Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


In-ground variability of decay intensity within a test field
2012 - IRG/WP 12-20496
Timber exposed in the ground faces most severe conditions in terms of exposure to wetting and fungal decay in the terrestrial environment, therefore wood durability tests are often conducted in test fields preferably ensuring the occurrence of all relevant decay organisms. One can also expect differences in decay within an individual field-test site due to localized distribution of certain organis...
C Brischke, S Olberding, L Meyer, T Bornemann, C R Welzbacher


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


The activity of a wood-decaying fungus during drying and rewetting cycles measured by isothermal calorimetry
2013 - IRG/WP 13-20526
Wood decaying fungi are an essential part of any ecosystems as they are the main decomposers of cellulose and lignin-containing materials. But as wood is a common building material the risk for decay fungi growth and subsequent degradation of our construction material is a concern. There are important physiological aspects of the growth and activity of decay fungi that are unknown today, and witho...
S Johansson, L Wadsö, A Pilgård, G Alfredsen


Development of a rapid method to assess the rate of fungal colonization of wood
2013 - IRG/WP 13-20531
Testing of wood durability is today done mainly with accelerated exposure tests under rather realistic conditions (in ground, outdoors with moisture traps etc). Although such tests are accelerated with respect to the conditions that outdoor exposed wood structures are exposed to, they tend to take rather long time. The present paper presents the development of a rapid method intended to assess at ...
L Wadsö


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Characterisation of fungal decay in cable car trestles in Svalbard
2023 - IRG/WP 23-11031
The Arctic will be strongly affected by climate change. In Svalbard the coal mining industry were established in the early 20th century. All man-made structures and sites dating before 1946 in Svalbard are protected by law and considered as cultural heritage. This included the massive cable car trestles that are constructed from untreated Norway spruce and mounted directly into the soil. We hereby...
G Alfredsen, L Ross, M Altgen, I A Yakovlev, A-C Flyen, M S Austigard, J Mattsson, N B Pedersen


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Co-operative studies on determining toxic values against wood-destroying Basidiomycetes: Progress report to May 1989
1989 - IRG/WP 2339
This document reports progress on the co-operative study between nine laboratories set up following the proposals contained in Document IRG/WP/2316. Results have been received from two laboratories. Toxic values data have been established successfully using the test fungus Coniophora puteana but problems have been encountered with the other test fungi....
A F Bravery, J K Carey


Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley