IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 603 documents. Displaying 25 entries per page.


Field trials of groundline remedial treatments on soft rot attacked CCA treated Eucalyptus poles
1983 - IRG/WP 3222
A total of 17 CCA treated Eucalyptus poles, which were found to contain 2-5 mm of soft rot in October, 1980, were reinspected in October, 1982. In 1980, 11 of the poles were given a supplemental groundline bandage treatment of either Osmoplastic or Patox, while 6 of the poles were designated as untreated controls. Two years after remedial treatment, samples were removed from the poles for microsco...
W S McNamara, R J Ziobro, J F Triana


Durability of larch (Larix spp.) wood against brown-rot fungi
1997 - IRG/WP 97-10228
Durability of the heartwood of Larix decidua, L. sibirica, L. gmelinii, L. gmelinii var japonica, L. gmelinii var olgensis and L. sibirica x decidua against brown rot fungi Coniophora puteana, Poria placenta and Gloeophyllum trabeum was tested according to EN 113 test method. Parallel samples were used to study the amount and composition of wood extractives. The sample trees originated from the re...
H Viitanen, L Paajanen, P Saranpää, P Viitaniemi


The dry rot fungus and other fungi in houses. Part 1
1992 - IRG/WP 92-2389
J Bech-Andersen


Soft rot cavity widening - A consideration of the kinetics
1984 - IRG/WP 1227
Studies on the micromorphology of soft rot cavity formation by Phialophora hoffmannii in birch using time-lapse cinemicrography are briefly outlined. A mathematical model is constructed to describe the cavity widening process, particularly changes in the surface area of a hypothetical cavity during enlargement. On comparison with observed data it is concluded that the rate of cavity widening is de...
M D C Hale, R A Eaton


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Soft-rot ultrastructure
1981 - IRG/WP 1138 (+ Addendum)
The stages of growth of soft-rot fungal hyphae in birch cell walls has been studied using transmission electron microscopy. These observations are compared with time-lapsed cinemicrographic studies on infection and cavity development within wood cell walls which show a start-stop hyphal growth pattern. The fine structure of hyphae during each stage of the decay process shows that hyphae penetratin...
M D C Hale, R A Eaton


Some characteristics of Pinus radiata wood from trees subjected to resin extraction
1987 - IRG/WP 3403
35 year old Pinus radiata trees growing in La Puntilla (lat. 37° south, long. 72,4° west), Chile, were subjected to resin extraction 5 years ago. After harvesting them simultaneously with control trees of the same place and age, probes were taken from the bottom of each pole, at 3.4 m, 7.8 m and 11.4 m height. Analysis of ethanol/benzene extract, CCA salt penetration tests and sapstain and brown-rot development rate were performed. The extract content differed in both groups. In the ascendent sense it decreases in unextracted trees and increases in extracted. CCA salt penetration was deeper in treated trees than in untreated. Wood subjectect to resin extraction was less susceptible to sapstain development. No significant difference was detected in both groups in relation to the development of brown-rot.
M C Rose, J Navarrete, G Sandoval, A Bedoya, L Ortega, R Zurita


Physical and biological properties of albizzia waferboards modified with cross-linking agents
1995 - IRG/WP 95-40043
Chemically-modified low-density waferboards with cross-linking agents were produced using a fast-growing species of hardwood albizzia (Paraserienthes falcata Becker) as a raw materials and isocyanate resin as a glue adhesive. For the chemical modification, the vapor-phase formalization of the boards and the pad-dry-cure treatment of wafers with cross-linking agents were employed. The vapor-phase f...
S Yusuf, Y Imamura, M Takahashi, K Minato


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1982 - IRG/WP 3207
J Beesley


The influence of crystalline and amorphous cellulose on extracellular hydrogen peroxide production by brown-rot fungi
1991 - IRG/WP 1482
The production of hydrogen peroxide (H2O2) has been suggested to play a key role in the degradation of wood by wood-rotting fungi. The production of extracellular hydrogen peroxide was studied by a quantitative method which detects the oxidation of the 2,2-azinobis(3-ethylbenzthiazoline-6-sulphonic acid) (ABTS) by H2O2 and horseradish peroxidase (HRP) in liquid culture medium. The carbon sources u...
A-C Ritschkoff, L Viikari


Basidiosporogenesis by the white-rot basidiomycetes in vitr
1994 - IRG/WP 94-10081
Basidiospores of all forest-inhabiting basidiomycetes are a primary source of infection causing wood decay. However, most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the white-rot basidiomycetes, Schizophyllum commune and Tr...
S C Croan


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


Collaborative soft rot tests: Proposals for a standardized soil burial test
1971 - IRG/WP 201
A F Bravery


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Recent soft-rot research in softwoods and hardwoods
1980 - IRG/WP 1108
The purpose of this paper is to describe briefly the current status of our research on soft-rot fungi. The work to be discussed is still in progress and any results described must be regarded as provisional....
J A Butcher


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Rational weight per weight (w/w) qualifying retention from a pole bank in Bangladesh
2000 - IRG/WP 00-40187
Weight per weight (w/w) vs weight per volume (w/v) retention study revealed that the w/w % retention is found to be appropriate and uniform for all timber species in respect of its real effectiveness. The pole species having density below 512 kg/m3 (32pcf.) showing w/v retention below 20kg/m3 (1.25pcf.) have equal w/w retention of 4%. The apparently reduced w/v retention of low density poles will ...
A K Lahiry


Cytochemical localization of hydrogen peroxide in brown rot fungus Tyromyces palustris by cerium chloride technique
1999 - IRG/WP 99-10299
Cerium chloride (CeCl3) was used to localize H2O2 cytochemically for studying relationship between ultrastructural and functional characteristics of cellulose degradation by brown rot fungi. This technique proved very useful in localizing discrete electron-densereactionproducts at high resolution with minimal nonspecific deposition. The cytochemical localization of extracellular H2O2 by CeCl3 usin...
Yoon Soo Kim, Seung-Gon Wi


Biological performance of gypsum products containing borates
2000 - IRG/WP 00-30237
At suitable retentions borates have biostatic properties enabling them to be used for biodeterioration control in wood. They provide protection against decay fungi, mould, and termites, which are known to also attack gypsum products. Currently, many gypsum products contain added borates, which are used to improve physical and processing characteristics. Work examining the effect of borates at cont...
J L Fogel, J D Lloyd


The effectiveness test of chemicals against Serpula lacrymans
1984 - IRG/WP 2222
The effectiveness tests of wood preservatives against Serpula lacrymans were conducted in accordance with Japan Industrial Standard A 9302 and Japanese Wood Preserving Association Standard No. 1. Also, the soil treatment test against this fungus was carried out with two chemicals. The preservatives tested without Creosote oil (out of JIS) had sufficient preservative effect against Serpula lacryman...
S Doi


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Previous Page | Next Page