A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle


A baiting technique to monitor the development and control of decay in transmission poles
1981 - IRG/WP 2149
P I Morris, D J Dickinson


Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


Effect of felling time related to lunar calendar on the durability of wood and bamboo -Fungal degradation during above ground exposure test for 2 years- (Preliminary report)
2005 - IRG/WP 05-20311
Current study was carried out to know whether the felling time of trees and bamboos based on lunar calendar affects natural durability of felled wood-bamboo or not. Each of one sugi (Cryptomeria japonica) tree of 28 years old and one Moso bamboo (Phyllostachys heterocycla) of around 3 years old was cut 12 times between February and December in 2003. Six sets of sugi tree and bamboo were felled in ...
K Yamamoto, S Uesugi, K Kawakami


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...
G F Daniel, T Nilsson, J Volc


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


In-ground evaluation of a copper azole wood preservative (Tanalithâ E) at a tropical Australian test site
1996 - IRG/WP 96-30100
A field trial to determine the in-ground termite and decay resistance of Pinus radiata D. Don impregnated with a copper azole formulation, TANALITHâ E, has been established at a tropical site in the Northern Territory of Australia. Four retentions of TANALITHâ E, containing 1.54, 2.08, 2.92 and 4.30 kg/m³ of Cu, are being evaluated. For comparison, Pinus radiata specimens treated to two retenti...
J W Creffield, J A Drysdale, N Chew


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Examination of the Pilodyn as a non-destructive test method for detecting decay in CCA treated eucalypt poles
1982 - IRG/WP 2177
Below groundline condition of 274 CCA treated eucalypt poles comprising 13 different species was examined using 6 and 12 Joule Pilodyn units with 2 and 2.5 mm diameter pins. The data obtained was used to calculate regressions of density on pin penetration. A decrease in density was accompanied by an increase in pin penetration. The best correlation was found using the 6 Joule, 60 x 2.5 mm² diamet...
L E Leightley


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


Premature decay of CCA-treated pine posts in horticultural soils - An overview
1984 - IRG/WP 1241
The recent discovery in New Zealand of early decay in CCA-treated pine posts set in horticultural soils led to the establishment of a comprehensive research programme. The objectives and outline of this programme are presented together with an overview of research progress to date. Results suggest that premature decay of CCA-treated timber is restricted to material placed in highly cultivated soil...
J A Butcher


Calculation of preformance index of Bardac 20 (an alkylammonium compound) evaluated in a field stake test
1982 - IRG/WP 3206
Bardac 20 treated stakes have been in test for three years at the Westham Island test site near Vancouver, B.C. The Performance Index for the preservative was calculated and found to be 0.009 which infers that, at the standard retention, Bardac 20 added 0.9 y to the life of the stake. It may be concluded that when tested using a standard field stake test using ponderosa pine (Pinus ponderosa Laws)...
J N R Ruddick


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


Comparison between agar-block and soil-block methods for wood-destroying Basidiomycetes
1992 - IRG/WP 92-2401
The object of this work is to compare these methods in order to provide some information to help in the choice between them. The comparison was made by a statistical analysis (factorial completely randomized design) and by a discussion about other aspects of each method. An evaluation of some fungi on attacking wood and a comparison between Picnoporus sanguineus isolated from carpophore and decaye...
M B B Monteiro, S Brazolin, G Catanozi


Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 2: Laboratory fungal bioassays
2000 - IRG/WP 00-20204
Extracts from sawmill residues of the naturally durable white cypress, Callitris glaucophylla were tested for fungicidal activity in a series of laboratory bioassays. The effects of different extraction solvents, techniques and sources of material on the biocidal efficacy of the resultant extracts were evaluated. Soil jar decay tests were used initially however, contractual time constraints necess...
M A Powell, L M Stephens, L Francis, M J Kennedy


Field stake test assessment with the Pilodyn
1980 - IRG/WP 2136
The Pilodyn, which was originally developed to estimate the degree of soft rot in wooden poles, was thought to have potential for giving a quantitative measure of the extent or depth of decay in field test stakes. In the present work a 2-joule Pilodyn with 2.0-mm diameter pin was used in an attempt to limit depth of pin penetration (to 10-15 mm) without reducing scale sensitivity. The results show...
M E Hedley, R W Naish