Collaborative field experiment: Analysis of copper and chromium in stakes of the four reference timbers
1982 - IRG/WP 3213
The stakes analysed belong to the Swedish set of the four reference timbers of the collaborative field experiment (Document No: IRG/WP/367). Before the field exposure 60 mm were cut off the end of each stake. This was done in order to be able to carry out chemical analyses as well as different types of testing. Some of the material has been used in softrot tests (Document No: IRG/WP/1151)....
T Nilsson


Proposed test procedure to determine the effect of timber substrate on the effectiveness of a copper/chrome/arsenic preservative in seawater
1975 - IRG/WP 411
R A Eaton


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1983 - IRG/WP 3269
G C Johnson, J D Thornton


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


The effects of heat treatment on the toughness of beech wood
2004 - IRG/WP 04-40283
The effects of heat treatment on toughness of beech (Fagus orientalis) wood naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 5 x 5 x 5 cm. Heat treatment was than applied to the wood samples at three different temperatures (130 °C, 150 °C and 180 °C) and three different durations (2 h, 6 h and 10 h) under air atmospheres. ...
S Yildiz, Ü C Yildiz, E D Gezer, Ali Temiz, E Dizman


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


Absorption of inorganic salts solutions. Retentions of inorganic salts. Fire retardants
1990 - IRG/WP 3625
The study aims evaluated the impregnation capacity using fire retardants on woods with differents densities. At the same time, impregnation with several fire retardant salts were carried out in order to obtain their absortion and retention in wood....
A Garcia, J Navarro


X-ray analysis of selected anatomical structures in copper/chrome/arsenic treated wood
1973 - IRG/WP 320
Application of analytical electron microscopy to problems in wood preservation has been very limited. Indeed, less than ten workers appear to have published their results using the technique, and of these' only two papers deal with energy dispersion procedures in the scanning electron microscope; the others employ the more familiar wavelength dispersive methods of the electron probe....
H Greaves


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Co-operative Field Experiment: Performance of preservative-treated timber: Report on condition of specimens after seven years installed in New South Wales - Australia
1986 - IRG/WP 3362
R S Johnstone


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


IRG soft-rot stake test - Site 03 Australia. Progress Report No. 3
1982 - IRG/WP 3202
The performance of test stakes was examined after four (4) years. Hardwood stakes treated with CCA showed significant soft-rot attack. The exception to this was Alstonia scholaris which was similar in performance to Pinus sylvestris. A supplementary test containing stakes treated with CBC, PCP and creosote, showed attack in all hardwoods examined. Little decay was found in stakes of Pinus sylvestr...
L E Leightley, R S Johnstone


IRG soft rot stake test. Site: 03 Australia. Progress repor
1980 - IRG/WP 1114
IRG soft-rot test stakes were installed in site 03 Australia 16.6.77. The stakes have been inspected twice, (28.11.78 (Johnson, 1979) and 31.10.79) for signs of decay, and used to obtain fungal isolates. The condition of stakes in the supplementary soft-rot test has also been examined....
L E Leightley, D M Francis, R S Johnstone


Final proposals for collaborative work on laboratory soft rot testing
1987 - IRG/WP 2292
In this paper proposals are made to scope, timbers, preservatives, leaching, drying, soil type, moisture content, soil burial (blocks and stakes), incubation and dry weight determination and the expression of results....
D J Dickinson, S M Gray


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Testing method for the treatability of wood
1994 - IRG/WP 94-40031
In order to test and classify the treatability of wood species in pressure treatment processes with water-based solutions, a laboratory method was developed which allows the testing of small samples and limited sections of a stem, e.g. sapwood. The penetration of different liquids was determined separately concerning the three anatomical directions of wood. The common parameters for pressure impre...
A O Rapp, R-D Peek


The effect of creosote and Basilit on the boards of 4 wood species against destructive fungi in Northern Iran
1989 - IRG/WP 3555
The results of the experiments conducted on the boards of maple, hornbeam, alder and beech, show that under the humid and moderate climate condition of Northern Iran, after 30 months, the witness samples were about 10% destructed by fungi, especially by Schyzophyllum commune and Coriolus versicolor. The impregnated samples by Creosote Basilite using Rueping and Bethell methods, were quite intact. ...
D Parsapajouh


Studies on the destruction by marine wood boring organisms of fishing boats in the Eastern Black Sea of Turkey
1977 - IRG/WP 427
The present paper concerns the problem of fishing boats which are attacked by wood boring organisms in the Black Sea of Turkey. The aims of this study are: 1) to identify the marine wood boring organisms attacking fishing boats in the Northern Black Sea of Turkey; 2) to identify the wood species that are used in boat building construction and assess their durability; 3) to assess the degree of att...
R Ilhan, O A Sekendiz


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Investigation on different variation factors in the results of mycological test and means to reduce and avoid them
1986 - IRG/WP 2264
In order to clarify the causes of the dispersion observed in the results obtained with mycological tests made in accordance with standard EN-113, different factors assumed to be sources of the variations were studied. These included the moisture content of the test samples during the test, the influence of certain technological properties of the wood, the virulence of the fungus strains, the metho...
D Dirol


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...