay, dimensional stability, bending strength and modulus of elasticity of heat treated wood were evaluated and...
G Rep, F Pohleven, B Bucar


Effect of aqueous polymer treatments on wood properties. Part 1: Treatability and dimensional stability
1990 - IRG/WP 3610
Partially air-dried sapwood of sweetgum (Liquidambar styraciflua) and southern pine (Pinus spp.) was treated with either aqueous polyacrylate or aqueous dimethyloldihydroxyethyleneurea (DMDHEU) solutions. Tests for dimensional stability were conducted on matched treated and untreated pieces. Measurement of the antishrink efficiency indicated that DMDHEU was a better stabilizer than the polyacrylat...
Z Ashaari, H M Barnes, R C Vasishth, D D Nicholas, D E Lyon


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


Stability of bifenthrin in a commercial phenol-formaldehyde plywood glue
2003 - IRG/WP 03-30311
Liquid phenol formaldehyde (PF) glue mixes used for plywood manufacture are strongly alkaline. At this pH insecticidal additives may not be stable for long periods. In order to establish practical working life of the synthetic pyrethroid insecticide, bifenthrin, in liquid PF glues the concentration of bifenthrin in the glue mix was measured under laboratory conditions over a 24 hour period. Glu...
M J Kennedy, P A Collins, R D Vella


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


Previous Page | Next Page