Experiences from a Danish large scale test by means of a new method of treatment by attack of true dry rot fungus (Serpula lacrymans) in buildings
1994 - IRG/WP 94-10064
Experiences from a new and epoch-making method of treatment in connection with the repair of attack of the true dry rot fungus, Serpula lacrymans (Fr.) S.F. Gray, are described. The paper presents the background of a large scale test comprising repair of more than 150 Danish buildings over a period of approximate 5 years. The method being both gentle to the building and presenting savings of at le...
O Munck, H Sundberg


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Efficiency of wood impregnation processes
1980 - IRG/WP 3151
Many wood impregnation processes have been in use for a very long time, up to 150 years, but they have not been progressively modified. This paper considers impregnation processes in relation to current requirements, particularly impregnation efficiency and energy consumption. The term 'pore' is used throughout in its physical sense and is not confined to botanical 'pore...
B A Richardson


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Soil bed studies of the dimensional stability of composite products
1999 - IRG/WP 99-40134
The influence of boron and isocyanate resin on the dimensional stability of high moisture resistant particleboard was assessed after burial in a soil bed for one month. The samples were treated with two levels of a boron compound and coated in isocyanate resin. The samples were randomly placed in a fungal cellar in soils of two different water holding capacities. Weight differences and dimensional...
K M Filcock, P Vinden


Effects of drying processes on termite feeding behaviour against Japanese larch wood
2001 - IRG/WP 01-10390
We investigated the effects of current drying schedules for larch lumbers on the termite feedings. Thermal analyses were also conducted to investigate degradation of wood components. Choice feeding tests showed specimens dried under high-temperature schedules were evidently susceptible against termite attacks. These schedules produced the feeding-attractants, which were suggested by the TGA result...
S Doi, Y Kurimoto, H Takiuchi, M Aoyama


The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King


Application of energy dispersive X-ray fluorescence spectrometry to the quantitative analysis of organotin preservative solutions and treated wood
1978 - IRG/WP 3125
One technique frequently used for the quantitative analysis of material containing inorganic compounds is energy dispersive X-ray fluorescence spectrometry. It has been shown previously that this technique can be readily used to determine the retentions of chromated copper arsenate and ammoniacal copper arsenate treated wood. This paper reports the results of a preliminary study to determine wheth...
J N R Ruddick


A review of incising as a means of improving treatment of sawnwood
1994 - IRG/WP 94-40019
The use of incising, perforation of the wood surface, is increased because of the need to treat refractory wood species. This paper reviews the development of incising and shows how the required incising patterns can be determined and specified. Most of the development has been in the area of toothed-roller incisors because of their rapid throughput. Needle, Laser, drill and water jet incisors hav...
P I Morris, J J Morrell, J N R Ruddick


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Protection of buildings, other structures and materials in ground contact from attack by subterranean termites with a physical barrier - a fine mesh of high grade stainless stee
1993 - IRG/WP 93-10014
A new type of physical barrier for the prevention of attack by subterranean termites on buildings, other structures and materials in ground contact - a fine mesh of highalloy (originally 304, now 316) stainless steel - has recently been developed and patented worldwide by industry in Australia. The termite resistance of the material was assessed by CSIRO in laboratory and field trials. In the labo...
M Lenz, S Runko


A comparison between high and conventional incision densities for improving preservative treatment of Douglas-fir heartwood lumber
1993 - IRG/WP 93-40009
Incising is required for the preservative treatment of most wood species from the western United States; however, there is considerable debate about the density of incisions required to achieve adequate treatment. Previous studies have shown that the incision effect on treatment is relatively narrow, suggesting that incision densities should be significantly increased over current practices and st...
S T Lebow, J J Morrell


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Environmental consequences of various materials in utility poles - A life cycle analysis
1992 - IRG/WP 92-3726
A model for environmental life cycle analysis, LCA, has been created to compare environmental impact from transmission poles, made alternatively of concrete, steel, aluminium and pine wood treated with CCA type B or creosote. The main pollution sources and energy use are included in the LCA. One pole size, 12 meters long, is presented in the study, a so called "45 kV" pole. Poles of different mate...
M Erlandsson, K Ödeen, M-L Edlund


Comparison of the in-ground performance of pigment emulsified creosote (PEC) and high temperature creosote (HTC)
2000 - IRG/WP 00-30217
A long-term field trial was conducted in Australia to compare the in-ground performance of two oil-borne preservative formulations, conventional high temperature creosote (HTC) and a modified creosote formulation, pigment emulsified creosote (PEC). Three retentions (50, 100 and 200 kg/m³) were targeted for each formulation. An additional retention of PEC formulation (308 kg/m³), which contained ...
J W Creffield, H Greaves, N Chew, N K Nguyen


The loss of insecticidal action from synthetic pyrethroid-treated wood samples: The effect of high temperatures and relative humidities
1992 - IRG/WP 92-1569
This paper describes the results from bioassays using Hylotrupes bajulus, and chemical analyses, of pyrethroid-treated wood samples following storage for up to 3 years. A range of four storage environments was used consisting of combinations of two temperatures (20°C and 40°C) and two relative humidities (60% and 90%). It is concluded from the chemical analyses that, although losses at room temp...
R W Berry, S J Read


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


Tropical In-Ground Durability of Structural Sarawak Hardwoods Impregnated to High Retention with CCA-salts, CCA-oxide and FCAP after 20 Years Exposure
2005 - IRG/WP 05-30384
Statistical analysis (ANOVA) was conducted on durability (termite and decay combined) rating data collected over 20 years exposure period of over 140 species of Sarawak timbers with altogether 30,000 stake specimens, at the Forest Department’s Sibu “graveyard” stake test sites from 1977. About 20 replicated stakes were pressure-treated to refusal with 10% g/ml concentration of up to 3 CCA-sa...
Wang Choon Ling, A H H Wong


Accidental mold/termite testing of high density fiberboard (HDF) treated with borates and N’N-naphthaloylhydroxylamine (NHA)
2003 - IRG/WP 03-10462
High density fibreboard (HDF) was made from beech and pine furnish (50:50) and treated with boric acid (0.1-3%), borax (0.1-3%) or N'-N-(1,8-naphthalyl) hydroxylamine (NHA) (0.1-1%) prior to gluing with urea formaldehyde (UF) resin in order to determine resistance to Eastern subterranean termites (Reticulitermes flavipes Kollar), the most economically important termite species in North Am...
S N Kartal, H H Burdsall Jr, F Green III


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


CCA-treated Wood Disposed in Landfills and Life-cycle Trade-Offs With Waste-to-Energy and MSW Landfill Disposal
2005 - IRG/WP 05-50231
CCA-treated wood as a solid waste is managed in various ways throughout the world. Although some wood is combusted for the production of energy in the U.S., more often than not, CCA-treated wood is disposed in landfills. In other countries, wood, often including CCA-treated wood, is combusted for the production of energy. This paper is presented in two parts. Part I evaluates the impact of CCA-tre...
J Jambeck, K Weitz, T G Townsend, H M Solo-Gabriele