IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 618 documents. Displaying 25 entries per page.


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


The remaining concentration of inorganic wood preservative components in EN 252 stakes after ground contact
2000 - IRG/WP 00-50159
In order to determine the biological efficiency and the remaining concentration of different inorganic and organic active ingredients during service, EN 252 specimens were impregnated with 3 copper based wood preservatives. The stakes were installed in the test field of the DESOWAG GmbH, Rheinberg, for at least 7 years. At the end of the field test some of these stakes were divided into 10 uniform...
E Melcher, H-W Wegen


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Field Trials with mini-stakes
2002 - IRG/WP 02-20244
In 1995 an extensive field test program with wood mini-stakes, 8 x 20 x 200 mm, was started. In these trials a large number of parameters are being evaluated, including several new wood preservatives, differently chemically modified woods and natural durability of various wood species. The test sites are three fields in Sweden for in-ground and “close to ground” testing, one subterranean termi...
M Westin, A O Rapp, Y S Hadi, T Nilsson


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Effectiveness of wood preservatives by IUFRO's method
1984 - IRG/WP 3305
Pinus elliottii and Eucalyptus saligna stakes treated with 4.9; 6.9; 9.6 and 13.5 kg/m³ of CCA-A, CCA-C and CCB and with 30-50; 60-80; 90-110 and 120-140 kg/m³ of Benzotar and CNSL (cashew-nut shell liquid) were exposed in seven test sites in Sao Paulo State, Brazil. After 4 years it was concluded that the mean useful life of untreated Pinus elliottii stakes was 8 months and of untreated Eucalyp...
G A C Lopez, E S Lepage, O B Neto


In ground performance of wood treated with a substituted isothiazolone
1990 - IRG/WP 3612
Isothiazolones (I.T.A.'s) are a class of biocides that have potential for use as wood preservatives. The substituted ITA, RH-287, (4,5,dichloro-2-n-octyl-isothiazolone-3-one) is being evaluated as a broad spectrum wood preservative. The evaluation program includes in ground stake tests which were established at two test sites in Mississippi, USA The tests used southern yellow pine treated...
L E Leightley, D D Nicholas


Leaching from field test stakes. Part 2: The distribution in and leaching from different parts of test stakes
1994 - IRG/WP 94-50026
Field test stakes treated with Boliden K33 (copper, chromium and arsenic) and Cuprinol Tryck (CT86) (copper and N-alkylbenzyldimethylammoniumchloride) respectively were exposed in ground contact at two different test fields in Sweden and rejected due to decay after 2 to 28 years. Stakes treated with the same preservatives were also exposed during 7 years above ground. The test stakes have been ana...
F G Evans, B Nossen, M-L Edlund


Working plan: Second international collaborative field trial
1995 - IRG/WP 95-20056
This paper describes the scope, objectives, and approaches to be used in the second international collaborative field trial approved by the Scientific Programme Committee for partial funding in 1994. The trial is designed to develop a broad data base on causal mechanisms, interactions, and factor affecting the performance of treated wood in ground contact. The trial encompasses 12 different field ...
H M Barnes, T L Amburgey


Control of wood biodeterioration by fungal metabolites
1992 - IRG/WP 92-1527
Treating wood with different conventional preservative chemicals for protection and economic utilisation is well known. Tough some of these chemicals are toxic to skin, their use as wood preservative is unavoidable as they should be toxic to biodeteriorating organisms also. Recent advances in chemistry of natural products enabled the use of wood extractives as biocidal compounds against biodeterio...
H S Ananthapadmanabha, H C Nagaveni, V V Srinivasan


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


The wood preservative performance of biocide mixtures containing chlorpyrifos
1994 - IRG/WP 94-30055
Chlorpyrifos (O,O-diethyl[3,5,6trichloro-2-pyridyl]phosphorothioate) was evaluated as a wood preservative insecticide in two long term field tests. In the first project, pine sapwood blocks treated with chlorpyrifos (CPF) were exposed to Coptotermes formosanus using an above-ground test format. CPF is effective in protecting wood from attack by this termite, but its activity appears to decrease wi...
P E Laks


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Comparative performance of copper azole and copper-chrome-arsenate treated rubber wood in Australian, Malaysian and New Zealand tests sites
2000 - IRG/WP 00-30213
Rubberwood (Hevea brasiliensis) has been used for non-structural products where appearance is important. It has rarely been used for structural uses where preservative treatment is required. In order to evaluate the in-ground durability of preservative-treated rubberwood, test stakes (20 x 20 x 500 mm3) were treated to four retentions of CCA and copper azole (Tanalith® E) and installed in test si...
J A Drysdale, M E Hedley, E Loh, L T Hong


A field evaluation of modified and unmodified alkylammonium compounds
1987 - IRG/WP 3436
Laboratory soil block studies of alkylammonium compounds (AAC's) at Forintek and other research establishments have shown that they can prevent decay by standard wood-destroying fungi. Their performance in field tests, however, has been disappointing. Following investigation of possible causes for this poor field performance, stakes treated with modified AAC's were installed at W...
J N R Ruddick


Assessment of untreated Papua New Guinean timbers against subterranean termites. Progress Report 1
1990 - IRG/WP 1436
Eight major commercial timber species (Intsia palembanica, Pometia pinnata, Homalium foetidum, Dracontomelon dao, Calophyllum spp., Eucalyptus deglupta, Nothofagus spp., and Alstonia scholaris) were exposed in ground contact against termites. Five replicates of heartwood stakes of 25x25x250 mm³ of each species were randomly embedded in the soil. Results after 24 months exposure showed that Kwila ...
M Rokova, H C Konabe


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


One year performance of graveyard stakes in the Northern Territory of Australia
2006 - IRG/WP 06-30398
This paper presents the one year progress performance of in ground graveyard stakes exposed to numerous termite species and decay fungi in tropical field conditions. The field study examines the efficacy of a new timber preservative formulation developed at the University of Melbourne, Australia. The biocides used in the formulation are fipronil (a phenyl pyrazole) and trimethyl borate. The pre...
B Ahmed, J Hann, S Przewloka, P Vinden, P Blackwell, P Plews


Performance of softwood preservative treated stakes after 4 years exposure in-ground to decay fungi and termites in tropical Australia
2008 - IRG/WP 08-10643
This field study was based on the 1993 IUFRO method and designed as a graveyard (in-ground) test in the tropical region of the Northern Territory to examine the efficacy of novel preservative formulations developed as alternative protection for softwood timber against decay fungi and termites for Hazard Class 3 and 4. This study was supported by the Forest and Wood Products Research and Develop...
B M Ahmed (Shiday), J R J French, S R Przewloka, P Vinden, J A Hann, P Blackwell


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Previous Page | Next Page