Preliminary laboratory bioassay to evaluate engineered Fibre-boards against subterranean termites C. acinaciformis (Isoptera: Rhinotermitidae)
2012 - IRG/WP 12-10768
In Australia, laboratory bioassays with subterranean termites typically contain groups of workers and soldiers in a substrate of moist mound material. This termite substrate may affect termite consumption, and the test materials create a favorable termite condition for the test. The main purpose of this test is to examine the effect of a melamine formaldehyde treatment of wood panels to evaluate t...
B M Ahmed (Shiday), H Militz, B Ozarska, I Ali, L Kloeser


Termite resistance of wood impregnated with phenol-formaldehyde (PF) modified boron compounds
2012 - IRG/WP 12-30604
In order to investigate the effect of phenol-formaldehyde (PF) modified boron compounds on termite resistance of two main plantation-grown wood species, namely, Masson pine (Pinus massoniana Lamb.) and Chinese fir (Cunninghamia lanceolata (Lamb.) Hook.), laboratory termite tests and field tests were carried out according to AWPA standard E1-97 and AWPC protocols/2007. Different concentrations of b...
Jinzhen CAO, Liping YU, Xuexiang HE


Curing kinetics of nano cupric oxide (CuO) modified PF resin as wood adhesive: Effect of surfactant
2013 - IRG/WP 13-40620
The effect of nano cupric oxide (CuO) in combination with surfactants on the curing kinetics of phenol formaldehyde (PF) resin, as well as the bonding strength of plywood prepared using the modified resin were investigated in this study using dynamic and isothermal differential scanning calorimetry (DSC). The result showed that the incorporation of nano CuO along with alkane surfactant made in the...
Wei Gao, Guanben Du


Glue-bond strength of simul (Bombax ceiba) plywood made of Neem (Azadiracta indica) leaves treated veneers
2013 - IRG/WP 13-40647
The glue-bond qualities of plywood made of treated simul (Bombax ceiba) veneers were investigated. The veneers were treated with cold and hot water solution of neem (Azadiracta indica, A. Juss.) leaves of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated simul plywood ...
K Akhter, M A Hashem, S Akhter


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Development of composite furniture using bamboo strips, bamboo mat and rubber wood veneer
2014 - IRG/WP 14-40679
Bamboo offers cost-effective component in panel form is well suited to wood substitute can be used as furniture components. In the present study, borak (Bambusa balcooa ) bamboo were used for manufacturing bamboo panel. Mitinga (B. tulda) bamboo were used for making mat and rubber wood veneers were used for manufacturing mat overlaid veneer board. Borax-boric acid (BB) treatments were given to enh...
K Akhter, M Mahabubur Rahaman, M H Chowdhury, M Zahirul Alam


Penetration of phenol formaldehyde (PF) resin into beech wood studied by light microscopy
2015 - IRG/WP 15-20558
In this study, we examined the distribution and penetration depth of phenol-formaldehyde (PF) resin into wood specimens by light microscopy (LM). Two PF resins from different producers, of concentrations 9, 18 and 27 wt % in water, were vacuum impregnated into European beech wood (Fagus sylvatica) blocks of 15x25x50 mm³. The presence of chemical agent in the wood was carried out by way of their i...
V Biziks, S Bicke, H Militz


Decay resistance of beech wood and plywood treated with different type of phenol-formaldehyde (PF) resins
2016 - IRG/WP 16-40717
In this study treatment of beech and poplar wood veneers with (PF) resin industrial scale and screening tests of nine different phenol-formaldehyde (PF) resins were made. Specifically, the effect of different phenol-formaldehyde (PF) resin types on the resistance of beech wood against brown- and white-rot fungi was evaluated. Criteria for selection of optimal (PF) resin were based on minimum WPG ...
V Biziks, S Bicke, H Militz


