IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 55 documents. Displaying 25 entries per page.


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Pole yield of some softwood and hardwood species grown in Bangladesh
1999 - IRG/WP 99-40143
Growth study on 9 timber species planted in Bangladesh soils revealed that 6 species fall under wooden electric pole yield group-A, produce 33% poles within 10 years, another 33% within 15 years and additional 33% within 20 years of rotation. Two species under yield group-B produce 33% poles within 15 years and another 33% within 20 years. One species under yield group-C produce at best 25% poles ...
A K Lahiry


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


Standardization of CCA treated 45 hardwood species grown in Bangladesh for REB crossarms
1995 - IRG/WP 95-20059
Researches on 45 hardwood species grown in Bangladesh regarding density, moduli of rupture (MOR), colour and treatability of sapwood and heartwood, seasoning property and natural durability of heartwood revealed that both sapwood and heartwood of 17 species could be full cell pressure treated with CCA at impregnation pressure of 14-18 kg/cm² and only sapwood of rest 28 species could be pressure t...
A K Lahiry


Hardwood Field Experiment: Progress Report 1977-1986
1986 - IRG/WP 3391
The international hardwood field experiment was planned in l976 and set up in same 30 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance. It was hoped that a picture of performance of a range of economically important species would be built up and at the same time provide vital background inform...
D J Dickinson, S M Gray


The influence of drilling patterns on the distribution of toxicants from Polesaver Rods in hardwood poles
1994 - IRG/WP 94-30051
Polesaver Rods are solid rods of wood preservative that are used as a groundline maintenance treatment to control biodeterioration in hardwood transmission poles in Australia. The rods are inserted in holes that are drilled in a prescribed manner to distribute the toxicants into the critical groundline region of the poles. To determine the influence of drilling patterns on the distribution of toxi...
W D Gardner, C N McEvoy


Prevention of non-microbial sapwood discolorations in hardwood lumber: chemical and mechanical treatments
1997 - IRG/WP 97-30137
Sapwood discolorations in hardwood lumber that are non-microbial in origin result from the formation of pigmented starch-like granules in ray parenchyma cells. These discolorations can be prevented by treating unseasoned lumber with an antioxidant (sodium bisulfite). Exposing unseasoned lumber to microwaves or treating logs with fumigants also will prevent these discolorations. Subjecting unseason...
T L Amburgey, S Kitchens


Effects of chemicals used for ground-line protection of hardwood poles on termite attack
1988 - IRG/WP 1356
The majority of chemicals formulatet to protect the groundline of hardwood poles in Australia have been fungicides. Nine products were tested against Coptotermes lacteus attack to determine their value in preventing attack by subterranean termites. Results indicated that Busan, high temperature creosote, pigment emulsified creosote, copper naphthenate gel and "Blue 7" had a repellent effect on Cop...
R S Johnstone, R H Eldridge


The effect of concrete embedment on CCA treated hardwood and softwood timbers
1985 - IRG/WP 3340
Small size stakes of Eucalyptus maculata and Pinus elliottii were treated with CCA to various retentions and embedded in concrete collars containing varying amounts of a fungicide additive. During the 30 month trial period stakes were removed after 12, 18, 24 and 30 months and assessed for residual strength. Stakes which showed significant strength reductions were microscopically examined for the ...
L E Leightley, G A Willoughby


Micromorphology of oak wood degraded by brown rot fungus Coniophora puteana
2000 - IRG/WP 00-10356
To characterize the degradation of hardwood by brown rot fungus, Coniophora puteana was incubated on the wood blocks of Quercus accutissima. For comparison, the same fungus was also incubated on the pine wood blocks of Pinus densiflora. In softwood, the shape of the wood cells and thickness of the cell appeared unchanged even the loss of birefringence in the affected areas. In contrast, oak wood d...
Yoon Soo Kim, Seung-Gon Wi, Kwang-Ho Lee


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


Neem leaves, a potential source for protection of hardwood against wood decaying fungus
2005 - IRG/WP 05-30370
Neem leaves are widely recognized for their insecticidal, pesticidal, fungistatic and fungitoxic ability. The present study is to investigate the efficacy of neem leaves extractives against wood destroying microbes, a brown and a white rot. Neem leaves extractives prepared in various solvents such as petroleum ether, acetone, ethanol, methanol and hot water were tested at a concentration levels of...
S Dhyani, S Tripathi, V K Jain


