Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


A new concept for the evaluation of wood durability for out of ground contact using accelerated L-joint testing
1997 - IRG/WP 97-20123
Since the wood preservation sector is developing in favour of defining exactly the utilization of wood products and preservation techniques as a function of the envisaged hazard class, more in particular the hazard classes 3 and 4 (EN 350) there is obviously a need for a test method evaluating natural durability for out of ground contact applications. Based on the L-joint test as described in the ...
J Van Acker, M Stevens


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen


Overview of European discussions on Standardisation and list of proposed standards for WPC performance qualification
2006 - IRG/WP 06-20345
The standardisation is a driving force to promote the development of Wood Polymer Composites (WPC) by giving confidence to users and consumers. In Europe, the high interest of WPC require at this time a diffusion of information concerning the performances of WPC products. The WPC performances must be assessed according relevant standards in order to qualify the intrinsic properties of WPC (mechani...
G Labat, M Vernois, T Gay


Study of natural durability of Spanish Eucalyptus globulus wood
2007 - IRG/WP 07-10617
In some countries such as Australia, the wood of Eucalyptus globulus is recommended, due to its high durability, in risk situations where attack by organisms is likely to occur. In Galicia this species has been used for many decades for timber structures, which are still used. However, European Standard EN-350-2 places Eucalyptus globulus in the worst category of natural durability, a situation th...
D Lorenzo, M T Troya, M J Prieto, C Baso, M Touza


Natural durability and anatomical features of teak (Tectona grandis) from plantations in Costa Rica
2008 - IRG/WP 08-10671
Teak (Tectona grandis) possesses superior mechanical properties and durability and is thus frequently used as an alternative to impregnated timber in Europe. Demand on teak has resulted in severe exploitation of the tropical teak forests in recent decades, but today the imported timber originates mainly from plantations and is certificated according to the Forest Stewardship Council (FSC) policy. ...
U J Wolfsmayr, N Terziev, G Daniel


Study on the natural durability of Eucalyptus grandis wood from Argentina
2009 - IRG/WP 09-10689
In Argentina eucalypts are in second place of importance in planted area, after pines. Due to its high growth rates (from 35 to 55 m3/ha/yr), Eucalyptus grandis is the most important among the eucalypts planted in Argentina. Moreover, E. grandis is one of the species with the greatest potential in the country, because of its diversity of uses for high end and added value solid products. Due to the...
D Lorenzo, M T Troya, J C Piter, M Sánchez, C Baso


Study on the natural durability of Eucalyptus globulus wood from Spain
2009 - IRG/WP 09-10690
The wood of Eucalyptus globulus is recommended in some countries, such as Australia, due to its high durability, in risk situations where attack by organisms is likely to occur. In Galicia this species has been used for many decades for timber structures and other uses, which are still used. However, European Standard EN 350-2 places Eucalyptus globulus in the worst category of natural durability,...
D Lorenzo, M T Troya, M Touza, C Baso


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Potential valorization of wood extractives from waste products of steam distillation of Aniba rosaeodora: antitermitic activity
2013 - IRG/WP 13-30629
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. The wood is also composed with alkaloid compounds like anibin. These compo...
N Amusant, A Digeon


Resistance against marine borers: About the revision of EN 275 and the attempt for a new laboratory standard for Limnoria
2020 - IRG/WP 20-20669
Wood protection technology in the marine environment has changed over the last decades and will continue to do so. New active ingredients, newer formulations, and novel wood-based materials including physically- and chemically-modified wood, together with increasing concerns over environmental impacts of wood preservatives, urgently demand a major revision of EN 275 “Wood preservatives – Deter...
S Palanti, S Cragg, R Plarre


Development of procedures for sampling, testing, and classification to determine the biological durability of wood and wood products
2020 - IRG/WP 20-20676
This paper informs about a research project, which deals with several shortcomings and a lack of clarity within EN 350:2016. The project started in January 2020, will run for 3 years, and is operated by the Institute of Wood Technology Dresden (IHD) and the University of Goettingen (UGOE). Determination and classification of durability of wood and wood products against wood-destroying organisms ...
W Scheiding, K Jacobs, S Bollmus, C Brischke


Laboratory durability testing of preservative treated wood products – first attempts and observations
2023 - IRG/WP 23-20697
In the past, durability classes (DC) had been assigned to wood species, sometimes also to homogenously modified wood-based materials such as thermally modified wood. More recently, some standards allow for classifying the biological durability of chemically modified wood, preservative treated wood and wood composites. Even treated products may be subject to durability classification, but necessary...
C Brischke, M Sievert, M Schilling, S Bollmus


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


European Biocides Directive (98/8/EC): Programme for systematic examination of all active substances of biocidal products on the market on May 13, 2000 Article 16(2)
2001 - IRG/WP 01-50166-03
PPT-Presentation...
K Rasmussen, A B Payá Pérez


Comité International Permanent pour la Recherche sur la Préservation des Matériaux en Milieu Marin. Information from the Wood Group
1980 - IRG/WP 460
E G B Jones


Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


Bioaccumulation of pentachlorophenol in rainbow trout and zebra fish muscles
1986 - IRG/WP 3372
The bioaccumulation of pentachlorophenol in Rainbow Trout and Zebra fish has been evaluated by partition coefficient n-octanol/water determination at ph 7 and measured in vivo according to the OECD guidelines and the European directive 79/831/EEC. The obtained results confirm the low bioaccumulation potential of this product in aquatic organims....
J C Palla, M Dion