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


Lignin-Based Adhesive for Engineered Wood Products
2016 - IRG/WP 16-50319
Lignin as a naturally occurring polyphenolic compound has an excellent potential to replace petroleum-based phenol in formulation of phenol-formaldehyde adhesive that are used in manufacturing of engineered wood products. However, there are three major obstacles in application of polymeric lignin as phenol replacement: 1) low reactivity toward phenol, 2) high molecular weight, and 3) high polydisp...
I Kalami, M Arefmanesh, E Master, M Nejad


Dimensional Stability of Melamine Formaldehyde-Treated Southern Pine
2017 - IRG/WP 17-40774
The objective of this preliminary study was to evaluate the influence of different levels of melamine formaldehyde (MF) and curing cycle on the dimensional properties of southern pine. Thirty samples for each combination of treatment and curing regimen plus untreated controls and controls subjected to the same curing regimen were tested. Shrinkage/swelling coefficients showed that up to 60% ASE c...
H M Barnes, L S Sites, T S F A França, M G Sanders, F J N França


The potential and the challenges of acetylated wood in timber bridges - experiences from an ongoing project
2017 - IRG/WP 17-40792
Acetylated wood is known to be a durable and dimensional stable alternative for high performance materials, and has high potential for exterior timber structures. Research has shown that acetylated wood can be effectively bonded by various adhesive types. However, one of the most common used adhesives for timber constructions, Melamine Urea Formaldehyde (MUF), shows a high degree of delamination o...
A Treu, R Bredesen, F Bongers


Properties and potential use of Irvingia gabonensis and Irvingia wombolu kernel extracts as natural wood adhesives: Towards formaldehyde free wood composite products
2018 - IRG/WP 18-40832
Irvingia species are widely distributed in central and West Africa as well as parts of Asia and are earmarked for domestication due to the multitude of potential products that can be obtained from them. With renewed interest in renewable sources, the current study establishes the feasibility of utilizing extracts from Irvingia gabonensis and Irvingia wombolu kernels as wood adhesives. Proximate an...
A O Alawode, S O Amiandamhen, M Meincken, L Tyhoda


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Longterm Performance of Treated Timbers in Marine Exposures
2020 - IRG/WP 20-10969
The performance of preservative-treated or modified woods in marine exposures was evaluated at test sites in Newport, Oregon, USA and Brisbane, Queensland, Australia. All samples have exhibited excellent performance at the Newport, Oregon site, while attack was more aggressive at the sub-tropical Brisbane site. Acetylated wood as well as samples treated with 7.3% chromated copper arsenate (CCA-T...
M Konkler, A R Zahora, J Norton, J J Morrell


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Phenol formaldehyde modification and termite resistance under laboratory testing
2022 - IRG/WP 22-40952
The development of phenol formaldehyde (PF) resins as a means of impregnating solid wood is one that has been explored for several decades, both in terms of conventional impregnation processing (Impreg) or compressional impregnation (Compreg). However, it is only recently with advances in processing conditions that the method truly affords a means of achieving conventional modification for solid t...
L Nunes, A Pitman, M Duarte, B Stefanowski, D Jones


Long-term Performance of Treated Timbers in a Sub-tropical Marine Exposure
2023 - IRG/WP 23-11015
The long-term performance of preservative-treated and modified wood in marine exposures was assessed in Brisbane, Queensland, Australia. This report describes the final destructive assessment of the surviving Australian panels after 11 years of exposure. This site presents the potential for attack by shipworms (likely Bankia spp.), pholads (Martesia striata), Limnoria and Sphaeroma terebrans. Mos...
E L Galore, J Norton, A Zahora


Resistance of phenol formaldehyde impregnated beech (Fagus sylvativa L.) LVL against biodegradation in soil contact
2023 - IRG/WP 23-40965
Alternatives to preservative impregnation are emphasized in Germany and other European countries. Even though these treatments significantly improve wood's resistance to decay, they often do not have a beneficial impact on the dimensional stability. One alternative product, which may be used in ground contact for items like poles and railway sleepers, could be beech (Fagus sylvatica L.) laminated ...
M Slabohm, C Brischke, S Bicke, H Militz