IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 116 documents. Displaying 25 entries per page.


Comparative study between full cell and passive impregnation method of wood preservation for laser incised Douglas-fir lumber
2007 - IRG/WP 07-40359
Many wood species are highly resistant to conventional pressure treatment. To improve the chemical impregnation into Douglas-fir (Pseudotsuga menziesii Franco) lumber, the passive impregnation method had been developed. In this study, ability of the passive impregnation for lumber was compared with a conventional full cell method. Square Douglas-fir lumber with the incising density of 10,000 holes...
Md N Islam, K Ando, H Yamauchi, Y Kobayashi, N Hattori


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticity, MOE and modulus of rupture, MOR) of Turkish fir (Abies bornmulleriana Mattf.). Wood samples were mechanically tested after a mild full ce...
I Usta, M Hale


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Resistance of Alstonia scholaris vestures to degradation by tunnelling bacteria
1992 - IRG/WP 92-1547
Electron microscopic examination of vessels and fibre-tracheids in the wood of Alstonia scholaris exposed to tunnelling bacteria (TB) in a liquid culture showed degradation of all areas of the secondary wall. The highly lignified middle lamella was also degraded in advanced stages of TB attack. However, vestured pit membranes and vestures appeared to be resistant to degradation by TB even when oth...
A P Singh, T Nilsson, G F Daniel


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


Water-based water repellents for treatment of wood
1987 - IRG/WP 3446
The water uptake by wood can be reduced by treatment with a water repellent. The water repellents most commonly used are solvent based. In the present work a new type of water repellent that is water-based has been investigated. Two different treatments have shown an effect of the same order as a commercial solvent based product. The cellular distribution of the water repellents has been investiga...
I G Svensson, G Hägglund, I Johansson, W B Banks


Copper naphthenate-treated Southern Pine pole stubs in field exposure. -Part 2: Chemical characterization of full size pole stubs 12 years after treatment
2000 - IRG/WP 00-30246
This study examines the influence of pre-treatment and post-treatment steaming on the character and physio-chemical nature of copper naphthenate in hydrocarbon solvent treated pine in larger, pole diameter, pole stub-length samples. This work is the continuation of two projects that began almost a decade ago. Previous reports indicated that certain morphological changes might occur in small labora...
H M Barnes, D P Kamdem, M H Freeman


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


Ultrastructural aspects of bacterial attacks on an archaeological wood
1993 - IRG/WP 93-10007
Transmission electron microscopy of wood from a Chinese ship submerged in the mud for over 900 years showed bacteria to be the main factor for its deterioration. The micromorphology of degraded wood cell walls was similar to that observed during the attacks of wood by erosion bacteria. Other bacterial forms, previously considered lo be scavenging bacteria, were also abundant in degraded areas of t...
Yoon Soo Kim, A P Singh


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


EELS (Electron Energy Loss Spectroscopy) - a technique for quantification of nitrogen and other light elements in the cell wall
1999 - IRG/WP 99-20163
A literature survey was performed to find progress in techniques for monitoring penetration of synthetic resins in wood cell walls. Electron energy loss spectroscopy (EELS) in combination with transmission electron microscopy (TEM) was successfully applied for the high resolution examination of the distribution of a partly methylated hydroxymethyl melamine resin in Norway spruce (Picea abies Karst...
A O Rapp, H Bestgen, W Adam, R-D Peek


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Étude in vitro de la colonisation et de la dégradation structurale du bois d'aubier de Pin sylvestre par la Mérule: Serpula lacrymans Schum. ex Fr. S. F. Gray
1979 - IRG/WP 198
The degradation of Scots pine sapwood cell walls by Serpula lacrymans, a brown rot fungus, is observed after various periods of exposure from two weeks to twelve weeks. The observation by microscopy shows that the hyphae of Serpula rapidly invade the wood tissues as cell wall degradation starts. That deterioration is not gradual, it is observed to be very irregular as well within the whole of the ...
D Dirol


Previous Page | Next Page