Observations on the uptake and penetration of various liquids in clear heartwood and sapwood of Pinus radiata D.Don
1983 - IRG/WP 3224
Volumetric uptake of water (aqueous copper-chrome-arsenic (CCA)) or methanol, applied by bulk hydrostatic pressure to air dried clear heartwood specimens of Pinus radiata D. Don, far exceeds that of a wide variety of polar and non-polar solvents. In air dried sapwood, the volumetric uptake of CCA tends to be less than that achieved for most solvents including methanol. No comprehensive explanation...
J E Barnacle


Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer


Effects of boron treatments on partially decayed oak and pitch pine heartwood
1996 - IRG/WP 96-30106
This paper reports results of borate based preservative treatment and leaching experiments on partially decayed oak and pitch pine heartwood. Previous experiments have shown little damage is caused to sound timber of these types when treated with Polybor and Boracol 20 preservatives. This experiment was carried out to assess the suitability of selected borate based preservatives for use in histori...
S McCutcheon, G M Smith, J W Palfreyman, P Durrant


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


Soft rot studies on CCA treated eucalypt power transmission poles
1981 - IRG/WP 1132
Initial results found for sixty CCA treated eucalypt poles, from a soft-rot survey are discussed. Retentions of CCA within above and below ground pole samples were variable. The variation was attributed mostly to biodegradation and effect of soil environment, rather than leaching. Bacterial decay was found in many poles and was severe in some cases. Although found in the presence of soft-rot decay...
L E Leightley


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


The effect of wick action on the moisture distribution in heartwood and sapwood stakes of Pinus radiata D. Don.
1999 - IRG/WP 99-40139
The pattern of moisture distribution in stakes of Pinus radiata D. Don. subjected to "wick action" is investigated. There was incomplete saturation of the stakes even after 93 days of continual soaking. Maximum moisture absorption occurred at the base of the stake and at the air/water interface of the stake. Incomplete saturation of the stake was thought to be due to air embolism within the wood. ...
J Hann, P Vinden


Diffusion of a copper naphthenate/boron paste through Douglas fir heartwood
1991 - IRG/WP 3671
Groundline wraps are an important portion of the remedial treatment strategies for protecting utility poles in North America from surface decay. The compositions of these wraps have recently shifted away from pentachlorophenol and creosote to formulations containing copper naphthenate and boron. These formulations have not yet been extensively tested, although the chemicals have been used for many...
P G Forsyth, J J Morrell


The influence of wood moisture content on the fungitoxicity of methylisothiocyanate in Douglas fir heartwood
1987 - IRG/WP 3430
The fumigant methylisothiocyanate (MIT) effectively controls decay fungi in large wood structures, but the influence of environmental factors on its performance are not well understood. Experiments found wood moisture content to greatly influence the fungitoxicity and sorption of MIT in Douglas fir heartwood. At constant, low MIT vapor concentrations (less than 1 µg/cc air), wood at 10% MC bound ...
A R Zahora, J J Morrell


Presteaming radiata pine heartwood to improve treatability
1983 - IRG/WP 3239
Steaming and holding before preservative treatment by the Bethell process greatly improved the treatment of radiata pine heartwood. Maximum penetration of preservative for the shortest holding period was obtained by the use of steam vacuum but the difference between this and steam venting was small when compared with the standard of treatment of air dried samples. A holding period of one day was s...
A J Bergervoet


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Effect of extractive fractions of Thuja plicata and Chamaecyparis nootkatensis heartwood on Coptotermes formosanus
2004 - IRG/WP 04-10535
Heartwood of some species has natural resistance to attack by termites due to the presence of toxic and/or repellent extractives, but the role of individual extractives in termite inhibition is poorly understood. Developing a better understanding of which extractives are most effective against termites may be useful for the identification of improved termite management strategies. The effect of se...
A Taylor, B L Gartner, J J Morrell, K Tsunoda


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Biochemical relationships between biodegradation of cellulose and formation of oxalic acid in brown-rot wood decay
1991 - IRG/WP 1472
Non-enzymic hydrolysis of cellulose with low concentrations of oxalic acid was examined. The incubation of pine wood pulp with 1% oxalic acid (pH 1.3) at 35°C for 4 weeks reduced the original viscosity to 60%. Reducing sugars were liberated from various cellulosic samples by the oxalic acid treatment. However, crystallinities of cellulose in those samples did not change before and after the treat...
M Shimada, Y Akamatsu, A Ohta, M Takahashi


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang


In-ground field test of scots pine (Pinus sylvestris L.) sapwood and heartwood
2004 - IRG/WP 04-30336
Scots pine (Pinus sylvestris L.) sapwood and heartwood stakes treated with CCA-C and creosote were tested for one- year in a field plot in Bartın region in Turkey. Scots pine heartwood stakes had lower preservative retention than sapwood stakes. Bending strength of the stakes was decreased after impregnation and one-year field test. While the bending strength of untreated sapwood was 93....
H Sivrikaya, H Hafizoglu


Soft Rot Decay of Cengal (Neobalanocarpus heimii) Heartwood in Ground Contact in Relation to Extractive Microdistribution
2003 - IRG/WP 03-10501
The heartwood of cengal (Neobalanocarpus heimii, fam. Dipterocarpaceae) is naturally durable. A square-sawn utility pole specimen of cengal heartwood, after 30 years in ground contact, showed 10-15 mm surface decay all around the ground line position, accompanied with isolated surface termite attack at the decayed region. Light and transmission electron microscopy (TEM) of the decayed regions prov...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi, Kwang Ho Lee


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


Previous Page | Next Page