Extracellular laccase production in brown-rot fungus Coniophora puteana
2001 - IRG/WP 01-10391
Coniophora puteana, one of representing brown-rot fungus, was investigated in terms of extracellular ligninolytic enzyme production. Three fungal strains of C. puteana were inoculated in liquid culture medium with sawdust of pine and oak wood. Extracellular laccase production was observed in some strains of C. puteana in the culture medium with sawdust of oak wood. The highest activity occurred at...
Kwang-Ho Lee, Seung-Gon Wi, Yoon Soo Kim


Lyctine susceptibility testing and dealing with rarely susceptible hardwood species
2007 - IRG/WP 07-10607
This study examined the lyctine susceptibility of 16 timber species or hybrids. Several of the timbers have been placed previously in a ‘rarely susceptible’ category, but for standards and compliance purposes, such in-between ratings are not acceptable. Timber specimens were spot tested for starch content, and exposed to three species of lyctine beetles in an insectary. New criteria were devel...
L J Cookson, J Carr, N Chew, J W Creffield


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


Assessment of the marine borer resistance and abrasion resistance of lesser known hardwood timber species for use in marine construction
2010 - IRG/WP 10-10711
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing both in the laboratory...
J R Williams, G S Sawyer, G Malyon, S M Cragg, J D Icely, J Simm, M Meaden


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Utilization of thermodesorption coupled to GC-MS to characterize volatiles formation kinetics during wood thermodegradation
2012 - IRG/WP 12-40587
Identification of volatile degradation products produced during wood mild pyrolysis is important to have better insight on thermodegradation mechanisms. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during wood thermodegradation indicating an higher susceptibility of hardwoods to thermodegradation compare to so...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Kamdem, P Gérardin


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Best handling practices for wood crossties (sleepers)
2015 - IRG/WP 15-40714
Wooden crossties (sleepers) dominate the rail industry in the USA. Most ties are hardwood treated with oil-borne preservatives using pressure treatment. Incipient decay (called ‘stack burn’) commonly develops during the pre-treatment drying process and reduces tie performance and longevity. Practices to minimize stack burn and enhance wooden tie performance are discussed as an aid to non-wood ...
N Irby, J Lloyd, A Taylor, J Watt


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


A Case Study of Long-term CCA Preservative Leaching from Treated Hardwood Poles in a Humid Tropical Condition
2016 - IRG/WP 16-50324
Chromated copper arsenate (CCA)-treated Malaysian hardwoods have long been used as utility poles, posts, construction piles and motorway fencing in soil contact exposed to the threats of decay fungi and termites. Despite global concerns citing predominantly temperate conditions of long-term leaching of CCA toxic heavy metals from wood into surrounding soils and groundwater since the 1990’s, the ...
A H H Wong, W S M Chin


Superior kempas hardwood protection with two proprietary microemulsion termiticdes based on permethrin and cyermethrin against Coptotermes termite attack under H2 an H3 weathered conditions found in buildings
2018 - IRG/WP 18-10931
SARPECO® and AXIL® solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping treatment but also for vacuum pressure tr...
D Messaudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


Exemplary aboveground hardwood protection from Coptotermes curvignathus under weathered conditions conferred by proprietary microemulsion-based cypermethrin (SARPECO®) and permethrin (AXIL®) biocides
2019 - IRG/WP 19-30749
SARPECO® (with cypermethrin) and AXIL® (with permethrin) solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping tre...
D Messaoudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


An overview of recent studies involving the thermal modification of hardwood species
2019 - IRG/WP 19-40869
This paper outlines recent activities related to the thermal modification of hardwood species, and particularly to tropical hardwood species. Timber demand is ever increasing, but this is being limited by the necessity to protect virgin forest stands. As such, the majority of supply of popular species is being met from juvenile short rotation stands. The limited age from these stands often plays a...
D Jones, M Gaff, F Kacik


Previous Page | Next Page