Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


Evaluation and approval of wood preservatives. Unification of European requirements
1988 - IRG/WP 2310
This paper reviews the current activities within the European Homologation Committee for Wood Preservatives (EHC) towards unification of the requirements on evaluation and approval of wood preservatives in Western European countries....
J Jermer


Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Current models used by the European Health Authorities to evaluate the volatilization of active ingredients from treated wood used inside dwellings. A case study: Volatilization of azaconazole and propiconazole from treated wood
1990 - IRG/WP 3565
The use of wood preservatives inside houses may result in measurable aerial concentrations of active ingredients. These airborne contaminants may be inhaled by the inhabitants over periods lasting from a couple of days to several months. To assess the potential health hazard of preservative residues in the air, various risk-assessment models have been worked out. Three schemes, currently used by t...
A R Valcke, L Van Leemput


Autoxidation of beech condensate
2003 - IRG/WP 03-40261
Liquid effluent from steaming beech wood was studied. The effluent contains many phenolic compounds which can present a significant toxicity. The effluent was treated by oxidation was carried out at 250 rpm for 30 min with NaOH. This was followed flocculation with CaCl2 for 30 min. The influence of parameters such as pH, time of autoxidation were studied. Experimental results reveal the electrosta...
M Irmouli, J P Haluk


Protection of beech veneer for fruit and vegetable boxes
1981 - IRG/WP 3176
In Yugoslavia about 50,000 m³ of low quality beech logs annually are rotary cut into veneer from which boxes are made for transporting fruit and vegetables. Because of steaming before rotary cutting, beech veneer becomes extremely sensitive to mould attack which decreases the quality and commercial value of the final product. To avoid mould attack, veneer sheets are dried to 16% moisture content ...
N Vidovic


Comparison between the Hylotrupes bajulus strains of different European laboratories
1980 - IRG/WP 1118
In several European countries, wood preservatives of the same formulation are subjected for the quality label to particular tests according to standards established by the CEN. The different laboratories which carry out these tests have had their cultures for many years. The insects are kept in optimal nutritional and climatic conditions and have always mated amongst themselves. On the one hand, e...
M-M Serment


Incursion of Hylotrupes bajulus Linnaeus (European House Borer) into Western Australia
2005 - IRG/WP 05-10558
In January 2004, an adult Hylotrupes bajulus Linnaeus was detected emerging from a beam of Pinus pinaster in a house in Perth, Western Australia. The timber had been locally grown and milled. Surveys to define the extent of the infestation show it is restricted to dead pine trees in 28 sites around Perth. The biological and economic feasibility of eradication is being assessed. Since about 2001, k...
M Grimm


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


Work programme of CEN/TC 38 (March 2000) and European publications
2000 - IRG/WP 00-20206
Remind of stage significance Stage 32 : Working document existing and circulated in the technical body (TC, WG). Stage 40 : Document available in the CEN/CS to start CEN/CENELEC enquiry (6 months). Stage 43 : Second CEN/CENELEC enquiry started (2 to 4 months). Stage 49 : Document available in the CEN/CS to start formal vote or ENV vote. New scope of the CEN/TC 38 " Standardization of the nat...
R Hüe


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


European laboratory termite testing
1986 - IRG/WP 1299
As with all testing of wood preservatives the evaluation of the resistance to termites of treated wood requires methodology which is approriate to, and can be readily extrapolated to, the practical situation. Thus not only must the variations in possible treatment systems be taken into account (eg dip, brush or pressure application) so too must the range of termite species and the type of exposure...
R W Berry


Fungi used in standard tests on the toxicity value of wood preservatives in various European countries
1975 - IRG/WP 255
The aim of the present paper is to make the comparative analysis of test fungi used in various European countries in order to define the toxicity value of wood preservatives against fungi of the Basidiomycetes class. Only the methods with national standard rank, present on the currently binding standards list are taken for consideration. The analysis of similarities and differences in the choice o...
J Wazny


Comparative life cycle assessment of Swiss railroad sleepers
1998 - IRG/WP 98-50117
The results of an environmental LCA carried out on railway sleepers made of prestressed concrete, sectional steel and creosote impregnated beech as used on main lines of Switzerland's railways are presented. All extractions from and insertions into the environment which were connected with the manufacture, use and disposal of the different types of sleeper were inventoried and assessed, i...
T Künniger, K Richter


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...
A Karimi, M Ghorbani


Commercial potential of the four-cycle method for the impregnation of green beech sleepers in Yugoslavia
1975 - IRG/WP 347
This paper was presented to the Conference on Wood Protection held in Sarajevo (Yugoslavia) in 1973. The paper was based partially on the report prepared by J. Struhar and G. F. Franciosi, who were appointed in 1972 as FAO consultants to demonstrate the new impregnation process for green beech sleepers in Yugoslavia. The so-called 4-cycle method was developed at the State Forest Research Institute...
N Vidovic


Towards harmonisation of regional approaches for an International Standard for the approval of wood preservatives
1997 - IRG/WP 97-20122
Recent proposals from the European Standards body (CEN) for an ISO Standard on wood preservatives has initiated debate on whether there is any prospect of an acceptable common approach among ISO member countries, to a harmonised framework of hazard classes, with agreed supporting biological tests, leading to a unified rationale for demonstrating compliance with minimum performance standards for sp...
A F Preston, A F Bravery


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp