Your search resulted in 3797 documents. Displaying 25 entries per page.
Influence of different triazoles as co-biocides in wood preservatives on efficacy and the environmental impact
2018 - IRG/WP 18-50333
In this study we investigated the efficacy and impact on the environment of different co-biocide triazoles in wood preservatives. Four different formulations (all containing 9.5% Copper) contained individual and combinations of cyproconazole, tebuconazole, propiconazole as co-biocides. Four formulations were tested according to EN 113 and EN 84 (ageing) to determine the brv for each formulation. T...
M Klamer, T Jensen, S Bang-Achton, E Morsing
CCA wood preservative: Trust with destiny
2019 - IRG/WP 19-30731
This paper traces the history of Copper-Chrome-Arsenic (CCA) and its current status in India and worldwide. CCA was invented as ASCU at the Forest Research Institute, Dehra Dun in 1933 by Dr. Sonti Kamesam. Although its efficacy was doubted by the British colonial rulers resulting in several hiccups at home, the patent rights were purchased by US Bell Telephone Co. and it was adopted by the US woo...
S Kumar
COPPER NAPHTHENATE: A Product for All Seasons: Protecting the Americas’ Infrastructure for Over 100 Years and Potential for Expanded Usage in Europe
2019 - IRG/WP 19-30738
This paper is a brief review of the history and use of the wood preservative Copper Naphthenate, with a focus on use patterns within the USA and opportunities for expansion in Europe and Canada. This paper reviews how copper naphthenate has performed to preserve and protect cellulosic and wooden items essential to critical infrastructure, and why it is the ideal choice for use in the replacement o...
M H Freeman, J A Brient, M Manning
Effect of damage to polyurea coatings on metal losses from ammoniacal copper zinc arsenate treated Douglas-fir pile sections
2019 - IRG/WP 19-40867
Metal-based preservatives remain the most widely used treatments for protecting wood in soil or water contact. While these treatments are highly effective, one drawback is a tendency for small amounts of metal to migrate into the surrounding environment. The greatest risk in this regard is copper because many organisms are highly sensitive to this metal. While post treatment practices can reduce ...
M J Konkler, J J Morrell
Effect of pretreatment of wood surfaces with a copper monoethanolamine solution on the natural weathering performance of semitransparent stains
2019 - IRG/WP 19-40881
Semitransparent stains for wood products are favored for outdoor applications in Japan because these finishes do not hide the wood grain. However, the photoprotective effects of wood surfaces are low, therefor there is a need to improve the weathering performance. We examined the natural weathering performance of semitransparent stains on wood pretreated with a copper monoethanolamine solution (Cu...
S Isaji, H Shibui, Y Hirabayashi
Adhesion durability of the thinnest CLT in Japan treated by solvent recovery system
2019 - IRG/WP 19-40882
The purpose of this study is to clarify the adhesion durability of the thinnest CLT (36 mm thickness) in Japan impregnated with preservatives (azole neonicotinoid compounds (AZN)) under solvent recovery system so called “dry pressure process” for long-term durability. The adhesion durability tests were conducted in accordance with the Japanese Agricultural Standard (JAS) of Cross-Laminated-Tim...
K Kawakami, W Ohmura
Incidence of treated wood in a wood recycling facility in Western Oregon, USA: an update
2019 - IRG/WP 19-50346
Preservative treated wood provides excellent long-term performance under a variety of adverse conditions, but it must eventually be replaced. The US Environmental Protection Agency recommends reuse in a similar application, but if that is not an option, disposal in a municipal solid waste facility equipped with a leachate management system. Concerns about diminishing landfill capacity have led m...
J J Morrell
Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski
Impregnation of railway sleepers - Investigation of a system-sleeper as an alternative for creosote treated sleepers
2020 - IRG/WP 20-40896
For nearly 200 years wooden railway sleepers are impregnated with creosote. After initially using vacuum pressure processes for impregnation, empty-cell processes have been developed quickly and are used until today. Because of political developments, creosote will probably be banned on the European market in the near future. The Fürstenberg-System-Sleeper, which combines for Europe innovative as...
M Starck, A Heidel, C Brischke, H Militz
Longterm Performance of Treated Timbers in Marine Exposures
2020 - IRG/WP 20-10969
The performance of preservative-treated or modified woods in marine exposures was evaluated at test sites in Newport, Oregon, USA and Brisbane, Queensland, Australia. All samples have exhibited excellent performance at the Newport, Oregon site, while attack was more aggressive at the sub-tropical Brisbane site. Acetylated wood as well as samples treated with 7.3% chromated copper arsenate (CCA-T...
M Konkler, A R Zahora, J Norton, J J Morrell
Potenzy of Azadirachta indica heart wood extracts as wood bio-preservative against termite attack
2020 - IRG/WP 20-10972
Extractives in wood are one of the main reasons for wood resistance against bio-degradation. The chemical compositions of extractives from matured Azadirachta indica that are known to be very resistant against bio-degradation were studied to assess their role as wood preservative. Ethanol and toluene were used in the extraction of these compounds from the heartwood of Azadirahcta indica. Chemical ...
L O Aguda, O B Olajide, O Y Aguda
Macro biological degradation of wood treated with sorbitol and citric acid – first results from marine environment and termite exposure
2020 - IRG/WP 20-40901
Most European wood species are rapidly and severely degraded in termite-infested areas and the marine environment. There is a need for new solutions, especially in the marine environment, since we lack wood preservatives approved for marine applications in Europe. Several wood modification systems show high resistance against both marine borers and subterranean termites. However, the existing comm...
A Treu, L Nunes, E Larnøy
Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz
Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site.
The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht
Development of Wooden Fireproof Structures for Mid- and High-rise Buildings in Japan
2021 - IRG/WP 21-30757
When constructing a mid-to-high-rise building more than 4 stories in general in Japan, it is necessary to have a fireproof structure stipulated by the Building Standard Law. The performance required as a fireproof structure in Japan is generally stricter than in other countries, and it is required to be structurally sound after a fire even without fire extinguishing activities. In order to satisfy...
D Kamikawa, M Harada, H Matsunaga, R Takase, N Hattori, Keisuke Ando, M Miyabayashi
Efficiency of three resin fractions from Aucoumea Klaineana Pierre, Canarium schweinfurthii Engl and Dacryodes edulis (G. Don) H. J. Lam from Gabon combined with Tebuconazole as wood preservatives
2022 - IRG/WP 22-10998
Pure resins from Aucoumea Klaineana, Canarium schweinfurthii and Dacryodes edulis were harvested and then hydro-distilled to obtain essential oils and purified resins fractions. Due to the potential leaching and volatility hazards of the compounds that constitute these fractions, resins and essential oils were combined with tebuconazole to produce both antifungal and anti-termite wood preservative...
W F Bedounguindzi, K Candelier, P Edou Engonga, S Dumarcay, M-F Thevenon, P Gerardin
Copper-octanoate - a potential reference preservative replacement for CCA in field test standards?
2022 - IRG/WP 22-20688
Finding a CCA reference replacement for use in standardised test methods is of high priority since this chemical is being phased out and may in the near future be banned also for experimental and approval purposes. In this paper we assess the possibility to replace CCA reference preservative with an historical copper octanoate product. There is a huge amount of lab and field test data available fo...
R Ringman, M Westin, M Klamer, A Christof, F Friese
A new approach to wood protection: Potential of biologically synthesised CuO and ZnO nanoparticle formulation as a wood preservative
2022 - IRG/WP 22-30758
Even though metal nanoparticles are effective in protecting wood, they are less preferred, as they are synthesised using methods which are expensive and are not environmentally friendly. Biological synthesis of nanoparticles using plants, fungi, yeast, bacteria and viruses, has been accepted as an alternative approach and is referred to as green synthesis. Utilization of biologically synthesised n...
Shiny K S, R Sundararaj, N Mamatha
Comparative study on the efficacy of biobased wood preservative over conventional wood preservatives against fungi and termites
2022 - IRG/WP 22-30761
The current focus of wood preservation research is on developing wood preservatives from natural and environmentally compatible compounds for industrial application. Liquefaction of wood is one of the promising approaches to utilize woody waste where the wood powder is converted into a chemically active liquid with the help of a liquefying agent like phenol, cresol, plant-based solvent as CNSL and...
A Kumar, A John, B N Hazarika
Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec
Comparative study of the properties of silicate coatings with different mineral pigments (titanium dioxide, iron (III) oxide, copper (II) oxide) on the surface of wood
2022 - IRG/WP 22-40936
Silicate coatings are attractive alternatives to conventional organic-based coatings for wood protection. In this work, silicate coatings were prepared with a potassium silicate binder modified with a methyl siliconate solution, and three types of mineral pigments titanium dioxide, iron (III) oxide and copper (II) oxide. The coatings were applied on beech wood and cured under ambient conditions. T...
A M Cheumani Yona, M Petrič
Evaluation of the physical properties of heat-treated native Peruvian woods for their application as coverings in buildings located in in arid, semi-warm and humid climates
2022 - IRG/WP 22-40943
Wood is a material that has properties suitable for its use in construction: as a structural component, cladding or decorative element, however, it is necessary to have knowledge of its physical, mechanical and thermal properties in order to have a logical criterion when applying it. It is known that wood has hygroscopic properties, so it tends to absorb the relative humidity of the natural enviro...
K Ayala Castro, A Loayza Argüelles, V J Pilco Mamani
Evaluation of Decay Resistance for the Larch Wood Heat-treated with Superheated Steam
2022 - IRG/WP 22-40956
Heat-treatment of wood is a process that involves applying heat ranging 160–260°C to improve its physico-mechanical properties and resistance against wood rot fungi. The level of the changes in the wood properties by heat-treatment differs depending on the temperature and duration of heat-treatment, as well as the types of heat transfer media used for heat-treatment. The heat-treatment on wood ...
Y Park, S-M Yoon, H Kim, W-J Hwang
Virtual Reality of Wood Protection
2023 - IRG/WP 23-20698
Virtual reality (VR) is a technology that allows people to explore and interact with computer generated environments using devices that stimulate different senses (sight, sound and touch). VR is mainly used for education, training and entertainment, but it also has the potential to provide new insights into scientific phenomena. In this paper we describe the evolution of VR and its many uses, focu...
D Feng, Y Liu, M Turner, A Limaye, P D Evans
Sensitivity of copper indicators for detecting preservative penetration
2023 - IRG/WP 23-20701
Chrome azurol S (CAS), 1-(2-pyridylazo)-2-naphthol (PAN), and rubeanic acid (RA) are the three copper indicators currently used by the timber industry to assess preservative penetration. Although only the American Wood Protection Association (AWPA) standards specify indicator sensitivity, it is unclear how those limits were developed. The sensitivity of each copper indicator was determined in solu...
T Yi, J Norton, S Meldrum, J J Morrell