Flow charts for termite and decay tests to determine the natural durability of Japanese cedar (Cryptomeria japonica D. Don)
2008 - IRG/WP 08-20385
This paper deals with the experimental flow charts that were used for determination the effects of fungal decay and termite attack on Sugi heartwood during the course of the study of “Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivate”, which was carried out by Usta et al (2006)....
I Usta, S Doi


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Removal of heavy metals from treated wood using biological methods
2005 - IRG/WP 05-50226
Heavy metals were removed from wood treated with copper based preservatives using brown-rot fungus Fomitopsis palustris. The amount of effective elements removed by treatment methods was examined. The relationship between oxalic acid concentration and the amount of heavy metals removed from each treated wood was also investigated. The relationship between fungus weight and removal rate was also in...
Dong-won Son, Dong-heub Lee


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Comparison of the effect of different soil sources on the type and rate of decay of CCA-treated pine exposed in a soil-bed
1984 - IRG/WP 2213
The types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand can be reproduced using a soil-bed exposure. Radiata pine stakelets, untreated or treated to 1.4, 2.7, or 5.4 kg/m³ with Tanalith NCA, were exposed to six different soil sources. The local nursery soil used for all standard laboratory tests was found to represent the greatest decay hazard to untreated...
J A Drysdale


Effect of permeability and extractives on the decay rate of southern pine sapwood in above grund exposure
2005 - IRG/WP 05-20310
The effects of wood permeability and hydrophilic and hydrophobic extractives on the decay rate of southern pine sapwood in above ground exposure were investigated. Permeability was determined by water sorption measurements, and the effect of extractives was studied by pre-extracting the test samples prior to outdoor exposure using water to extract hydrophilic extractives or sequential methanol/cy...
D D Nicholas, T Schultz, L Sites, D Buckner


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


Effect of light and ventilation condition on the rate of wood decay by the brown rot basidiomycete, Tyromyces palustris
1991 - IRG/WP 1517
Effect of light and the ventilation conditions of incubation jars on the wood decay by Tyromyces palustris (Berk. et Curt.) Murr. FFPRI 0507 was investigated. Under no irradiation of light, the ventilation conditions gave extensive effect on mass loss of the test pieces when the culturing was performed with culture medium designated in Japanese Industrial Standard (JIS) A 9302 (Medium A; glucose 4...
T Suzuki, M Higaki


The effect of felling time of year on CCA fixation rate and quality of selected hardwoods
1998 - IRG/WP 98-40116
White birch (Betula papyrifera), poplar (Populus sp.) and red maple (Acer rubrum) trees were harvested in winter, in spring, before the leaves flushed, after leaf flush and later in the summer. Sapwood discs were cut from the freshly felled trees, dried and cut into 25 mm and 19 mm cubes. The cubes were pressure impregnated with CCA-C and fixed under high relative humidity and at 50°C or at room ...
Y T Ung, A Taylor, P A Cooper, D P Kamdem


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


The treatment of sawn whitewood with organic solvent wood preservative
1982 - IRG/WP 3192
The impregnation schedules approved in the UK for the treatment of sawn European whitewood (Picea abies) with organic solvent borne preservatives result in comparitively high loadings relative to the limited depth of penetration they achieve. Results are presented, which show how substantial reduction in the overall loading may be achieved without concomitant reduction in penetration. A model for ...
L D A Saunders


The rate of losses of creosote from power transmission poles during storage
1998 - IRG/WP 98-50101-24
The purpose of this work was to study the rate of losses of creosote from power transmission poles and its consequences on the expected life of the poles stored for a long period in horizontal position. Apart from this main target of the study, the results could allow a rough estimate of the load of creosote substances on the soil especially when the poles are stored and this load accumulates over...
Z Vassou, A Satanakis, C Koutsikopoulus, J Petinarakis


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...
A Omidvar, M H Schneider, A R P Van Heiningen


A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


L-joint trials: Part 2: The relationship between colonisation by decay fungi and long-term performance
2002 - IRG/WP 02-20251
Many of the L-joint trials conducted at BRE were assessed during the early stages to establish the rate of colonisation by fungi, principally basidiomycetes. At that time, a system of assessment incorporating colonisation studies was proposed for inclusion within the European Standard EN 330 but was rejected for the final version of the standard. The long-term trials associated with the colonisa...
J K Carey


An initial evaluation of the environmental impact of potential marine biocides
1978 - IRG/WP 441
Pilings and other structures in the marine environment are protected primarily by impregnation with creosote alone, or in combination with coal tar or waterborne preservatives such as copper-chrome-arsenate. Some of these materials are considered as possible ecological hazards and face an uncertain future; perhaps newly developed treatments to replace these conventional ones will pose different pr...
J D Bultman, P J Hannan


L-joint trials: Part 3: Relative performance of a range of preservative products
2002 - IRG/WP 02-30292
Long-term trials using the L-joints described in BS EN 330 and AWPA Standard E9-97 have been in progress at BRE since 1982. This paper records the current assessments of decay of L-joints in trials started between 1982 and 1994 with treatments applied to both Scots pine sapwood (Pinus sylvestris) and spruce (Picea sp.). Data are provided on a range of active ingredients including TnBTO, PCP, a...
J K Carey


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part I. Effect of density and growth rate
2002 - IRG/WP 02-10445
Seed origin trials of Douglas fir (Pseudotsuga menziesii) in Britain have provided important information on growth differences between origins (Lines, 1987), but the variation in wood properties between origins has not been reported. The present paper describes a study of the variation in natural durability against two brown rot fungi (Coniophora puteana and Postia (Poria) placenta) and in a fung...
S Akhter, M D C Hale


Trial to determine a suitable schedule for radial and longitudinal treatment of plug samples by comparison of changes in the fluid retention and the treated area
2001 - IRG/WP 01-40211
A full-cell process was carried out using different treatment schedules for radial and longitudinal samples because of the anisotrophy of flow. When timbers are impregnated with preservatives much better penetrations are obtained via the end grain than laterally (across the grain). Therefore, suitable schedules for radial and longitudinal flow directions were determined in an trial experiment usin...
I Usta


Studies of the ray parenchyma cell ends on the radial flow of Sitka spruce (Picea sitchensis)
2000 - IRG/WP 00-40164
It is widely accepted that either ray tracheids or ray parenchyma cells offer the major flow pathways radially for the impregnation of softwood with preservative chemicals. It is now generally recognised that, if radial flow does occur through ray parenchyma cells, the cross-field pits play a dominating role for the liquid movement in the radial direction. In this case, the radial flow of fluid is...
I Usta


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Penetration and distribution of styrene in pressure treated hardwoods
1997 - IRG/WP 97-40094
A styrene impregnation method was used to compare liquid distribution in several species as affected by flow direction, sapwood/heartwood, and method of impregnation. Twenty-five mm ( 1") cubes were cut from the sapwood and heartwood of red maple (Acer rubrum), white birch (Betula papyrifera), yellow poplar (Liriodendron tulipifera), trembling aspen (Populus tremuloides), red oak (Quercus rubra), ...
P A Cooper, T S Janezic, U Srinivasan, A Omidvar


Previous Page | Next Page