Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Field evaluation of the above-ground susceptibility of Pinus heartwood and untreated or treated sapwood to two species of Australian subterranean termites
1996 - IRG/WP 96-10147
Plantation-grown Pinus elliottii, Pinus caribaea and Pinus radiata specimens containing heartwood and untreated or preservative-treated sapwood were exposed above ground to the subterranean termites Coptotermes acinaciformis or Mastotermes darwiniensis near Sydney (NSW), Brisbane and Townsville (Qld), and Darwin (NT), using a variety of exposure techniques. Heartwood of Pinus elliottii and Pinus c...
M J Kennedy, J W Creffield, R H Eldridge, B C Peters


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Performance of copper-chrome formulations in ground contact in five test sites in New Zealand
1996 - IRG/WP 96-30113
Copper-chrome-arsenate (CCA), copper-chrome-boron (CCB), copper-chrome-fluoride (CCF) and copper-chrome-phosphate (CCP) have been tested at four retentions each in ground contact (25 x 50 x 500 mm³ radiata pine sapwood stakes) for 16 years in five test sites in New Zealand. Results to date show that test site characteristics have a marked effect on relative performance. In a warm and wet site (an...
M E Hedley, R N Wakeling, J Foster, B E Patterson


In ground performance of wood treated with a substituted isothiazolone
1990 - IRG/WP 3612
Isothiazolones (I.T.A.'s) are a class of biocides that have potential for use as wood preservatives. The substituted ITA, RH-287, (4,5,dichloro-2-n-octyl-isothiazolone-3-one) is being evaluated as a broad spectrum wood preservative. The evaluation program includes in ground stake tests which were established at two test sites in Mississippi, USA The tests used southern yellow pine treated...
L E Leightley, D D Nicholas


Comparison of various types of bait containers designed to aggregate large numbers of foraging subterranean termites from natural populations in below-ground mound colonies
1995 - IRG/WP 95-10116
At Walpeup in the semi-arid mallee country of north-west Victoria (350 km from Melbourne), there are several indigenous subterranean termite species, none of which build above-ground mound colonies but build their colonies below-ground and/or in trees. This paper describes a baiting experiment in which three types of bait containers were compared in their ability to aggregate large numbers of fora...
J R J French, B M Ahmed


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


Accelerated testing for out of ground contact using natural biological preconditioning
1996 - IRG/WP 96-20088
Small blocks made of Scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. Bacteria and moulds colonised the vermiculite and miniblocks well. Aureobasidium pullulans was common on TnBTO tre...
S Molnar, D J Dickinson, R J Murphy


Performance of preservative-treated timber commodities in above-ground service tests
1995 - IRG/WP 95-20064
Service tests established by NZ FRI are of commodities where treatment has been undertaken in commercial plants and although such data as preservative uptake of individual items is recorded and sample analysis undertaken, material is usually "run-of-mill" for the commodity being treated. The NZ FRI Service Test database includes a wide range of preservative/species combinations in virtually all ab...
M E Hedley, D R Page


Benzalkonium chloride (an AAC preservative): Criteria for approval, performance in service, and implications for the future
1985 - IRG/WP 3328
The data base generated for benzalkonium chloride was considered adequate for commercial approvals, particularly after revision in late 1982. Field trials, although not part of the approval criteria, generally supported commercial use; decay observed in one test (post and rails) after 6 years' exposure would have resulted in some caution in setting retentions. No laboratory trial, nor fie...
J A Butcher


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Performance of above ground decay test units treated with a substituted isothiazolone
1989 - IRG/WP 3503
RH 287, a substituted isothiazolone, was evaluated for efficacy against decay fungi in an above ground test in Mississippi. After 45 months of exposure, all test units that were pressure treated with this biocide at levels of 0.026 pcf and higher have no deterioration. In addition, the test units that were dip-treated with a solution concentration of 0.5% also have no deterioration. Compared to pe...
D D Nicholas, J A Wilson, D E Greenley


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


Above and Below-Ground Depletion of Copper, Chromium and Arsenic from Pinus radiata and Fagus sylvatica at Thirteen Test Sites in New Zealand and Australia
2006 - IRG/WP 06-30402
The objective was to determine the significance of site and wood species on preservative depletion for a copper chrome arsenate preservative (CCA) from 20 x 20 x 500 mm field test stakes after 5.5 and 4.5 years for pine and beech respectively. At least 5 sacrificial stakes were used to produce site means. Site and wood species had a major effect on copper, chromium and arsenic loss from CCA treate...
R Wakeling


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


Predicting the decay resistance of timber above-ground: 2. When can reliable field data be obtained?
2007 - IRG/WP 07-20368
Application of modern performance-based engineering and design requires building products that are thoroughly characterised in terms of their ability to perform as expected over time. The engineering community is attempting to use this information to provide predicted service-lives for various building elements. Increasingly, this service-life prediction must be based on objective measurement coup...
L P Francis, A J Swain, J J Morrell


Durability of some alternatives to preservative-treated wood. Progress report 2: Results from field tests after 5 years’exposure
2007 - IRG/WP 07-30442
A number of alternatives to preservative-treated wood have been tested according to EN 252 (stake test) and a specially designed ground-proximity field test, the latter in Sweden as well as in Hawaii, USA. Seven untreated wood species and four alternative wood treatments labelled as environmentally friendly (acetylation, linseed oil, heat treatment, vinyl polymer) were included in the study. Four ...
M-L Edlund, J Jermer


Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Above ground testing at tropical test sites, what have we learned?
2011 - IRG/WP 11-20473
Three different above ground test methods have been utilized at a selection of five tropical and sub-tropical test sites with a variety of treated and untreated material. The results show that a multi-site approach to above ground field tests presents the opportunity for exposure to un-predicted biodeterioration hazards, which may be important for developmental products of poorly characterized fu...
A Preston, A Zahora, Y Cabrera, L Jin, C Schauwecker, P Walcheski


Durability of timber products –Part 1: Inventory and evaluation of above ground data
2012 - IRG/WP12-20498
The material-inherent resistance of wood is one of the most important qualities influencing the durability of timber. Hence, it has also a major effect on the service life to be expected from a timber construction. In addition, design details and the respective climatic conditions determine durability and make it impossible to treat wood durability as an absolute value. Moreover, the reference mag...
C Brischke, L Meyer, G Alfredsen, M Humar, L Francis, P O Flæte, P Larsson Brelid


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken