Kiln drying of CCA-treated wood - Some safety and environmental considerations
1987 - IRG/WP 3443
Vapours and condensate from a condenser kiln in which CCA-treated wood was being dried have been collected and analysed. The concentrations of arsenic, copper and chromium found in the vapours from the drying process were well below Swedish threshold limit values. The contents of arsenic and chromium were also low in the condensate, although the copper content was fairly high. The latter result wa...
J Jermer, B Lundberg


Dip-diffusion of dressed timber - Effect of drying
1989 - IRG/WP 3509
The effect of drying on dip-diffused dressed freshly sawn timber was determined by the depth of penetration of boron achieved on the two test timber species, White cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that light density White cheesewood was completely penetrated even after 3 days drying while Light hopea, treated immediately achieved 5.2 mm p...
H C Konabe


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Laboratory tests on artificial weathering of Quercus rubra crossties
1986 - IRG/WP 2252
Clear red oak (Quercus rubra) blocks were used to evaluate various types of accelerated aging tests including boil, steaming, and cyclic weathering. It was found that the repeated vacuum and pressure treatment of wood in water, steaming, oven-dry, and freezing appeared to be most effective in reducing the MOE in compression and hardness modules of wood specimens. Red oak crossties which were press...
P Chow, A J Reinschmidt, E J Barenberg, S L Lewis


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


Effects of drying processes on termite feeding behaviour against Japanese larch wood
2001 - IRG/WP 01-10390
We investigated the effects of current drying schedules for larch lumbers on the termite feedings. Thermal analyses were also conducted to investigate degradation of wood components. Choice feeding tests showed specimens dried under high-temperature schedules were evidently susceptible against termite attacks. These schedules produced the feeding-attractants, which were suggested by the TGA result...
S Doi, Y Kurimoto, H Takiuchi, M Aoyama


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Dip-diffusion of dressed timber - Effect of drying
1990 - IRG/WP 3603
The effect of drying on BFCA dip-diffused, dressed, freshly sawn timber was determined by the depth of penetration of boron achieved on two test timber species, White Cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that the light density White cheesewood was completely penetrated even after 3 days drying while Light Hopea, treated immediately achieved 5...
H C Konabe


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Leaching from CCA-impregnated wood to food, drinking-water and silage
1987 - IRG/WP 3433
During the last years The Norwegian Institute of Wood Technology (NIWT) has analysed different foodstuff for contamination by copper, chrome and arsenic from CCA-impregnated wood. There has been some interest for using CCA-impregnated wood in contact with food and drinking-water. Before giving their permission the Norwegian Health Authorities want results from experiments. NIWT therefore started t...
F G Evans


A note on te seasoning, preservative treatment and suitability of debdaru (Polyalthia longifolia Benth & Hooker.) for poles
1995 - IRG/WP 95-40056
The main work is to determining the suitability of Debdaru (Polyalthia longifolia Benth.) as poles from Government and Village forests are investigated. The poles of Debdaru are easily treatable with CCA preservative by full-cell pressure method, but difficult to dry (air & kiln). Proper quality control must be maintain from procurement to treatment, specially during physical selection & d...
G N M Ilias, M D Rokib-ul-Hafiz


Biological resistance of wood treated with waterbased resins and drying oils in a mini-block test
1998 - IRG/WP 98-40107
In recent years it was found that the resistance of wood against fungal degradation could be increased by impregnation with an etherificated melamine formaldehyde resin. Using this resin as a reference, a waterbased fatty acid modificated alkyd-resin and two drying-oils were assessed for their biological performance in a mini-block laboratory test. Although drying-oils, like linseed-oil, are often...
M Sailer, A O Rapp, R-D Peek


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg


The effect of preservative distribution in small blocks of Pinus sylvestris on the toxicity of tributyltin oxide to Reticulitermes santonensis Feytaud
1971 - IRG/WP 206
Small blocks of Pinus sylvestris (50x25x15 mm³) were treated by a full-cell method with various concentrations of tributyltin oxide in benzene. Replicate blocks were then freeze dried, rapidly air dried or slowly air dried and exposed to surface attack by the subterranean moistwood termite Reticulitermes santonensis Feytaud. At all concentrations it was found that the freeze-dried blocks were mor...
M P Levi, D N R Smith


Heat transfer and wood moisture effects in moderate temperature fixation of CCA treated wood
1994 - IRG/WP 94-40022
Practical aspects of heat transfer and fixation of wood exposed to drying conditions after CCA treatment are considered. The rates of heat transfer and CCA fixation are substantially influenced by the cooling effect of water evaporating from the wood surface when drying occurs during fixation. At least in the early stages of fixation, the wood temperature approaches the wet bulb temperature, rathe...
J Chen, M Kaldas, Y T Ung, P A Cooper


Alternatives to preliminary oven-drying prior to spot-testing treated timber for borate or TBTN preservative penetration
1995 - IRG/WP 95-20067
Commonly-used penetration test procedures for timber treated with borate or organotin wood preservatives demand preliminary oven-drying before application of the spot-testing reagent(s), in order to achieve reliable results. The delay of 12 hours or more during oven drying is often a nuisance. Modifications to the spot-testing procedures, involving alternative solvents and acidification conditions...
M J Kennedy, A Zosars, J Norton


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry