A proposal for an international wood preservation standard
1994 - IRG/WP 94-20031
Two factors are driving the need for an international wood preservation standard. First, the global need to use our natural resources more wisely and second, the movement towards free trade exemplified by the General Agreement on Tariffs and Trade. The International Research Group on Wood Preservation is the ideal organisation to undertake the task of developing such a standard. This paper is inte...
P I Morris


Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


European standardization for wood preservation
1989 - IRG/WP 2335
G Castan


Proposed standard laboratory method for testing fungicides for controlling sapstain and mould on unseasoned lumber
1977 - IRG/WP 292
This laboratory method is for determining the effective concentration, or concentration for zero growth (CGo), for fungicides or preparations of fungicides which are potentially useful in protecting packaged or unseasoned lumber in storage and shipment from biodeterioration by sapstain fungi and moulds. The test is rapid and may be completed in three weeks and gives a good indication of the toxici...
A J Cserjesi


Conforming to european standards for preservative-treated timber: Specifying with confidence
2000 - IRG/WP 00-20194
A four-year collaborative study between four industrial partners and BRE has assessed timber treated by current UK industrial practices in the light of current European Standards. Data were collected for CCA and creosote treated timber components, and compared with the requirements laid out in EN351-1 and -2. A number of difficulties were encountered that have been described in previous IRG papers...
E D Suttie, R J Orsler


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Draft Business Plan of CEN/TC 38 - Durability of wood and wood-based products - Introduction
2000 - IRG/WP 00-20207
CEN Technical Committees and Business Planning. The extension of formal business planning to CEN Technical Committees (CEN/TCs) is an important measure which forms part of a major review of business processes (known as 'Optimization'). The aim is to align the CEN work programme with expressed market needs and to ensure the adequate resourcing of projects through their development...
R Hüe


Mycological testing of plywood and board materials. Part 1: Review of information supplied by IRG members
1978 - IRG/WP 284
In December 1975 IRG members were asked for published information, information of current work in progress and views on mycological test methods for board materials. The object was to stimulate discussion and possibly establish a joint research effort within IRG in order to establish a meaningful test with reproducible results....
C R Coggins


A critical review of the AWPA standard method (M12-72) for laboratory evaluation to determine resistance to subterranean termites
1986 - IRG/WP 1298
The American Wood Preservers' Association standard (M12-72) for evaluation of candidate wood preservatives against subterranean termites is reviewed and suggestions for revision are made. The most serious flaws in the current test procedure involve a failure to recognize inter- and intraspecific variation and a lack of quantification of test results....
J P La Fage, M Jones


European standardization for wood preservation
1990 - IRG/WP 2359
G Castan


The biocides directive
1995 - IRG/WP 95-50040-25
G Wilson


Wood preservation in East European countries
1989 - IRG/WP 3527
The paper discusses the main problems of wood preservation in Bulgaria, Czechoslovakia, German DR, Hungary, Poland, Rumania and the USSR. The main types of wood preservatives produced have been presented, as well as the state of standarization to test their properties. There have been considered methods of wood treatment in use and application range of treated wood....
J Wazny


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Current models used by the European Health Authorities to evaluate the volatilization of active ingredients from treated wood used inside dwellings. A case study: Volatilization of azaconazole and propiconazole from treated wood
1990 - IRG/WP 3565
The use of wood preservatives inside houses may result in measurable aerial concentrations of active ingredients. These airborne contaminants may be inhaled by the inhabitants over periods lasting from a couple of days to several months. To assess the potential health hazard of preservative residues in the air, various risk-assessment models have been worked out. Three schemes, currently used by t...
A R Valcke, L Van Leemput


Evaluation and approval of wood preservatives in the Nordic countries
1988 - IRG/WP 2311
This paper reviews the system for evaluating and approving the efficacy of wood preservatives for industrial use currently in force in the Nordic countries Denmark, Finland, Iceland, Norway and Sweden....
B Henningsson, J Jermer


Evaluation and approval of wood preservatives. Unification of European requirements
1988 - IRG/WP 2310
This paper reviews the current activities within the European Homologation Committee for Wood Preservatives (EHC) towards unification of the requirements on evaluation and approval of wood preservatives in Western European countries....
J Jermer


Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan


Leaching of CCA from Pinus patula during marine trials in the southern hemisphere
1991 - IRG/WP 4167
Pinus patula stakes were treated with CCA to retentions of 31 kg/m³ salts, and were sited in the sea of Port Alfred, South Africa, for two years. Samples were then removed to the laboratory and analysed as before for copper and arsenic. Prelimiary data showing CAA losses from these stakes in the marine environment showed that CCA was longitudinally leached from them, and was also transversly redi...
G D Shelver, C D McQuaid, A W W Baecker


Practical consideration in developing an international hazard class standard: The hazards and risks
1996 - IRG/WP 96-20091
This paper discusses the concept of hazards and risks in relation to the way in which the hazard class philosophy may be used for international standardization. The difference between hazard and risk is considered as a basis for a simple classification of biological hazards for timber in use based upon its service environment. The paper proposes that the moderating influences within a service envi...
R J Orsler


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


Transmission poles with sub-standard retentions protected by Field Liners outperform standard poles in service
1997 - IRG/WP 97-40095
Eucalyptus cloeziana 12m transmission poles were treated with sub-standard creosote retentions of 80kg/m3 and Field Liners were fitted to the poles before they were placed in service at Umbumbulu, Kwazulu Natal. Poles treated with standard creosote retentions of 130kg/m3 but without Field Liners were also placed in service in the same area. Core samples were taken from both groups of poles after 1...
M R Behr, G D Shelver, A A W Baecker


Previous Page | Next Page