Your search resulted in 58 documents. Displaying 25 entries per page.


The effects of preservative treatment and exposure to wood degrading fungi on fiber reinforced polymer (FRP) materials used for structural wood reinforcement
2001 - IRG/WP 01-40204
Glass fiber reinforced phenolic (GFRP) composite materials are becoming increasingly accepted for use in the construction industry because they combine advantages of both wood and advanced polymeric materials. Addition of only 1-3% FRP in the tension zone, for example, can typically improve the strength of the hybrid system by 200%. As more applications are found for wood/FRP hybrids, (e.g. lamina...
C Tascioglu, B Goodell


Development and Implementation of a DNA – RFLP Database for Wood Decay and Wood Associated Fungi
2004 - IRG/WP 04-10527
We are developing Restriction Fragment Length Polymorphism (RFLP) and Internal Transcribed Spacer (ITS) sequence databases for wood decay basidiomycetes and other fungi associated with wood. These databases currently house information for 39 fungal species consisting of 9 brown-rot basidiomycetes, 12 white rot basidiomycetes, 1 soft rot, 1 stain fungi, and 16 molds or other ascomycetes or imperfe...
S V Diehl, T C McElroy, M L Prewitt


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson


Fungal decay resistance of Rubber wood treated with heartwood extract of Rosewood
2005 - IRG/WP 05-30367
Alcoholic extract of Dalbergia latifolia heartwood was studied for its toxicity towards wood decaying fungi. Rubber wood blocks were treated with this extract to three different retention levels (0.1%, 0.2% & 0.5%) and the treated wood blocks were assessed for their resistance towards two white rot and two brown rot fungi. Treated blocks showed improved resistance over the control blocks. At 0...
A K Sethy, H C Nagaveni, S Mohan, K T Chandrashekar


Production of monoclonal antibodies to fungal metabolites
1986 - IRG/WP 1306
The role of fungal extracellular enzymes in wood biodegradation is incompletely understood. Our lab is beginning a project utilizing monoclonal antibodies to characterize extracellular metabolites of the brown rot fungus Poria placenta Fr. (Cooke). Monoclonal antibody technology takes advantage of the ability of antibody secreting spleen cells from immunized mice to fuse in the presence of polyeth...
J Jellison, B Goodell


Inhibition of the biodegradation of coniferous and broadleaved wood by new imidazolium salts
2003 - IRG/WP 03-30320
Studies were carried out on fungicidal values of fourteen potential wood preservatives – modified quaternary heteroaromatic compounds using the screening agar-block. The vacuum treated blocks (22mm x 17mm x 12mm) of Scots pine (Pinus sylvestris L.), spruce (Picea excelsa L.), beech (Fagus silvatica L.) and birch (Betula verrucosa Ehrh.) with testing compounds were exposed to Coniophota puteana a...
J Zabielska-Matejuk, J Pernak, W Wieczorek


The characteristics of biodegradation mechanism of gamma-irradiated wood
2007 - IRG/WP 07-20352
Gamma radiation, as an easy, fast and effective sterilisation method, changes molecular structure in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in wood properties crucial for laboratory testing of wood-preservative effectiveness. Natural durability of wood against rot fungi in lab conditions dependency on different sterilisat...
R Despot, M Hasan, F Pohleven, M Humar, G Rep


Chelator-Mediated Fenton Chemistry in Wood Degraded by Fungi
2007 - IRG/WP 07-10618
Wood specimens were colonized by individual isolates of brown rot, white rot, soft rot and blue (sap) stain fungi. Ethyl acetate extracts of the ground wood were analyzed for their iron-reducing capabilities using a ferrozine-based assay. Extracts from wood colonized by brown rot fungi showed a significantly greater iron-reducing capability than extracts from wood colonized by white rot fungi or n...
B Goodell, G Daniel, J Jellison, Yuhui Qian


The Current Situation Of Wood Poles Installed In Ilha Do Mel: A Wood Pole Biodegradation Diagnostic
2007 - IRG/WP 07-40373
Wood CCA and CCB poles installed in Ilha do Mel, an island of Parana State, Brazil, are failed earlier than expected: just five years after being installed many poles need to be replaced with financial implications for the State Energy Company – COPEL. In an effort to answer what causes this failure, this work shows the deterioration diagnostic of Ilha do Mel’s poles. In fact, such poles have...
C C Borges, J C Moreschi


Practice Makes Perfect: A Biodeterioration Diagnostics Database that Makes Practice
2008 - IRG/WP 08-10648
Replacement of bio-based materials deteriorated by pests costs billions annually and wastes natural resources. Wood replacement rates have remained relatively stable despite significant advances in wood preservation. This may be explained, in part, by poor end-use by uninformed users and by inadequate pest management once products are in service. This problem may be exacerbated by two opposing fac...
J S Schilling


Wood boring species present in the Tagus Estuary and the severity of their attack on wooden piles exposed in the area: a case study
2008 - IRG/WP 08-10664
Wood exposed in the marine environment is subject to degradation by wood boring organisms. This is probably one of the reasons why wood has been substituted by concrete and steel in maritime structures in many European coastal areas. Wooden piles obtained from a wharf exposed in the Tagus Estuary, Porto Brandão (Almada, Portugal) provided an opportunity to understand the main agents of biodeter...
L M S Borges, L Nunes, A A Valente, P Palma


Utilidad práctica de mini estacas en ensayos de campo
2008 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Fungal Attack on Lignin and Cellulose: Elucidation of Brown- and White-Rot Mechanisms Comparing Biomimetic and In-Vivo Degradation Patterns
2010 - IRG/WP 10-10714
This paper examines research and hypotheses that have been developed over several years on wood degradation mechanisms. This information is combined with new data and analyses to explain why wood decay patterns caused by brown-rot fungi and specific types of white-rot fungi are different. New data, including work with both biomimetic studies on low molecular weight compounds, degradative enzymes, ...
V Arantes, B Goodell, A M F Milagres, Yuhui Qian, T Filley, J Jellison, S Kelley


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Degradations and conservation strategies for an XVIII-th century wooden church from Oltenia County, Romania
2010 - IRG/WP 10-40521
The wooden churches construction has a rich tradition in Romania, the technique spreading from North – Maramures, to South, especially in hill and mountain areas. The church from Ursi village, Oltenia County, represents a particular case, the church being abandoned since 1913. The lack of a roof for a long time resulted in severe deterioration of the whole structure. Yet the inner and outer wall...
G Niculescu, O Chachula, A Nicolaescu


Fungal biodegradation of CCA-treated wood wastes
2011 - IRG/WP 10-50276
Fungal biodegradation could be employed as a pretreatment method to alleviate problems caused by landfill disposal of CCA-treated wood wastes (e.g. a shortage of landfill space and a release of leacheate). It could be used to decrease the volume of waste and to remove metals from waste simultaneously. We have screened hundreds of decay fungi, including fungi isolated from CCA-treated wood in servi...
Gyu-Hyeok Kim, Yong-Seok Choi, Jae-Jin Kim


Decrease of stiffness properties of degraded wood predicted by means of micromechanical modeling
2011 - IRG/WP 11-40570
Wood exhibits a highly anisotropic mechanical behavior due to its heterogeneous microscopic structure and composition. Its microstructure is organized in a strictly hierarchical manner from a length scale of some nanometers, where the elementary constituents cellulose, hemicelluloses, lignin, and extractives are found, up to a length scale of some millimeters, where growth rings composed of earlyw...
T K Bader, K Hofstetter, G Alfredsen, S Bollmus


Improvement of the biological performance and dimensional stability of two tropical woods by thermal modification
2012 - IRG/WP 12-40605
Pink cedar wood and rubberwood were thermally modified at 230°C in air for 4 h or for 8 h, and then subjected to bending, compression and hardness tests to evaluate the effect of the treatment on these mechanical properties. The biological performance of the modified wood was also determined, according to EN113, and the dimensional stability measured by means of the anti-swelling efficiency. The ...
M M González-Peña


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen


What molecular biology can tell us about the biodegradation of lignocellulose: the utilization of molecular techniques for the detection, identification and enhanced understanding of wood degrading organisms
2013 - IRG/WP 13-20528
Molecular techniques are now routinely used in the identification, detection and analysis of wood degrading organisms. An overview of some of the early work on nucleic acid isolation and characterization will be followed by a discussion of the power of sequencing and other procedures for better understanding: the mechanisms involved in the biological degradation of wood, the metabolic basis of pre...
J Jellison, B Goodell, G Alfredsen, D Eastwood, G Daniel, S M Cragg, J K Grace


Thermal durability and biodegradation of tannin lignin adhesives
2014 - IRG/WP 14-40657
Mimosa tannins and lignosulfonates were used in wood adhesives formulation to substitute resins based on formaldehyde. Mimosa tannins were mixed with either glyoxalated sodium lignosulfonates or glyoxalated ammonium lignosulfonates. The ratios of mimosa tannins and sodium lignosulfonates varied from 20% tannins to 60% tannins. The thermal durability of the adhesives were analysed by thermogravimet...
L Chupin, B Charrier, A Pizzi, F Charrier


Evaluating the Effects of Post Dip-Treatment Laser Marking on Resistance to Feeding by Subterranean Termites
2016 - IRG/WP 16-10854
Dip-treatment of wood packing materials is often used instead of pressure treatment mainly because of issues relating to simplicity and cost. Packaging boxes fabricated for the United States Army are required to be dip-treated for at least one minute in an approved preservative solution prior to use. These boxes are expected to have a service life of up to 20 years in a wide variety of environment...
R A Arango, B Woodward, S Lebow


Biodegradation of creosote by white rot fungus Phanerochaete chrysosporium and a strains of Pseudomonas
2017 - IRG/WP 17-50329
The aim of this study was to determine degradation effectiveness of polycyclic aromatic hydrocarbons (PAH) contained in creosote by white rot fungus and bacteria. The following two species of bacteria Pseudomonas putida and Pseudomonas sp. as well as Phanerochaete chrysosporium fungus characterised by the ability to decompose aromatic compounds were selected for experiments. Bacterial strains were...
J Zabielska-Matejuk, A Stangierska, A Kropacz, E Kaczorek


Exploration of waterlogged piles and wooden constructions of Riga Dome Cathedral
2017 - IRG/WP 17-10901
The Riga Dome Cathedral’s waterlogged wood piles and the roofs and tower's wooden structures were investigated, the extent of biological damage was evaluated, and the wood rot fungi and insects were identified. The pile wood’s component composition and elemental composition were analysed; the wood structure damage by erosion bacteria was microscopically determined. In the roofs and tower ...
B Andersons, I Andersone, I Irbe, V Fridrihsone, R Lūsis