A comparative field test of the effectiveness of anti-sapstain treatments on radiata pine roundwood
1986 - IRG/WP 3376
Peeled radiata pine posts were sprayed with one of six antisapstain formulations, with and without a wax water-repellent additive, to evaluate the protection given by each treatment. After 3 months' outside storage the best treatments tested were 4% product Busan 30, 2% product Busan 1009, and 2% active sodium pentachlorophenoxide (NaPCP) with 1.5% borax. After 6 months' storage ...
J A Drysdale, R M Keirle


Framework document for an international code of good practices for wood preservation and wood protection (anti-sapstain) facilities
1992 - IRG/WP 92-3683
At the Kyoto meeting, the Health & Safety committee agreed to form a task force to prepare a global plan for writing a code of good practices (Code) for wood protection and preservation facilities (Doc. No. IRG/WP/3681). The Canadian document had been presented to the IRG group earlier (Doc. No. IRG/WP/3447) and similar documents were solicited from other countries for preparing a framework do...
V N P Mathur, G Das


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


Some tests on ES - AS 11, a novel anti-sapstain formulation, and its properties
1987 - IRG/WP 3399
The results of some tests with the formulation ES - AS 11 are given. The formulation is an attempt to improve the performance of an anti-sapstain chemical by: 1) increasing its penetrability 2) uniquely combining its active ingredients. Very short times of treatment (dipping not longer than 5 seconds), low concentrations of active ingredients, and lower toxicological and environmental risks may be...
U Straetmans


Co-operative research at the Naval Research Laboratory on wood extractives and related compounds as antiborer agents
1977 - IRG/WP 429
J D Bultman, K K Parrish


Production of preservative-treated wood in some countries
1990 - IRG/WP 3598
This report presents figures of the production of preservative-treated wood and wood treated with anti-stain chemicals in 26 and 20 countries respectively from all over the world....
J Jermer


A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen


The use of chlorothalonil for protection against mold and sapstain fungi. Part 1: Laboratory evaluation
1989 - IRG/WP 3515
Laboratory screening of chlorothalonil alone and in combination with other fungicides was conducted against six mold and sapstain fungi. The most promising treatments appear to be chlorothalonil supplemented with CCA or copper-8-quinolinolate. Field tests have been implemented....
J A Micales, T L Highley, A L Richter


The preliminary evaluation of selected sulfonium salts for use in wood preservation
1984 - IRG/WP 3278
Five sulfonium compounds, including two sulfonium methosulfates, one sulfonium bromide and two amphoteric sulfonium propanesulfonates, were prepared in crude form and subjected to various biocidal screening tests. A rapid screening test in which treated Pinus radiata pulp pellets were exposed to one of three wood-decaying fungi growing on malt agar revealed that dodecyl dimethyl sulfonium methosul...
D V Plackett


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals


Preliminary note on the fungal problem of rubber wood
1983 - IRG/WP 3246
Susceptibility of rubber wood to fungal attack limits its wider utilisation. Fungal problems encountered in treating rubber wood with boron compounds by diffusion process have been discussed. Sodium pentachlorophenoxide and 2-thiocyanomethylthio benzothioazole (TCMTB) were investigated for possible control of fungal growth during diffusion storage and their performance has been reported....
R Gnanaharan


Evaluation of an alkyl ammonium compound as a fungicide to control sapstain and mould during diffusion storage
1984 - IRG/WP 3282
An alkyl ammonium compound ('Akzo' ES 255) was evaluated for its effectiveness against mould and sapstain during diffusion storage of boron-treated rubber wood. Though ES 255 at 1.0% concentration was effective against mould (71%) and sapstain (89%) it is less satisfactory compared to 0.5% sodium pentachlorophenoxide against mould (92%) and sapstain (98%)....
R Gnanaharan


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


Chapter 6 - Preservatives of bamboo
2007 - IRG/WP 07-10635-06
Almost all currently available oil-borne, water-borne and compound types of preservatives suitable for the preservation of bamboo or wood have been described along with their classifications, applications, formulations, merits and demerits, history of invention or discovery and development. The preservatives suitable for wood are also considered suitable for bamboo....
A K Lahiry


Effect of borate on uptake and efficacy of an anti-sapstain treatment
2005 - IRG/WP 05-30380
The potential for using borates to enhance uptake and efficacy of propiconazole-based anti-sapstain chemicals was assessed on ponderosa pine sapwood wafers. Borates had no consistent effect on either net solution absorption or propiconazole distribution in the wood. Even small amounts of borate, however, markedly improved the performance of propiconazole against fungal discoloration. These resul...
Jianju Luo, Hua Chen, J J Morrell


Field and laboratory studies on anti-sapstain preservatives
1982 - IRG/WP 3205
The field tests included 11 different anti-sapstain preservatives and were carried out at different sawmills in southern Sweden. Drying conditions, climate and the local fungus flora were not identical for the different preservatives and comparisons between the preservatives should therefore be made with caution. Results obtained in the field tests are, however, in relatively good agreement with t...
M-L Edlund, B Henningsson


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


Effects of methoprene on Coptotermes formosanus (Isoptera: Rhinotermitidae)
1987 - IRG/WP 1322
Methoprene affected differentiation and survival of Coptotermes formosanus Shiraki in laboratory studies. At 5, 9, 13, and 17 weeks, superfluous intercastes and presoldiers were produced when termites were allowed to feed on concentrations of 1,000 and 2,000 ppm methoprene in wood blocks. Colony numbers were significantly reduced after 13 and 17 weeks of exposure to the insect growth regulator. Te...
S C Jones


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


A potential anti-sapstain chemical for sawmills
1984 - IRG/WP 3300
Several biocidal formulations were tested under laboratory conditions in order to discover an alternative antisapstain chemical to chlorophenoxides. The formulations tested were experimental water solutions containing a quaternary ammonium chloride, a commercial fungicide and/or a sodium salt of some carboxylic acids. The effect of sodium carbonate and borax decahydrate in mixture with a quaternar...
I A Linderborg


Preliminary field and laboratory findings regarding the efficacy of a novel anti-marine wood borer agent
2000 - IRG/WP 00-10380
Blocks of sapwood of Pinus nigra were treated by vacuum impregnation with Biocide A to retentions of 0.5, 1 and 2 kg m-3. Similar blocks were vacuum-pressure impregnated with CCA to retentions of 2, 24 and 38kg m-3. The blocks were exposed subtidally in Mourilyan Harbour (Queensland, Australia). After 5 and 10 months exposure, blocks were removed, examined for superficial signs of attack by wood b...
A Praël, S M Cragg, R A Eaton


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Comparative study on physical properties of four fast growing timber species of Bangladesh
2006 - IRG/WP 06-10570
Ghoraneem (Melia azedarach), Rain tree (Albizia saman), Sissoo (Dalbergia sissoo Roxb.) and Akashmoni (Acacia auriculiformis) plantations are started as a fast growing timber specie from a few years back in Bangladesh. Initian objectives were to get fuel wood only from those trees, but a very positive response was found for Ghoraneem, Rain Tree, Sissoo and Akashmoni timber in the users market by c...
M M Islam, B K Dey, M O Hannan, G N M Ilias


A status report on code of good practices
1991 - IRG/WP 3679
Code of Good Practices - Anti Sapstain documents, presented to IRG meetings in the past, are the basic documents for health and safety of the workers and the environment in Canada. The BC Ministry of Environnment has now issued regulations in the area of effluent discharge. While Pentachlorophenols (PCP) are not used by the industry, the documents are still used as a guideline document for the oth...
V N P Mathur, G Das


Previous Page | Next Page