Your search resulted in 237 documents. Displaying 25 entries per page.


Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller


Inspection results of preservative treated stakes, maximum 33 years in field
1992 - IRG/WP 92-3690
Since in 1958, we have undertaken field experiments in Japan. For these field experiments, we used sapwoods of Japanese cedar called Sugi (Cryptomeria japonica) because of majority of plantation forest soft wood species in Japan. For some preservatives, we added sapwood of Japanese beech called Buna (Fagus crenata), a main Japanese hard wood species. Dimensions of these specimens were 30 x 30 x 60...
K Suzuki, K Yamamoto, M Inoue, S Matsuoka


Depletion of boron and copper from CCB treated test specimens using different leaching protocols
2004 - IRG/WP 04-50208
The objective of this study was to measure the depletion of inorganic wood preservative components regarding the proposed OECD guideline "Estimation of emissions from preservative-treated wood to the environment: laboratory method for wooden commodities exposed in the use class 4 and 5" as part of the project "Investigations concerning the influence of test parameters on the release of biocidal ac...
E Melcher, R-D Peek, U Schoknecht, R Wegner


Preliminary results of investigations on screening test of chemical compounds suitable for the preservation of lignocellulosic materials against biodeterioration
1976 - IRG/WP 262
This paper investigates the possibilities of reducing the time needed for the determination of the effectiveness of chemical compounds from the point of view of their eventual application to lignocellulosic materials for preservation against decay and soft-rot....
K Lutomski, S S Neyman


Results of co-operative studies on determining toxic values against wood-destroying Basidiomycetes. Preliminary report to Sub-group members
1986 - IRG/WP 2271
A F Bravery, J K Carey


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Exposure trial at tropical marine sites of pyrethroid/creosote mixtures as wood preservatives: Preliminary results
1989 - IRG/WP 4155
Pinus sylvestris sapwood blocks measuring 25 x 25 x 200 mm³, impregnated using a Lowry or Rüping pressure treatment cycle with solutions of permethrin, cypermethrin or deltamethrin in BS144 creosote, have been exposed at marine sites in Australia, Papua New Guinea, the U.K. and Singapore. The effectiveness of these solutions in preventing marine borer attack is being compared with the efficacy o...
S M Cragg


Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler


Determination of the preventive efficacy against wood destroying basidiomycetes fungi, EN V 839 - CEN/TC 38 WG 9
1993 - IRG/WP 93-20015
The WG 9 of CEN TC/38 has presented to EC a mycological test to assess efficacy of preservatives applied by surface process. This method is now an experimental standard (EN V 839) which has to be approved by the different european delegations. The following paper is not the standard as it has been proposed but is a presentation of the principle of the method. The experimental standard specifies a ...
D Dirol


Rapport sur l'activité du CEN/TC 38
1983 - IRG/WP 2204
M Pottevin


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner


Update on lab and field test results for polymeric alkylphenol polysulfide treated wood
2002 - IRG/WP 02-40240
The possibility of using Polymeric Alkylphenol Polysulfide (PXTS) as a wood preservative has been undergoing evaluation in our laboratories for the past four years. Various formulations prepared from this compound have been tested and found to be effective against wood decay fungi and insects in field stakes after 42 months exposure. In accelerated soil bed tests, PXTS has been shown to be consi...
J Goswami, A Abramson, R Buff, D D Nicholas, T Schultz


Results on termite resistance of building materials against Coptotermes formosanus by choice test
1998 - IRG/WP 98-10275
Various building materials, included wood species, wooden board materials, thermal insulation materials and fire-protection materials, were tested for grading of termite resistance against Coptotermes formosanus. The dimension of most specimens were 2x2x2cm3. Ten repeats were prepared. The specimens were put between Akamatsu sapwood control specimens on a laboratory cultured mound colony of termit...
K Suzuki, K Hagio


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


Proposals for collaborative work on laboratory soft rot testing
1986 - IRG/WP 2265
Proposals for collaborative experiments based on soil burial are presented. It is intended to study the use of defined horticultural loams with a view to obtaining more reproducability in laboratory soft rot tests....
D J Dickinson, S M Gray


A comparison of the effectiveness of a vacuum oven and a wind tunnel in the accelerated ageing of treated wood by evaporation
1989 - IRG/WP 2334
R J Orsler, G E Holland


Bibliographie sur les produits organiques en solvant pour la préservation du bois
1971 - IRG/WP 38
H Alliot


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie


Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki


Field Test Results after Nine Years for CCA and ACQ Preservative-treated Wood Fixed in Different Climates
2003 - IRG/WP 03-30303
During assessment of the ground contact stakes in the Norwegian test field, we have frequently found that the first visual rot attack is in the zone of the stakes, where the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour. To inves...
F G Evans


Previous Page | Next Page