The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Resin bleed after light organic solvent preservative treatment - the effect of drying method and process type
1986 - IRG/WP 3378
The effects of drying method and treatment process type on resin bleed were investigated. High-temperature drying of resinous radiata pine (Pinus radiata D. Don) heartwood resulted in improved wood permeability, higher preservative uptake, and greater resin bleed when treated by the Rueping process. Resin bleed was reduced substantially when timber was treated by the Lowry process, and totally eli...
P Vinden


Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


Kiln drying of CCA-treated wood - Some safety and environmental considerations
1987 - IRG/WP 3443
Vapours and condensate from a condenser kiln in which CCA-treated wood was being dried have been collected and analysed. The concentrations of arsenic, copper and chromium found in the vapours from the drying process were well below Swedish threshold limit values. The contents of arsenic and chromium were also low in the condensate, although the copper content was fairly high. The latter result wa...
J Jermer, B Lundberg


Dip-diffusion of dressed timber - Effect of drying
1989 - IRG/WP 3509
The effect of drying on dip-diffused dressed freshly sawn timber was determined by the depth of penetration of boron achieved on the two test timber species, White cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that light density White cheesewood was completely penetrated even after 3 days drying while Light hopea, treated immediately achieved 5.2 mm p...
H C Konabe


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


Laboratory tests on artificial weathering of Quercus rubra crossties
1986 - IRG/WP 2252
Clear red oak (Quercus rubra) blocks were used to evaluate various types of accelerated aging tests including boil, steaming, and cyclic weathering. It was found that the repeated vacuum and pressure treatment of wood in water, steaming, oven-dry, and freezing appeared to be most effective in reducing the MOE in compression and hardness modules of wood specimens. Red oak crossties which were press...
P Chow, A J Reinschmidt, E J Barenberg, S L Lewis


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Effects of drying processes on termite feeding behaviour against Japanese larch wood
2001 - IRG/WP 01-10390
We investigated the effects of current drying schedules for larch lumbers on the termite feedings. Thermal analyses were also conducted to investigate degradation of wood components. Choice feeding tests showed specimens dried under high-temperature schedules were evidently susceptible against termite attacks. These schedules produced the feeding-attractants, which were suggested by the TGA result...
S Doi, Y Kurimoto, H Takiuchi, M Aoyama


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Leaching from CCA-impregnated wood to food, drinking-water and silage
1987 - IRG/WP 3433
During the last years The Norwegian Institute of Wood Technology (NIWT) has analysed different foodstuff for contamination by copper, chrome and arsenic from CCA-impregnated wood. There has been some interest for using CCA-impregnated wood in contact with food and drinking-water. Before giving their permission the Norwegian Health Authorities want results from experiments. NIWT therefore started t...
F G Evans


Trial to determine a suitable schedule for radial and longitudinal treatment of plug samples by comparison of changes in the fluid retention and the treated area
2001 - IRG/WP 01-40211
A full-cell process was carried out using different treatment schedules for radial and longitudinal samples because of the anisotrophy of flow. When timbers are impregnated with preservatives much better penetrations are obtained via the end grain than laterally (across the grain). Therefore, suitable schedules for radial and longitudinal flow directions were determined in an trial experiment usin...
I Usta


A note on te seasoning, preservative treatment and suitability of debdaru (Polyalthia longifolia Benth & Hooker.) for poles
1995 - IRG/WP 95-40056
The main work is to determining the suitability of Debdaru (Polyalthia longifolia Benth.) as poles from Government and Village forests are investigated. The poles of Debdaru are easily treatable with CCA preservative by full-cell pressure method, but difficult to dry (air & kiln). Proper quality control must be maintain from procurement to treatment, specially during physical selection & d...
G N M Ilias, M D Rokib-ul-Hafiz


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg


The effect of preservative distribution in small blocks of Pinus sylvestris on the toxicity of tributyltin oxide to Reticulitermes santonensis Feytaud
1971 - IRG/WP 206
Small blocks of Pinus sylvestris (50x25x15 mm³) were treated by a full-cell method with various concentrations of tributyltin oxide in benzene. Replicate blocks were then freeze dried, rapidly air dried or slowly air dried and exposed to surface attack by the subterranean moistwood termite Reticulitermes santonensis Feytaud. At all concentrations it was found that the freeze-dried blocks were mor...
M P Levi, D N R Smith