Your search resulted in 153 documents. Displaying 25 entries per page.


Improvement of liquid penetration of wood by precompression under appropriate conditions and recovery process
1993 - IRG/WP 93-40014
A new system for enhancing the penetration of liquid into wood using a precompression treatment was designed, and the effects of compressive deformation and recovery on liquid uptake were evaluated. Precompression of up to 60% under appropriate moisture and heat conditions effectively increased the penetration of liquid into refractory wood samples of practical sizes without producing any strength...
I Iida, Y Imamura


Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


The effect of selective additives and conditions on the decomposition of Basamid in Douglas fir heartwood
1992 - IRG/WP 92-3698
Basamid is a solid, powdered chemical used as an agricultural soil fumigant. Decomposition of Basamid isothiocyanate, hydrogen sulfide, methyl amine, and formaldehyde. Basamid has some potential as a wood fumigant, but it decomposes too slowly to be effective. Various additives and conditions were tested for their ability to enhance Basamid decomposition in Douglas-fir heartwood. Higher MC&apo...
P G Forsyth, J J Morrell


Treating Eucalyptus tereticornis wood with boron: Optimizing treatment conditions
2005 - IRG/WP 05-40309
Even though Eucalyptus tereticornis wood is suitable for small timber purposes, being non-durable, it needs to be treated with preservative chemicals. As it is a heavy, hard and difficult to treat species, the possibility of using diffusible boron compounds was investigated. The present study explored the effect of impregnation conditions such as treatment schedule, concentration of treatment solu...
T K Dhamodaran, R Gnanaharan


Leaching of CCA components from treated wood under acidic conditions
1993 - IRG/WP 93-50004
The leaching of CCA components from treated wood under acidic conditions were investigated. Western hemlock treated with three types of CCA and two levels of target retention was subjected to leaching at four different levels of pH. After leaching tests, leached samples were subjected to laboratory decay and soft rot tests. The amount of CCA components leached was dependent on acidity of leaching ...
Jae-Jin Kim, Gyu-Hyeok Kim


Examining environmental conditions and the biodeterioration of historic waterlogged wood: the Kolding Cog
2002 - IRG/WP 02-10441
Survival of waterlogged wood from thousands and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depositional environment, have not been completely degraded. This paper discusses the biodeterioration of a submerged shipwreck buried in Kolding Fjord, Denmark for the past 1000 years....
B A Jordan, D J Gregory, E L Schmidt


List of wood-destroying fungi in Iran
1976 - IRG/WP 138
This list gives information on the wood-destroying fungi collected in the Iranian forests and from felled logs and boards in sawmills until now. They are mainly from the region of the Caspian Forests and from the climatically dry region between Teheran and Azarbaidjan, North Iran. It is understood, that this document may help to give more knowledge outside the country about the specific problems o...
P Soleimani


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva


Optimum growth conditions for the metal-tolerant wood decay fungus, Meruliporia incrassata TFFH 294
1999 - IRG/WP 99-50142
There is a worldwide need for alternative methods for the treatment and disposal of CCA-treated waste wood. Illman and Highley (IRG/WP 96-10163) reported the isolation of a unique strain of Meruliporia incrassata (TFFH 294) with tolerance to CCA. The strain is capable of degrading CCA treated waste wood, giving a 40% weight loss in the ASTM soil block test. The strain is an ideal candidate for deg...
V W Yang, B Illman


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


ATP assay for the determination of mould activity on wood at different moisture conditions
1992 - IRG/WP 92-2397
To determine fungal responses to fungicides and environmental conditions and for detection of microbial activity in wood, sensitive and objective methods are needed. We have developed a suitable assay based on analysis of adenosine triphosphate (ATP) by using the luciferin-luciferase reaction. With the aid of this assay the activity of Penicillium brevicompactum on wood at different RH levels was ...
J Bjurman


Délavabilité de bois ronds traités avec un sel CCA dans des conditions réelles de stockage. Incidence pratique de la fixation accélérée par étuvage. Impact effectif sur l'environnement
1993 - IRG/WP 93-50001-23
Un essai de terrain a été organisé pour mesurer concrètement, dans des conditions aussi proches que possibles des conditions réelles de terrain, les pertes effectives en produit de traitement lorsque le bois traité est soumis à des intempéries. L'essai a été conduit sur des bois ronds (poteaux), traités en autoclave par procédé Bethell avec un sel CCA de type C, avec comme fi...
M Rayzal, F Larroze


Effects of fixation conditions and seawater on leaching of wood treated with marine retention CCA
1997 - IRG/WP 97-50088
The effect of post-treatment conditioning temperature and humidity on leaching of chromated copper arsenate (CCA) was compared in seawater and deionized water. Southern pine cubes treated to 40 kg/m3 CCA were stored at 2° C and 82% relative humidity (RH), 24° C and 65% RH, or 32° C and 30% RH for 3, 10, or 17 days. Cubes were then leached in deionized water or artificial seawater. The rate of l...
S T Lebow


The critical moisture and temperature conditions for the growth of some mould fungi and the brown rot fungus Coniophora puteana on wood
1988 - IRG/WP 1369
The growth of some mould fungi on pine and spruce sapwood was studied in 40 different constant moisture and temperature conditions. The temperature range was between +10 and +40°C and the relative humidities varied from 76 to 100% relative humidity (RH). The incubation time was 12 weeks. The mixed mould inoculation used included typical fungi growing on wood: Aspergillus versicolor, Cladosporium ...
H Viitanen, L Paajanen


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...
M Maoz, J J Morrell


Curing conditions for a low formaldehyde etherificated melamine resin
1998 - IRG/WP 98-40108
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. Previous studies indicated that the resin with the lowest formaldehyde content tested showed the best results regarding fungal resistance, dimensional stability and formaldehyde emissions after curing. In the present paper the influence of ...
D Lukowsky, R-D Peek, A O Rapp


Effect of mini-block test conditions on activity of Coniophora puteana
2000 - IRG/WP 00-20184
The influence of various factors of the mini-block test method on growth and activity of different strains of Coniophora puteana was studied. Decay rates of spruce samples in Petri dishes of different depths, at different wood fibre orientations and at various distances between growth medium and wood were compared. In deep Petri dishes, there were no significant differences between activity of the...
F Pohleven, M Petric, J Zupin


Limiting Conditions for Decay in Wood Systems
2002 - IRG/WP 02-10421
Hygrothermal models can predict temperature and moisture conditions in wall components subjected to real weather data, but specific data and a fundamental understanding of how temperature and wood moisture content dictate the progression of decay under these conditions is required for modellers to predict consequences of decay on building performance. It is well understood that wood will decay abo...
P I Morris, J E Winandy


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Wood preservation in Portugal
1985 - IRG/WP 3325
This report deals with the forest potential of Portugal and its timber industry and outlines the evolution of wood preservation in the country. The main hazards to timber in service are noted and the timbers used classified according to their natural durability and treatability. The wood preservatives used are detailed with estimates of the total consumption of the different types. Addresses are l...
D De Sousa Castro Reimão, R Cockcroft


The use of propionic acid to prevent Pinus patula biodeterioration during outside chip storage in Zululand
1989 - IRG/WP 3531
Pinus patula SCHIEDE ET DEPPE IN SCHLD. ET CHAM. is susceptible to biodeterioration during outside chip storage (OCS), reducing pulp quality and tear and burst indices of resulting paper. Accelerated laboratory trials showed that chips treated with 2% (w/v) propionic acid and stored for 17 weeks, produced pulp of quality indistinguishable from fresh untreated chips. Pulp tests during field trials ...
S Ismail, E J Smith, A A W Baecker